Criteria for evaluating the quality of defectoscopic materials in penetrant testing (review)

Skorobogatko D.S., Golovkov A.N., Kudinov I.I., Kulichkova S.I.
Skorobogatko D.S., Golovkov A.N., Kudinov I.I., Kulichkova S.I. Criteria for evaluating the quality of defectoscopic materials in penetrant testing (review) // Proceedings of VIAM. 2023. No. 4. DOI: 10.18577/2307-6046-2023-0-4-128-136. URL: https://viam-works.ru/en/journal/2023/4/12
Keywords
non-destructive testing, penetrant testing, quality of defectoscopical materials, penetrant testing technology, reveal ability
Abstract

A review of the physicochemical properties of defectoscopic materials that affect the results of penetrant testing has been carried out. The rationale for the need to determine and verify each parameter of a set of defectoscopic materials is presented. The properties of the components of the kits that are not specified in the quality certificates and manufacturer's certificates are considered. It has been established that the characteristics and properties specified in the technical documentation of the manufacturer are not enough to assess the quality of defectoscopic materials. Parameters for quality assessment are proposed, which will allow choosing the most technologically advanced modern sets of defectoscopic materials.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Modern materials – the basis of innovative modernization of Russia. Metally Evrazii, 2012, no. 3, pp. 10–15.
  3. Kablov E.N. Russia in the market of intellectual resources. Ekspert, 2015, no. 28 (951), pp. 48–51.
  4. Skorobogatko D.S., Golovkov A.N., Kudinov I.I., Kulichkova S.I. Revisiting the ecotoxicity and efficiency of different classes of industrial nonionic surfaces used for cleaning metal surfaces in the process of capillary control of details of the aviation technology (review). Aviation materials and technologies, 2021, no. 4 (65), paper no. 11. Available at: http://www.journal.viam.ru (accessed: May 17, 2022). DOI: 10.18577/2713-0193-2021-0-4-98-106.
  5. Klyuev V.V., Evlampiev A.I., Popov E.D. et al. Non-destructive control and diagnostics: a reference book. Moscow: Mashinostroenie, 2003, 656 p..
  6. Karyakin A.V., Borovikov A.S. Luminescent and color flaw detection. Moscow: Mashinostroenie, 1972, 240 p.
  7. State Standard 18442-80. Unbrakable control. capillary methods. Moscow: Publishing house of standards, 1987, 24 p.
  8. Prokhorenko P., Migun N., Dezhkunov N. Development of penetrant test theory based on new physical effects. Proceedings of the 13th World Conference of Non-Destructive Testing (Sao Paulo, Brazil, October 18–23, 1992), 1992, pp. 538–542. DOI: 10.1016/B978-0-444-89791-6/50116-5.
  9. Prokhorenko P., Migun N. Quantitative model of liquid penetrant hydrodynamics. AIP Conference Proceedings, 2000, vol. 509, is. 1, pp. 1865. DOI: 10.1063/1.1306257.
  10. Gulak Y., Braido D. Capillary models of solvent diffusion. Chemical Engineering Science, 2013, vol. 101, is. 20, pp. 515–522. DOI: 10.1016/j.ces.2013.07.016.
  11. Prokhorenko P., Migoun N. Calculation of Penetrant Testing Sensibility for Powder Developer. Proceeding of the 4th European Conference (London, UK, September 13–17, 1987), 1992, pp. 2774–2782. DOI: 10.1016/B978-0-08-036221-2.50071-1.
  12. Prokhorenko P., Migun N., Grebenshchikov S. Experimental studies of polar indicator liquids used in capillary penetrant testing. International Journal of Engineering Science, 1987, vol. 25, is. 7, pp. 769–773.
  13. Beril A. Capillarity effect analysis for alternative liquid penetrant chemicals. NDT & E International, 1997, vol. 30, is. 1, pp. 19–23. DOI: 10.1016/S0963-8695(96)00044-8.
  14. Krasnov I.S., Lozhkova D.S., Dalin M.A. Evaluation of deficiency of titanium alloy forgings for probabilistic calculation of gas turbine engine disks fracture risk. Aviation materials and technologies, 2021, no. 2 (63), paper no. 12. Available at: https://journal.viam.ru (accessed: November 11, 2022). DOI: 10.18577/2713-0193-2021-0-2-115-122.
  15. Lobanova I., Kalinichenko A. Investigation of the Liquid Flow on Rough Surfaces to Solve the Problems of Liquid Penetrant Testing. Progress in Material Science and Engineering. Springer International Publishing Switzerland, 2021, pp. 89–99. DOI: 10.1007/978-3-030-68103-6-9.
  16. Prokhorenko P., Migun N. Film-flow mechanism of flaw development in penetrant-dye test. Russian Journal of Nondestructive testing, 2002, vol. 38, pp. 704–708.
  17. Deutsch S. A Preliminary Study of the Fluid Mechanics of Liquid Penetrant Testing. Journal of Research of the National Bureau of Standards, 1977, vol. 84, is. 4, pp. 287–292. DOI: 10.6028/jres.084.012.
  18. Migoun N., Prokhorenko P., Gnusin A. et al. On the reliability of quantitative evaluation of penetrant systems quality. AIP Conference Proceedings, 2002, vol. 615, pp. 1991–1996. DOI: 10.1063/1.1473037.
  19. Prokhorenko P., Migoun N., Stadthaus S. Quantitative model of liquid penetrant hydrodynamics. AIP Conference Proceedings, 2000, vol. 509, pp. 1865. DOI: 10.1063/1.1306257.
  20. Zolfaghari A., Kolahan F. Reliability and sensitivity of visible liquid penetrant NDT for inspection of welded components. Material Testing, 2017, vol. 59, is. 3, pp. 290–294. DOI: 10.3139/120.111000.
  21. Kulichkova S.I., Golovkov A.N., Kudinov I.I., Laptev A.S. Modern flaw detection materials, equipment and automation of the process of capillary non-destructive testing. Kontrol. Diagnostika, 2019, no. 2, pp. 52–57. DOI: 10.14489/td.2019.02.pp 052-057.
  22. Loshchinin Yu.V., Pakhomkin S.I., Razmakhov M.G. Phase transformation temperatures and calorimetric analysis of powder compositions of nickel-based superalloys. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 79–85. DOI: 10.18577/2071-9140-2020-0-1-79-85.
  23. Evgenov A.G., Shurtakov S.V., Prager S.M., Malinin R.Yu. On the development of a universal calculation method for assessing the degradation of recycled metal powder materials, depending on the cyclicity of use in the selective laser melting process. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 3–11. DOI: 10.18577/2071-9140-2020-0-4-3-11.