High-temperature corrosion of titanium alloys (review)
UDC
620.193:669.295
DOI
10.18577/2307-6046-2023-0-4-27-39
Article PDF (Russian)
(842.12 KB)
How to cite
Zavarzin S.V., Duyunova V.A., Fomina M.A. High-temperature corrosion of titanium alloys (review) // Proceedings of VIAM. 2023. No. 4. DOI: 10.18577/2307-6046-2023-0-4-27-39. URL: https://viam-works.ru/en/journal/2023/4/3
Keywords
titanium, high-temperature corrosion, hot corrosion, sulfide-oxide corrosion, sodium sulfate, sodium chloride
Abstract
Titanium alloys often have an advantage over steel in terms of weight and corrosion-resistant characteristics. However, their use in the «hot» parts of gas turbines is limited by the low maximum operating temperature, which is due to their corrosive behavior in the high-temperature region. The paper analyzes the main mechanisms proposed to describe the corrosion behavior of titanium alloys in the main environments typical for the operation of gas turbines. The determining role of titanium in these processes is shown, which limits the possibilities of alloying alloys.
Reference list
- Boyer R.R. Titanium for aerospace: Rationale and applications. Advanced Performance Materials, 1995, vol. 2, no. 4, pp. 349–368.
- Dzunovich D.A., Alekseyev E.B., Panin P.V., Lukina E.A., Novak A.V. Structure and properties of sheet semi-finished products from various wrought intermetallic titanium alloys. Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 17–25. DOI: 10.18577/2071-9140-2018-0-2-17-25.
- Belov N.A., Belov V.D., Dashkevich N.I. The phase composition of multicomponent gamma luminaries based on titanium aluminides. Ed. E.N. Kablov. Moscow: VIAM, 2018, 340 p.
- Nochovnaya N.A., Bazileva O.A., Kablov D.E., Panin P.V. Intermetal alloys based on titanium and nickel. Ed. E.N. Kablov. Moscow: VIAM, 2018, 308 p.
- Appel F., Paul J.D.H., Oehring M. Gamma titanium aluminide alloys: science and technology. John Wiley & Sons, 2011, 745 р.
- Aleksandrov D.A., Muboyadzhyan S.A., Lutsenko A.N., Zhuravleva P.L. Hardening of the surface of titanium alloys by ion implantation method and ionic modification. Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 33–39. DOI: 10.18577/2071-9140-2018-0-2-33-39.
- Duyunova V.A., Oglodkov M.S., Putyrskiy S.V., Kochetkov A.S., Zueva O.V. Modern technologies for melting titanium alloy ingots (review). Aviation materials and technologies, 2022, no. 1 (66), paper no. 03. Available at: http://www.journal.viam.ru (accessed: November 23, 2022). DOI: 10.18577/2071-9140-2022-0-1-30-40.
- Peskova A.V., Sukhov D.I., Mazalov P.B. Exami-nation of the formation of the titanium alloy VT6 structure obtained by additive manufacturing. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 38–44. DOI: 10.18577/2071-9140-2020-0-1-38-44.
- Kablov E.N., Nochovnaya N.A., Panin P.V., Alekseev E.B., Novak A.V. Study of the structure and properties of heat-resistant alloys based on titanium aluminides with gadolinia microdists. Materialovedenie, 2017, no. 3, pp. 3–10.
- Skvortsova S.V., Zolotareva A.Yu. The effect of coatings on the kinetics of oxidation of intermetallic titanium alloys of the Ti2AlNb and γ-TiAl. Korroziya: materialy, zashchita, 2019, no. 5, pp. 1–7.
- Luthra K.L. Stability of protective oxide films on Ti-base alloys. Oxidation of metals, 1991, vol. 36, no. 5, pр. 475–490.
- Perkins R.A., Chiang K.T., Meier G.H. Formation of alumina on Ti–Al alloys. Scripta metallurgica, 1987, vol. 21, no. 11, pp. 1505–1510.
- Meier G.H., Pettit F.S., Hu S. Oxidation behavior of titanium aluminides. Le Journal de Physique IV, 1993, vol. 3, no. C9, pp. C9-395–C9-402.
- Rahmel A., Spencer P.J. Thermodynamic aspects of TiAl and TiSi2 oxidation: the Al–Ti–O and Si–Ti–O phase diagrams. Oxidation of Metals, 1991, vol. 35, no. 1, pp. 53–68.
