1
The work is devoted to the development of a technology for producing a cold-rolled sheet from a heat-resistant alloy of the Fe–Cr–Al–Y system. The alloy of the Fe–Cr–Al–Y is intended for the manufacture of honeycomb seals for the flow path of gas turbine engines with an operating temperature of up to 1100 °С. This alloy is intended to replace heat-resistant alloys ЭИ435 and ЭИ868, which are currently used for the manufacture of honeycomb seals. In terms of heat resistance, the alloy of the Fe–Cr–Al–Y system is significantly superior to nickel alloys ЭИ435 and ЭИ868.
-
2
The paper presents a comparative analysis of the microstructure, size and distribution of carbides, hardness and tribotechnical properties during research and testing under the same conditions of bearing steel grades 60Kh13S-ShD, 95Kh18-Sh and 110Kh18M-ShD, commercially used in the Russian industry. Based on the results of the research, steel grades were identified that have the best set of properties after hardening heat treatment.
-
3
This article presents the results of studies of the influence of various modes of hot isostatic pressing (HIP) and heat treatment on the mechanical properties and structure of cast samples from the VT40L alloy. The temperature of the polymorphic transformation in the alloy was determined experimentally using the test quenching method. Tensile tests were carried out to determine the short-term strength and yield strength, the endurance limit on the basis of N = 2·107 cycle, impact strength and hardness were determined. Based on the test results, a casting processing mode was selected that provides a set of properties necessary for parts of aircraft products.
-
4
A porous carbon material and a metal composite material (MCM) based on an aluminum casting alloy of the Al–Si–Cu system containing 79±2 % (vol.) carbon, obtained using the vacuum-compression impregnation technology, have been studied. A study of the structure of MCM was carried out, the density, volumetric filling and temperature coefficients of linear expansion (TCLE) of the carbon frame and MCM were measured in the temperature range from 20 to 200 °C. It has been established that depending on the direction of the basal planes, the TCLE value decreases by 30–35 % at the carbon frame and by 15–20 % at MCM.
-
5
The process of agglomeration of granules of high-temperature metal-ceramic material based on molybdenum by high-temperature diffusion is discussed. The dependence of the size of the obtained granules on the agglomeration temperature is established. The influence of the agglomeration temperature on the strength of diffusion bonds arising between granules during high-temperature exposure is given is demonstrated.
-
6
Using the method of high-speed solidification of a hanging drop of a melt, discrete of the Ме–3TiC–2B4C, where Me is a metal Co, Ni or Fe. The microstructure of the alloy was studied, and mechanical properties of discrete fibers were obtained. To assess the effect of high-speed solidification of the melt on the properties of the alloys, cast samples were made without quenching. It was shown that the cobalt – based alloy in the initial state after quenching contains a metastable phase whit a face-centered cubic lattice, the proportion of which is 58 %. In addition, cobalt-based fibers contain metastable disperse intermetallic compounds of Co2B and Co3B.
-
7
The influence of conditions and duration of storage on the characteristics of a prepreg based on a melted thermosetting polyimide binder grade VS-51 and high-temperature carbon fiber reinforced plastic based on it are studied. In accordance with the data obtained, the guaranteed shelf life of the prepreg was determined in the temperature range from –(18±5) to +(20±5) °С. The binder, reinforcing carbon filler, prepreg and carbon fiber reinforced plastics were manufactured at the technological base of the NRC «Kurchatov Institute» – VIAM.
-
8
Environmental problems, primarily such as the inability to recycle materials and, consequently, the formation of uncontrolled landfills, are powerful incentives for the development of biodegradable materials. Due to its environmental and economic advantages, as well as its technical characteristics, natural fibers become a likely replacement for synthetic ones for use as fillers in polymer composite materials. Flax fibers, due to their high availability and specific properties, are the most valuable products of the bast type. Physical and chemical processing of fibers allows them to be used for structural materials as well.
-
9
The use of parts made of polymer composite materials in the design of aircraft poses additional challenges to prevent contact corrosion. Polymer composite materials differ significantly in electrochemical properties from metal materials used in airframe construction. The article presents studies of the corrosion behavior of electrically conductive metal coatings in contact with carbon fibers by the method of constructing anodic and cathodic polarization curves, as well as the results of corrosion testing of fasteners with protective coatings in a salt fog chamber.
-
10
The article presents a review of the scientific and technical literature in the field of methane pyrolysis in the process of chemical vapor deposition of pyrolytic carbon, summarizes the results of studies of the process depending on the parameters of deposition and the substrates used, analyzes the compositions of pyrolysis products, mechanisms and pathways of chemical reactions.
-
11
The adhesion and impact strength of paint coating systems based on the chromate-free primer VG-44 with enamels VE-69, AK-1206, UR-1161 and EP-140 after artificial aging using the LI-14 method (–60÷+80) were studied.)°С during 16 cycles, as well as after thermal aging at temperatures of 80 °C – 1000 hours and 100 °C – 500 hours. The decorative properties of coatings based on the chromate-free primer VG-44 with enamels VE-69, AK-1206, UR-1161 and EP-140 after artificial aging were determined. It has been shown that artificial aging of the above paintwork systems does not have a significant effect on the strength of coatings upon impact, but leads to a decrease in tensile strength, as well as a decrease in the gloss of the coatings.
-
12
The main development trends in the field of creating matte, wear-resistant paint and varnish coatings for painting instrument panels and aircraft cockpit elements are considered. The basic principles that should be followed when creating matte, wear-resistant paint and varnish coatings have been identified. The basic requirements that determine the selection of the main components for obtaining a matte wear-resistant coating are considered. Polymer film-forming agents and fillers have been identified for the development of coating compositions in accordance with the analysis. Leaders in the development of matte wear-resistant coatings have been identified.