    Kuzmina N.A., Petrushin N.V., Visik E.M., Eremin N.N., Naprienko S.A.

    A study of the structure of a single-crystal sample of a nickel heat-resistant alloy, brittle destroyed by mechanical cutting. The study was carried out using x-ray diffractometry – «swing» and the Laue method. The possibilities of the Laue method for studying local defects of various origin are shown. Based on the obtained data, an assumption is made about the recrystallization nature of structural defects in a single crystal of a nickel heat-resistant alloy; the elastic properties of the single crystal are estimated.

  • 2
    Petrova A.P., Kuznetsova V.A., Lukina N.F., Isaev A.Yu.

    Properties of glued joints of D16-AT aluminum alloy with previously put adhesive priming covering EP-0214, received using glue-hermetic Elasil 137-175M are given. Stability of properties of glued joints, both without first coat, and with first coat EP-0214 is shown, is direct after pasting and after thermal aging at temperatures up to 250 °С, influences of water, tropical conditions. Application of priming covering allows to increase gap between anodizing and pasting operations and to increase corrosion resistance.

  • 3
    Satdinov R.A., Veshkin E.A, Postnov V.I.

    The study of the operational properties of fiberglass, developed for use in the air conditioning system of aircraft, after exposure to accelerated climatic factors. The results of studies of the properties of fiberglass based on phenol-formaldehyde binder grade VSF-16M after exposure to thermal and heat-moisture aging, the influence of aggressive media, as well as mycological tests are considered. The microhardness of a polymer matrix in plastic is investigated depending on the influence of operating factors. The assessment of the properties of fiberglass for compliance with the norms of AP-25 (p. 831 «Ventilation» – the content of toxic impurities in the air).

  • 4
    Gunyaeva A.G., Sidorina A.I., Klimenko O.N.

    The description of hybrid metalcarbon reinforcing filler is provided, results of determination of its properties are provided. As object for research it is considered CFRP on the basis of hybrid metalcarbon reinforcing filler of the VTkU-2.280M brand and the epoxy molten binding. Experimental samples of prepregs CFRP on the basis of epoxy molten binding and two types of fillers are made: hybrid metalcarbon reinforcing filler of the VTkU-2.280M brand and carbon equal strength filler of the VTkU-2.200 brand, properties of prepregs and CFRP are investigated, the comparative analysis of the received results is carried out. Possible options of application of hybrid metalcarbon reinforcing filler and PKM on its basis are considered.

  • 5
    Barannikov A.A., Postnov V.I., Veshkin E.A, Starostina I.V.

    Based on the study of the wetting phenomenon and the theory of adhesion, the surface of fiberglass of the VPS-53K brand was studied before and after its treatment with atmospheric pressure plasma, which is one of the advanced methods of surface preparation for various adhesion processes. Two methods for determining the free energy of a surface are considered – the OUN's, Wendt's, Rabel's, and Kjelbla's method and the extended Fowkes method. The values of the free energy of the surface and its components are obtained using two methods under consideration. The connection between the energy characteristics of the surface of fiberglass of the VPS-53 K brand and the strength of the adhesive joint based on it is established.

  • 6
    Lebedeva Yu.E., Afanasiev-Khodykin A.N., Prokopchenko G.M., Shavnev A.A., Serebryakov D.I.

    The interaction of the SiC–SiCw–B4C–AlN system ceramic composite material (CCM) with the EP648 alloy in the process of high-temperature brazing was studied. The smallest erosion activity both in relation to CCM, and to the EP648 alloy, has HMP solder VPr50. An experimental constructionally similar sample of the nozzle assembly sector was made using uncooled nozzle blade prototypes from CCM. Tests of an experimental constructionally similar sample of the nozzle assembly sector at a temperature of 1500 °C were carried out. No traces of material ablation from the surface of the CMC were found.

  • 7
    Krasnov E.I., Kurbatkina E.I., Shavnev A.A., Serpova V.M., Zhabin A.N.

    Рresents a review of the application of the active brazing method for joining fibrous compo-site materials based on titanium alloy with ceramics based on aluminum oxide and zirconium dioxide. The basic problem arising from the combination of metals and ceramics, examples of solving problems compounds represented by the relationship of the microstructure of the connection zone with mechanical properties and shows the effect of additives Ti, B and W on microstructure and mechanical properties. Conclusions are made about the possibility of obtaining high-quality and durable compounds and factors affecting them.

  • 8
    Evdokimov A.A., Imametdinov E.S., Malakhovskiy S.S.

    The article describes the results of research work on the reinforcement of concrete structures via carbon reinforcing filler with a cold curing resin. As an object of research were selected: brand of concrete M-350 and experimental cold curing carbon fiber based on an epoxy matrix. The physico-mechanical characteristics of carbon fiber are investigated. The properties of concrete samples externally reinforced with carbon fiber after conducting full-scale exposure in various conditions and without it are investigated. It was established, that strength gain of reinforced samples compared to purely concrete samples is up to 550%.

  • 9
    Klimenko O.N., Valueva M.I., Rybnikova A.N.

    Рrovides an overview of scientific and technical information – Russian and foreign periodicals, patents for inventions – in the field of the use of polymeric materials in the sports industry and sports infrastructure. Data on world manufacturers, applied technologies, Russian developments in this direction are presented, examples of the practical use of polymeric materialsin the sports industry are shown. Special attention is paid to polymer composite materials,in particular, based on carbon fibers.

  • 10
    Iatsyuk I.V., Dobrynin D.A., Doronin O.N., Pavlova T.V.

    Provides an overview of coating removal methods widely used in the aviation industry to prepare the surface of used parts for subsequent restoration and repair. The analysis of the main advantages and disadvantages methods of removing coatings is carried out. The results of the application of the promising method of electrolyte-plasma treatment are also presented.

    For the first time in the domestic and foreign aviation industry, VIAM has developed a comprehensive technology for repairing spent turbine blades, including removing coatings by electrolytic-plasma surface treatment.

  • 11
    Khodinev I.A., Monin S.A.

    The low cycle fatigue of heat-resistant nickel alloys with a single crystal structure VZHM7 and VIN3 was studied. The tests were carried out under conditions of monitoring the complete deformation in the cycle, loading of the type «tension-compression» occurred according to a sinusoidal law with a frequency of 0,5 Hz. For both alloys, tests were carried out for three crystallographic orientations ([001], [011], [111]) at two temperatures: 500 and 850 °C. Regression lines were constructed, the limits of limited endurance were found on the basis of 104 cycles. The influence of test temperature and crystallographic orientation on the endurance limit of alloys and RMS is analyzed.

  • 12
    Startsev V.O., Slavin A.V., Nikolaev E.V.

    The method of capillary electrophoresis was used to measure the content of aggressive ions in 7 geographical points of the Gelendzhik bay in the air atmosphere and sea water during the period from September 1, 2019 to January 31, 2020. The results of measurements of the contents of K+, Na+, Mg2+, Ca2+, , Cl-, F- are compared with meteorological indicators at the time of measurement. It is shown that the total concentration of cations and anions in sea water corresponds to its salinity measured by the standard method. A high correlation between the chemical composition of samples in air and sea water was revealed.