Investigation of deformation hardening tendency and to changes in corrosion resistance depending on the quenching temperature of 12Kh14AMF steel with a superequilibrium nitrogen content
1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru
2Federal State Budgetary Institution of Science «Institute of Metallurgy and Material Science of A.A. Baikov», Russian Academy of Sciences, Moscow, Russia; imet@imet.ac.ru
A comprehensive study was conducted to examine the effect of quenching temperature (900–1100 °C) on the structure, mechanical properties, strain hardening, and corrosion resistance of high-nitrogen martensitic steel grade 12Kh14AMF with a super-equilibrium nitrogen content, produced by electroslag remelting under nitrogen pressure. It was found that quenching from 1050 °C provides an optimal combination of properties: tensile strength, hardening index, hardening life and corrosion current in a 3.5% NaCl solution.
- Erasov V. S., Oreshko E. I. Mechanical testing and properties of structural aviation metallic materials: textbook / ed. by E. N. Kablov. Moscow: NRC «Kurchatov Institute» – VIAM, 2023. 344 p.
- Erasov V. S., Sibaev I. G. Scheme for development and evaluation of properties of structural aviation composite materials // Aviation materials and technologies. 2023. No. 1 (70). P. 61–81. URL: http://www.journal.viam.ru (accessed: 25.02.2026). DOI: 10.18577/2713-0193-2023-0-1-61-81.
- Gorbovets M. A., Khodinev I. A., Monin S. A. Testing of structural metallic materials for fatigue crack growth rate in a corrosion-active environment (review) // Trudy VIAM. 2022. No. 12 (118). P. 135–144. URL: http://www.viam-works.ru (accessed: 25.02.2026). DOI: 10.18577/2307-6046-2022-0-12-135-144.
- Marakhovsky P. S., Barinov D. Ya., Shorstov S. Yu., Vorobyov N. N. The issue of creating physical and mathematical models of heat and mass transfer in the manufacture of parts by additive technologies (review) // Aviation materials and technologies. 2022. No. 2 (67). P. 111–119. URL: http://www.journal.viam.ru (accessed: 25.02.2026). DOI: 10.18577/2713-0193-2022-0-2-111-119.
- Gorbovets M. A., Khodinev I. A., Karashaev M. M., Ryzhkov P. V. Low-cycle fatigue tests with hold in the cycle of heat-resistant metallic materials (review) // Trudy VIAM. 2022. No. 5 (111). P. 123–137. URL: http://www.viam-works.ru (accessed: 25.02.2026). DOI: 10.18577/2307-6046-2022-0-5-123-137.
- Khodinev I. A., Baranova E. V. Fatigue durability of a heat-resistant titanium alloy at various loading frequencies // Trudy VIAM. 2024. No. 9 (139). P. 71–82. URL: http://www.viam-works.ru (accessed: 25.02.2026). DOI: 10.18577/2307-6046-2024-0-9-71-82.
- Antipov V. V., Medvedev I. M., Kutyrev A. E., Zhitnyuk S. V. Study of electrochemical properties of unfilled anodic oxide coatings on aluminum alloys of grades 1163, V-1461 and V96Ts3p.ch. under accelerated tests // Trudy VIAM. 2019. No. 6 (78). P. 51–64. URL: http://www.viam-works.ru (accessed: 25.02.2026). DOI: 10.18577/2307-6046-2019-0-6-51-64.
- Fomina M. A., Zavarzin S. V., Demin S. A. Study of corrosion resistance of aluminum samples from alloy 1163-AT with electrically conductive galvanic coatings in contact with carbon fiber reinforced plastic VKU-39/VTkU-2.200 // Trudy VIAM. 2023. No. 10 (128). P. 96–104. URL: http://www.viam-works.ru (accessed: 25.02.2026). DOI: 10.18577/2307-6046-2023-0-10-96-104.
