Latest issue

№11 2026

  • 1
    G. S. Sevalnev, I. I. Vlasov, D. S. Kopylova, N. O. Yakovlev, E. I. Lukin, M. A. Samoilova

    A comprehensive study was conducted to examine the effect of quenching temperature (900–1100 °C) on the structure, mechanical properties, strain hardening, and corrosion resistance of high-nitrogen martensitic steel grade 12Kh14AMF with a super-equilibrium nitrogen content, produced by electroslag remelting under nitrogen pressure. It was found that quenching from 1050 °C provides an optimal combination of properties: tensile strength, hardening index, hardening life and corrosion current in a 3.5% NaCl solution.

  • 2
    M. M. Karashaev, A. V. Vostrikov, D. I. Sukhov

    This paper presents the key principles of modern disk blank production from nickel-based heat-resistant alloy powder granules produced by the granule metallurgy method (as-HIP). The results of studies devoted to this area are analyzed, and reflect the relationship between the structure and mechanical properties of nickel-based superalloys and the process parameters for producing disk blanks obtained using hot isostatic pressing technology.

  • 3
    P. A. Slobodskoy, N. S. Moiseeva, K. V. Dulnev, E. A. Yeliseyev, M. S. Alekseeva

    The article presents the results of a study of heat treatment modes on the phase composition, structure and properties of nitrogen-containing steel of the martensitic class. A comprehensive study of the steel phase composition after conducting various heat treatment processes, using thermodynamic modeling and X-ray phase analysis, showed a high degree correlation between calculated and experimental data. It was found that the most favorable combination of hardness and impact toughness is achieved when 3–5 wt.% of the residual austenite is preserved in the structure in the martensitic matrix.

  • 4
    M. S. Yashin, D. V. Kapitanenko, A. S. Shpagin, A. V. Vostrikov

    This article presents the results of a computer simulation of the isothermal deformation of blanks made of EI698 heat-resistant nickel alloy. Analysis of plastic deformation, temperature, shape, dimensions, energy-force parameters and trace lines allowed to plot a technological deformation process for the blank with optimal deformation parameters. After manufacturing forgings from EI698 alloy under isothermal conditions, the mechanical properties were evaluated. The test results confirmed the computer simulation results.

  • 5
    I. Benarieb, D. V. Zaytsev, Yu. A. Puchkov

    Quench-induced precipitates formed in a 1.2 mm thick sheet specimen of Al–0.73Mg–0.60Si–0.18Cu–0.27Mn–0.23Fe alloy (V-1341) after quenching at a cooling rate of 0.3 °C/s (below the critical cooling rate) and subsequent natural ageing were studied by transmission electron microscopy, Fourier-transform analysis, and energy-dispersive X-ray microanalysis. The precipitates were found to correspond predominantly to metastable β′(Mg9Si5) and B′(Al3Mg9Si7) phases. It was shown that copper can be incorporated into the quench-induced precipitates and, at increased local concentrations, may cause structural heterogeneity.

  • 6
    I. G. Lukachevskaia, O. V. Startsev, D. R. Nizin, A. A. Dyakonov, A. L. Tereshkin

    The effect of moisture content on the tensile strength of unfilled Etal-247 epoxy polymer cured with Etal-1472, Etal-45M, Etal-45TZ2 and Etal-M7 was studied. Increasing water content reduced the strength of all compositions, while the character and intensity of the relationship depended on the hardener. Etal-45TZ2- and Etal-M7-based systems showed the highest sensitivity to initial moisture uptake. Surface morphology may influence the initial stage of water ingress, whereas the principal mechanism governing the change in mechanical properties is plasticization of the bulk polymer network.

  • 7
    A. A. Evdokimov, E. A. Veshkin, A. V. Slavin, A. A. Barannikov

    The course of the research aimed at developing technology for manufacturing sheets of profiled fiberglass flooring is presented. The main stages of the manufacturing technology for structures made of PCM with dimensions of 3000×1500 mm based on epoxy and epoxy vinyl ester resins are described: the development of fiberglass, mathematical modeling of the infusion process and the establishment of an optimal technological regime of impregnation, taking into account the pot life of the resins, the determination of technological parameters for the manufacture of structure.

