Satdinov R.A., Veshkin E.A, Postnov V.I. Assessment of the impact of climatic factors on the performance properties of fiberglass VPS-42P/T-64 // Proceedings of VIAM. 2020. No. 10 (92). Ст. 03. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2020-0-10-21-29.

Assessment of the impact of climatic factors on the performance properties of fiberglass VPS-42P/T-64

Satdinov R.A., Veshkin E.A, Postnov V.I.
Abstract

The study of the operational properties of fiberglass, developed for use in the air conditioning system of aircraft, after exposure to accelerated climatic factors. The results of studies of the properties of fiberglass based on phenol-formaldehyde binder grade VSF-16M after exposure to thermal and heat-moisture aging, the influence of aggressive media, as well as mycological tests are considered. The microhardness of a polymer matrix in plastic is investigated depending on the influence of operating factors. The assessment of the properties of fiberglass for compliance with the norms of AP-25 (p. 831 «Ventilation» – the content of toxic impurities in the air).

Keywords
fiberglass, performance properties, air conditioning system, polymer matrix, climatic factors, properties.
Reference list
  1. Industry Standard 1 90368–86. Airplanes and helicopters. Selection of metal materials and coatings for anti-corrosion protection. 1987.94 s. Available at: https://gostost.ru/ost-1-90368-86 (accessed: July 22, 2020).
  2. State Standard 9.301–86. Unified system of protection against corrosion and aging. Metallic and non-metallic inorganic coatings. General requirements. Moscow: Standartinform, 2010. 16 p.
  3. Tomashev N.D. Theory of corrosion and protection of metals. Moscow: Publ. house of the USSR Academy of Sciences, 1959. 592 p.
  4. Berkushtis G.K., Clarke G.B. Corrosion of metals and alloys. Moscow: Metallurgizdat, 1963. 314 p.
  5. Mikhailovsky Yu.N. Atmospheric corrosion of metals and methods of their protection. Moscow: Metallurgiya, 1989. 103 p.
  6. Fomina M.A., Karimova S.A. Analysis of the corrosion state of materials of the airframe of aircraft of the «Su» type after long service life. Korroziya: materialy, zashchita, 2014. no. 9, pp. 20–24.
  7. Lukyanychev D.A., Tsygantsov I.A., Khusyanov Sh.M. Creation of a system for collecting, recording and analyzing corrosion defects arising during the operation of aircraft of the Su brand. Fundamental and applied research of corrosion and aging of materials in climatic conditions: problems and prospects: materials II scientific and technical. conf. Moscow, 2015. Available at: https://conf.viam.ru/sites/default/files/uploads/proceedings/696.rar (accessed: July 27, 2020).
  8. Fundamentals of the state policy of the Russian Federation in the Arctic for the period up to 2020 and further perspective. Available at: https://www.gov.spb.ru/static/writable/ckeditor/uploads/2018/05/14 (accessed: July 22, 2020).
  9. Strategy for the development of the Arctic zone of the Russian Federation and ensuring national security for the period up to 2020. Available at: https://www.gov.spb.ru/static/writable/ckeditor/uploads/2018/05/14 (accessed: July 22, 2020).
  10. Kablov E.N., Kirillov V.N., Zhilikov V.P., Zhirnov A.D. Study of climatic resistance of aviation materials. Collection of materials of the SB RAS «Ways of combining the potential of science in the interests of solving urgent fundamental and applied problems of strategic development of the subjects of the Russian Federation». Yakutsk, 2003, pp. 191–196.
  11. Kablov E.N. Composites: Today and Tomorrow. Metally Evrazii, 2015, no. 1, pp. 36–39.
  12. Kablov E.N. Materials for «Buran» spaceship – innovative solutions of formation of the sixth technological mode. Aviacionnye materialy i tehnologii, 2013, no. S1, pp. 3–9.