- Gurappa I. Protection of titanium alloy components against high temperature corrosion. Materials Science and Engineering: А, 2003, vol. 356, no. 1–2, pp. 372–380.
- Qu S.J., Tang S.Q., Feng A.H. et al. Microstructural evolution and high-temperature oxidation mechanisms of a titanium aluminide based alloy. Acta Materialia, 2018, vol. 148, pp. 300–310. DOI: 10.1016/j.actamat.2018.02.013.
- Leyens C., Braun R., Fröhlich M. et al. Recent progress in the coating protection of gamma Titanium-Aluminides. JOM, 2006, vol. 58, pp. 17–21.
- Xiang L.L., Zhao L.L., Wang Y.L. et al. Synergistic effect of Y and Nb on the high temperature oxidation resistance of high Nb containing TiAl alloys. Intermetallics, 2012, vol. 27, pp. 6–13.
- Zavarzin S.V., Oglodkov M.S., Chesnokov D.V., Kozlov I.A. Hot corrosion and protection of materials of gas turbine engines (review). Trudy VIAM, 2018, no. 3 (109), paper no. 11. Available at: http://www.viam-works.ru (accessed: November 23, 2022). DOI: 10.18577/2307-6046-2022-0-3-121-134.
- Stringer J. High-temperature corrosion of superalloys. Materials Science and Technology, 1987, vol. 3, no. 7, pp. 482–493.
- Rapp R.A. Hot corrosion of materials: a fluxing mechanism? Corrosion science, 2002, vol. 44, no. 2, pp. 209–221.
- Lai G.Y. High-temperature corrosion and materials applications. ASM International, 2007, 461 p.
- Gurappa I. Mechanism of degradation of titanium alloy IMI 834 and its protection under hot corrosion conditions. Oxidation of metals, 2003, vol. 59, no. 3, pp. 321–322.
- Anuwar M., Jayaganthan R., Tewari V.K. et al. A study on the hot corrosion behavior of Ti–6Al–4V alloy. Materials Letters, 2007, vol. 61, no. 7, pp. 1483–1488.
- Logan H., McBee M., Bechtoldt C., Sanderson B. et al. Chemical and physical mechanisms of salt stress-corrosion cracking in the titanium 8-1-1 alloy. Stress-Corrosion Cracking of Titanium. ASTM International, 1966, pp. 215–229.
- Rideout S., Louthan M., Selby C.L. Basic mechanisms of stress-corrosion cracking of titanium. Stress-Corrosion Cracking of Titanium. ASTM International, 1966, pp. 137–151.
- Yao Z., Marek M. NaCl-induced hot corrosion of a titanium aluminide alloy. Materials Science and Engineering: A, 1995, vol. 192–193, pp. 994–1000.
- Fan L., Liu L., Yu Zh. et al. Corrosion behavior of Ti60 alloy under a solid NaCl deposit in wet oxygen flow at 600 °C. Scientific Reports, 2016, vol. 6, art. 29019. DOI: 10.1038/srep29019.
- Ciszaka C., Popaa I., Brossardb J.-M. et al. NaCl induced corrosion of Ti–6Al–4V alloy at high temperature. Corrosion Science, 2016, vol. 110, pp. 91–104.
- Zimm B.H., Mayer J.E. Vapor pressures, heats of vaporization, and entropies of some alkali halides. The Journal of Chemical Physics, 1944, vol. 12, pp. 362–369. DOI: 10.1063/1.1723958.
- Ewing C.T., Stern K.H. Equilibrium vaporization rates and vapor pressures of solid and liquid sodium chloride, potassium chloride, potassium bromide, cesium iodide, and lithium fluoride. The Journal of Physical Chemistry, 1974, vol. 78, no. 20, pp. 1998–2005. DOI: 10.1021/j100613a005.
- Chen L., Jin X., Pang P. et al. Electrochemical Study of TA2 Titanium in a High-Temperature and Pressure Water Environment. Coatings, 2021, vol. 11, no. 6, art. 659. DOI: 10.3390/coatings11060659.
- Mckay P., Mitton D.B. An electrochemical investigation of localized corrosion on titanium in chloride environments. Corrosion, 1985, vol. 41, no. 1, рр. 52–62.