  • 8
    D. N. Shafiev, A. I. Tkachuk, E. S. Suvorova, G. B. Eldyaeva, A. V. Kovalenko, N. K. Sidelnikov

    The article provides the review of characteristics of the VPZ-25 syntactic polymer filler developed at the NRC «Kurchatov Institute» - VIAM considering climatic tests and kinetics patterns. The paper presents the results of a study of the characteristics of samples of VPZ-25 cold-curing syntactic polymer filler after climatic tests. Kinetic studies were conducted using the differential scanning calorimetry (DSC). Based on the research results, conclusions were drawn regarding the possibility of using this spheroplastic under conditions of elevated humidity and temperature, as well as its application in aircraft interiors.

  • 9
    N. M. Parashchenko, M. S. Kozhukharov

    The article focuses on the study of the microstructure and applications of polymer-derived ceramic (PDC) materials. It examines microstructure analysis techniques, including spectroscopic and microscopic approaches, along with key aspects of the evolution of of the microstructure during high-temperature processing. Special attention is given to the role of nanodomains and free carbon in shaping PDC properties. Promising application areas for such materials are discussed, including composites, coatings, microelectronics, and energy technologies.

  • 10
    A. V. Losev, A. I. Gulyaev

    The transcrystalline layer at the “fiber–polymer matrix” interface is a key structural component of thermoplastic composites, determining the effectiveness of interfacial interaction and the transfer of mechanical loads between the material components. Controlled formation of the transcrystalline layer is an effective tool for controlling the interfacial structure and performance properties of thermoplastic composites. Particular interest in transcrystallinity research is associated with the widespread adoption of high-temperature polymers, particularly polyaryletherketones.

  • 11
    P. M. Putilina, A. Yu. Isaev

    A review of the scientific and technical literature on the study of processes occurring during the with an electron beam of polymeric materials is presented. The technology of electron beam curing, its parameters and the equipment used are described. The advantages and disadvantages of the technology and its areas of application are highlighted. The types of electron beam curable polymers and polymerization initiators are examined. An analysis of the transformations of polymers under radiation processing and its impact on the properties of materials is provided.

  • 12
    D. V. Sidorov, A. D. Sidorov

    The article is devoted to a theoretical study of chemical reactions occurring during thermal decomposition of an isolated methyldichlorosilane molecule. The most probable chemical reactions of methyldichlorosilane decomposition and the mechanisms of their occurrence were determined. Using the quantum chemistry method thermodynamic were calculated characteristics of products and transition structures at different temperatures. The reaction rate constants at different temperatures have been also calculated.

  • 13
    N. V. Antyufeeva, I. V. Zelenina, A. V. Nacharkina, A. V. Kosyakova, A. V. Efremova, P. S. Marakhovsky

    In the study was investigated the effect of additional heat treatment at temperatures of 300, 320, and 350 °C on the properties of polyimide-based carbon fiber reinforced plastic. It was shown that increasing the post-curing temperature raises the glass transition temperature from 336 to 358 °C. When tested under room temperature conditions and after heat treatment, the flexural strength and interlaminar shear strength of the material decreased. Furthermore, the heat treatment influenced the thermophysical properties: coefficient of linear thermal expansion, thermal conductivity, thermal diffusivity and specific heat capacity.

  • 14
    A. A. Krivushina, D. N. Mosunova, Yu. S. Goryashnik, T. V. Yakovenko

    Data on the species composition of microscopic fungi isolated from polymeric materials in various climatic regions were analyzed and summarized. More than 250 microscopic fungal strains belonging to 98 species and 36 genera were isolated, most of them anamorphs of the Ascomycota phylum. The isolated strains hold promise for studies of the microbiological stability of materials and the effectiveness of biocidal agents used in various climatic regions.