  13. Kirillov V.N. Investigation of climatic resistance of composite non-metallic materials. Collection of abstracts of reports Intern. scientific and technical conf. «Topical issues of aviation materials science». Moscow: VIAM, 2007, pp. 133–134.
  14. Pavlov N.N. Aging of plastics in natural and artificial conditions. Moscow: Chemistry, 1982. 224 p.
  15. Startsev O.V. Aging of polymer aviation materials in a warm humid climate: thesis abstract, Dr. Sc. (Tech.). Moscow, 1990. 80 p.
  16. Startsev V.O., Mahonkov A.Yu., Kotova E.A. Mechanical properties and moisture resistance of PCM with damages. Aviacionnye materialy i tehnologii, 2015, no. S1, pp. 49–55. DOI: 10.18577/2071-9140-2015-0-S1-49-55.
  17. Buznik V.M., Kablov E.N., Koshurina A.A. Materials for complex technical devices for arctic applications. Scientific and technical problems of the Arctic development. Moscow: Nauka, 2015, pp. 275–285.
  18. Andreeva A.A. Methods for conducting climatic tests to assess the resistance of materials to the conditions of marine arctic and subarctic climates. Corrosion, aging and biostability of materials in a marine climate: materials of the II Intern. scientific and technical conf. Moscow, 2016. Available at: https://conf.viam.ru/sites/default/files/uploads/proceedings/890.rar (accessed: July 27, 2020).
  19. Veshkin E.A., Satdinov R.A., Postnov V.I., Strelnikov S.V. Modern polymeric materials for the manufacture of air conditioning elements in aircraft. Polymer composite materials and production technologies of a new generation: collection of articles. reports conf. Moscow: VIAM, 2017, p. 16.
  20. Standards of airworthiness of transport category aircraft: Aviation Regulations-25. Moscow: Aviaizdat, 2009. 267 p.
  21. Kuritsyna A. D. Application of the microhardness method to determine some properties of polymeric materials. Microhardness test methods. Moscow: Nauka, 1965. 264 p.
  22. Krumova M., Klingshirn C., Haupert F., Friedrich K. Microhardness studies of functionally graded polymer composites. Composites Science and Technology, 2001, vol. 61, pp. 557–563.
  23. Veshkin E.A., Postnov V.I., Semenychev V.V., Krasheninnikova E.V. Research of microhardness and sclero-metric characteristics of the binding UP-2227N, cured by different regimes. Aviacionnye materialy i tehnologii, 2018, no. 1 (50), pp. 39–45. DOI: 10.18577/2071-9140-2018-0-1-39-45.
  24. Goyal R.K., Tiwari A.N., Negi Y.S. Microhardness of PEEK / ceramic micro- and nanocomposites: Correlation with Halpin – Tsai model. Materials Science and Engineering A, 2008, vol. 491 (1-2), pp. 230–236.
  25. State Standard 9450–76. Measurement of microhardness by indentation of diamond tips. Moscow: Gosstandart USSR, 1976. 35 p.
  26. Veshkin E.A., Postnov V.I., Semenichev V.V. Methodology for assessing changes in matrix properties in the volume of polymer composites. The role of fundamental research in the implementation of «Strategic directions for the development of materials and technologies for their processing for the period until 2030»: materials of the V All-Russian. scientific and technical conf. Moscow: VIAM, 2019, pp. 219–239.
  27. Barbotko S.L. Development of the fire safety test methods for aviation materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 516–526. DOI: 10.18577/2071-9140-2017-0-S-516-526.
  28. Barbotko S.L., Kirillov V.N., Shurkova E.N. Fire safety evolution for polymer composites of aeronautical application. Aviacionnye materialy i tehnologii, 2012. no. 3, pp. 56–63.
  29. Satdinov R.A., Veshkin E.A., Postnov V.I., Strelnikov S.V. РСМ low-pressure air ducts in aircraft. Trudy VIAM, 2016, no. 8, paper no. 08. Available at: http://www.viam-works.ru (accessed: May 22, 2020). DOI: 10.18577/2307-6046-2016-0-8-8-8.