Investigation of the influence of the parameters of applying the ceramic layer of the ZrO2–7 % Y2O3 heat-shielding coating by plasma spraying on the productivity of the technological process

Artemenko N.I., Tatarnikov S.V., Doronin O.N.
Artemenko N.I., Tatarnikov S.V., Doronin O.N. Investigation of the influence of the parameters of applying the ceramic layer of the ZrO2–7 % Y2O3 heat-shielding coating by plasma spraying on the productivity of the technological process // Proceedings of VIAM. 2023. No. 4. DOI: 10.18577/2307-6046-2023-0-4-69-80. URL: https://viam-works.ru/en/journal/2023/4/7
Keywords
thermal barrier coating, ceramic layer, plasma spray, material utilisation rate, plasma, plasma torch, arc discharge
Abstract

The dependence of the coefficient of use of ceramic powder material on the parameters of coating by the plasma spraying method was obtained in the work. The dependences of the material utilization factor and arc current, the ratio of argon and nitrogen consumption, the total consumption of plasma gases, the spraying distance and the fractional composition of the powder material are established, and the natural limitations of the variability of these parameters are described. The dependence of the material utilization factor on the average value of the fraction range has been established.

Reference list
  1. Hasui A. Spraying technique. Ed. V.S. Blokhin, E.V. Melnikov. Moscow: Mashinostroenie, 1975, 288 p.
  2. Grechanyuk N.I., Kucherenko P.P., Grechanyuk I.N. et al. Modern heat-shielding coatings for gas turbine engine blades and equipment for their production. Naukoví notatki, 2011, no. 31, p. 92.
  3. Gurrappa I., Sambasiva Rao A. Thermal barrier coatings for enhanced efficiency of gas turbine engines. Surface CoatingsTechnol, 2006, no. 201, pp. 3016. DOI: 10.1016/j.surfcoat.2006.06.026.
  4. Kablov E.N., Ospennikova O.G., Svetlov I.L. Highly efficient cooling of GTE hot section blades. Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 3–14. DOI: 10.18577/2071-9140-2017-0-2-3-14.
  5. Treninkov I.A., Zavodov A.V., Petrushin N.V. Research of crystal structure and microstructure of the ZhS32-VI nickel-base superalloy synthesized by selective laser fusion method, after high-temperature mechanical tests. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 57–65. DOI: 10.18577/2071-9140-2019-0-1-57-65.
  6. Loshchinin Yu.V., Budinovskiy S.A., Razmakhov M.G. Heat conductivity of heat-protective coatings ZrO2–Y2O3 alloyed by REM oxides obtained by magnetronny application. Aviaсionnye materialy i tehnologii, 2018, no. 3, pp. 42–49. DOI: 10.18577/2071-9140-2018-0-3-42-49.
  7. Doronin O.N., Artemenko N.I., Stekhov P.A., Voronov V.A. Deposition of ceramic layers of heat protection coatings based on the system Gd2O3–ZrO2–HfO2 and Sm2O3–Y2O3–HfO2. Aviation materials and technologies, 2022, no. 1 (66), paper no. 10. Available at: http://www.journal.viam.ru (accessed: November 24, 2022). DOI: 10.18577/2713-0193-2022-0-1-129-142.
  8. Samsonov G.V., Borisova A.L., Zhidkova T.G. et al. Physical and chemical properties of oxides: a reference book. Moscow: Metallurgiya, 1978, 472 p.
  9. Kablov E.N., Karachevtsev F.N. Vaporization and thermodynamics of ceramics based on the La2O3–Y2O3–HfO2 system studied by the high-temperature mass spectrometric method. Rapid Communications in Mass Spectrometry, 2018, vol. 32, no. 9, pp. 686–694.
  10. Aleksandrov D.A., Muboyadzhyan S.A., Zhuravleva P.L., Gorlov D.S. Investigation of the effect of surface preparation and ion-assisted deposition on the structure and properties of erosion-resistant ion-plasma coating. Trudy VIAM, 2018, no. 10 (70), paper no. 08. Available at: http://www.viam-works.ru (accessed: November 25, 2022). DOI: 10.18577/2307-6046-2018-0-10-62-73.
  11. Matsumoto K., Itoh Y., Kameda T. EB-PVD process and thermal properties of hafnia-based thermal barrier coating. Science and Technology of Advanced Materials, 2003, no. 4, pp. 153. DOI: 10.1016/S1468-6996(03)00009-3.
  12. Sosnin N.A., Ermakov S.A., Topolyansky P.A. Plasma technologies. Guide for engineers. St. Petersburg: Publishing house of Polytech. Univ., 2013, 406 p.
  13. Hasui A., Morigaki O. Surfacing and spraying. Trans. from Japanese. Ed. V.S. Stepin, N.G. Shesterkin. Moscow: Mashinostroenie, 1985, 240 p.
  14. Kudinov V.V. Plasma coatings. Moscow: Nauka, 1977, 184 p.
  15. Thermal spraying: textbook. Ed. L.H. Baldaev. Moscow: Market DS, 2007, 344 p.
  16. Kudinov V.V., Bobrov G.V. Spray coating. Theory, technology and equipment: textbook for universities. Moscow: Metallurgiya, 1992, 432 p.
  17. Sidorov A.I. Restoration of machine parts by spraying and welding. Moscow: Mashinostroenie, 1987, 192 p.
  18. Kibzun A.I., Goryanova E.R., Naumov A.V., Sirotin A.N. Theory of Probability and Mathematical Statistics. Basic course with examples and tasks. Moscow: Fizmatlit, 2002, 224 p.