• 1
    Ovsepyan S.V., Akhmedzyanov M.V., Filonova E.V., Zaysev D.V.

    The effect of annealing at the temperature of 800–1040 °С on the η-phase formation in the weldable wrought VZh176 alloy of the Ni–Fe–Co–Nb–Ti system, intended for use in gas turbine engines, has been investigated. It is shown that annealing leads to the precipitation of η-phase particles and change the shape and distribution: from short plates at the grain boundaries to the Widmanstatten structure. The dependence of the quantity of the phase on the duration of processing is established. The composition and crystallographic structure of the η-plates are determined by the methods of transmission electron and scanning microscopy, using the methods of backscattered electron diffraction and х-ray microanalysis. A diagram of the change of the η-phase from temperature and duration of treatment was built.

  • 2
    Duyunova V.A., Trapeznikov A.V., Leonov A.A., Koreneva E.A.

    The article presents and summarizes data on the modification of cast aluminum alloys. In addition to the use of standard modifiers such as sodium, strontium, titanium, zirconium, scandium and titanium diboride, a positive effect of europium and hafnium on alloys has been shown. Despite the fact that many effective modifiers belong to the rare earth elements (REE), not all REE have a strong effect. The introduction of metals such as ytterbium and erbium into aluminum alloys had almost no effect on the morphology and size of the microstructure.

  • 3
    Zavarzin S.V., Duyunova V.A., Fomina M.A.

    Titanium alloys often have an advantage over steel in terms of weight and corrosion-resistant characteristics. However, their use in the «hot» parts of gas turbines is limited by the low maximum operating temperature, which is due to their corrosive behavior in the high-temperature region. The paper analyzes the main mechanisms proposed to describe the corrosion behavior of titanium alloys in the main environments typical for the operation of gas turbines. The determining role of titanium in these processes is shown, which limits the possibilities of alloying alloys.

  • 4
    Kondrashov S.V., Solovyanchik L.V., Minaeva L.A., Shorstov S.Yu.

    The problem of simultaneously reducing the amount of functional filler and achieving the required level of electrically conductive properties of polyamide compositions can be solved by using a hybrid filler based on carbon black and carbon nanotubes. It is shown that due to the high specific surface area of carbon in the extrusion process, the destruction of the initial agglomerates does not occur completely, in addition, the reactation of pre-dispersed TU/CNT particles can occur, which allows the formation of a complex structure of the material – a filler localized in small particles distributed throughout the volume of the polymer matrix.

  • 5
    Prokopenkov V.G., Kolpachkov E.D., Shosheva A.L.

    Results of a study on influence of glass fiber-reinforced bismaleimide composition and curing cycles on the level of its properties are shown. Current development and research in the field of bismaleimide resins and prepregs based on them both in the domestic and the international markets is examined. After testing, a series of physical and mechanical properties were obtained. Based on the results, composition with the highest flexural strength and glass transition temperature was chosen.

  • 6
    Korolev D.V., Valeev R.A., Piskorsky V.P., Morgunov R.B.

    Various aspects of the use of RE–TM–B alloys for the development of magnetocaloric cooling systems are considered. Thermodynamic analysis of temperature variations, magnetic part of entropy, internal energy and mechanical work performed in the Carnot cycle is given. The analysis of such factors as the limiting frequency of cycles, thermal conductivity and heat capacity of the working fluid, the density of particles with spin is given. The possibilities of creating hybrid magnetocaloric machines in which the transition between the para- and ferromagnetic states of rare-earth alloys are stimulated by external influences: temperature, mechanical stresses, laser and current remagnetization are discussed.

  • 7
    Artemenko N.I., Tatarnikov S.V., Doronin O.N.

    The dependence of the coefficient of use of ceramic powder material on the parameters of coating by the plasma spraying method was obtained in the work. The dependences of the material utilization factor and arc current, the ratio of argon and nitrogen consumption, the total consumption of plasma gases, the spraying distance and the fractional composition of the powder material are established, and the natural limitations of the variability of these parameters are described. The dependence of the material utilization factor on the average value of the fraction range has been established.

  • 8
    Losev A.V.

    A review of developments and scientific publications in the field of protective coatings based on polyvinylidene fluoride and vinylidene fluoride copolymers is presented. Chemical properties of the polymer, its polymorphic modifications, peculiarities of dissolution and properties of obtained dispersions in the environment of organic solvents are described. Advantages and disadvantages of obtained protective coatings are given. A review of research results on modification of polyvinylidene fluoride dispersions with inorganic fillers and preparation of superhydrophobic coatings is presented.

  • 9
    Kravchenko N.G., Shchekin V.K., Efimova E.A., Zherdev D.V.

    Comparative experiments were carried out to determine the protective properties of promising conservation oils in comparison with standard K-17 oil. The most effective conservation oils that can be used in the development of recommendations for the protection of aircraft parts and the revision of current regulatory documentation have been determined. Based on the analysis of the oil-soluble corrosion inhibitors contained in the tested oils and the mechanism of their action, an assumption was made to explain the effectiveness of a particular oil.

  • 10
    Startsev V.O., Vardanyan A.M.
    Part 3. Climatic aging of nanomodified cyanester carbon plastic

    In the third part of the article, the influence of additives of multilayer carbon nanotubes (astralene) on the change in the coefficient of linear thermal expansion (CLTE) of CFRP based on a cyanoether binder, exposed for 24 months in a temperate climate and laboratory simulation conditions, is considered. It is shown that the presence of 0.5 and 3.0 wt. % astralene significantly changes the CLTE in the glassy and highly elastic states of the binder carbon fiber in the initial state and at the stages of 24 months of climatic testing in the modes of standard exposure on an open atmospheric stand and exposure with weekly thermal cycles simulating the mode of takeoff and landing of an aircraft. The mechanism of the stabilizing effect of the nanomodifier was revealed when comparing the CLTE, compressive and bending strengths, and the glass transition temperature of the binder during the aging of carbon fiber in natural and simulated laboratory conditions.

  • 11
    Ivanov M.S., Pavlukovich N.G., Donskih I.N., Morozova V.S.

    Within the framework of the general qualification of the VRT-12 brand coated textile material developed by the «Kurchatov Institute» ‒ VIAM for the manufacture of a sealed shell of flexible air ducts of the air conditioning system of aircraft, studies of fire safety characteristics and the influence of operational factors on the properties of the material were carried out. Compliance of the material with aviation regulations on flammability, smoke formation and release of toxic gases has been established. Resistance to temperatures from ‒60 to +80 °C, high humidity, mold fungi and aggressive liquids has been confirmed.

  • 12
    Skorobogatko D.S., Golovkov A.N., Kudinov I.I., Kulichkova S.I.

    A review of the physicochemical properties of defectoscopic materials that affect the results of penetrant testing has been carried out. The rationale for the need to determine and verify each parameter of a set of defectoscopic materials is presented. The properties of the components of the kits that are not specified in the quality certificates and manufacturer's certificates are considered. It has been established that the characteristics and properties specified in the technical documentation of the manufacturer are not enough to assess the quality of defectoscopic materials. Parameters for quality assessment are proposed, which will allow choosing the most technologically advanced modern sets of defectoscopic materials.