- Kravchenko D. V., Kozlov I. A., Nikiforov A. A., Tolmachev Ya. V. Influence of surface preparation methods of aluminum alloy 1163-AT on adhesion of galvanic coatings // Trudy VIAM. 2022. No. 7 (113). P. 74–88. URL: http://www.viam-works.ru (accessed: 25.02.2026). DOI: 10.18577/2307-6046-2022-0-7-74-88.
- Krylov S. A., Evgenov A. G., Shcherbakov A. I., Makarov A. A. New electroslag pressure furnace DEShP-0.1: development and prospects // Trudy VIAM. 2016. No. 5 (41). P. 28–35. URL: http://www.viam-works.ru (accessed: 25.02.2026). DOI: 10.18577/2307-6046-2016-0-5-4-4.
- Bakradze M. M., Voznesenskaya N. M., Leonov A. V., Krylov S. A., Tonysheva O. A. Development and study of high-strength corrosion-resistant steel for bearing parts // Metallurg. 2019. No. 11. P. 39–44.
- Blinov V. M., Elistratov A. V., Kolesnikov A. G. et al. Influence of heat treatment on structural transformations and properties of high-nitrogen chromium steels // Metal Science and Heat Treatment. 2000. No. 6. P. 19–24.
- Sevalnev G. S., Vlasov I. I., Dulnev K. V. et al. Study of wear resistance and contact endurance of high-carbon and high-nitrogen steels after chemical-thermal and thermal treatment // Physical-mechanical testing, strength and reliability of modern structural and functional materials: proceedings of the XIV All-Russian conference on testing and research of material properties «TestMat». Moscow, 2022. P. 109–122.
- Rashev Ts. V. High-nitrogen steels. Metallurgy under pressure. Sofia: Publishing house «Prof. Marin Drinov», 1995. 268 p.
- Kostina M. V., Bannykh O. A., Blinov V. M. Features of steels alloyed with nitrogen // Metal Science and Heat Treatment. 2000. No. 12. P. 3–6.
- Rigina L. G. Research and development of ESR and ESRP of chromium-manganese steels alloyed with nitrogen: PhD thesis. Moscow, 2005. 149 p.
- Korobova E. N., Sevalnev G. S., Gromov V. I., Leonov A. V. Steels for the manufacture of special-purpose rolling bearings (review) // Trudy VIAM. 2021. No. 11 (105). P. 3–11. URL: http://www.viam-works.ru (accessed: 25.02.2026). DOI: 10.18577/2307-6046-2021-0-11-3-11.
- Gerasimov S. A., Kuksenova L. I., Lapteva V. G., Ospennikova O. G., Alekseeva M. S., Gromov V. I. Surface engineering and operational properties of nitrided structural steels: textbook / ed. by E. N. Kablov. Moscow: VIAM, 2019. 600 p.
- Hollomon J. H. Tensile deformation // Transactions of the Metallurgical Society of AIME. 1945. Vol. 162. P. 268–290.
- Johnson G. R., Cook W. H. A constitutive model and data for metals subjected to large strains, high strain rates and high temperatures // Proceedings 7th International Symposium on Ballistics. Hague, 1983. P. 541–547.
- Umbrello D., M'Saoubi R., Outeiro J. C. The influence of Johnson–Cook material constants on finite element simulation of machining of AISI 316L steel // International Journal of Machine Tools and Manufacture. 2007. Vol. 47. No. 3–4. P. 462–470. DOI: 10.1016/j.ijmachtools.2006.06.006.
- Sevalnev G. S., Sevalneva T. G., Kolmakov A. G., Dulnev K. V., Krylov S. A. Study of tribotechnical characteristics of corrosion-resistant steels with different mechanisms of bulk hardening // Trudy VIAM. 2021. No. 10 (104). P. 3–11. URL: http://www.viam-works.ru (accessed: 25.02.2026). DOI: 10.18577/2307-6046-2021-0-10-3-11.
- Berns H., Ehrhardt R. Carbon or nitrogen alloyed quenched and tempered stainless steel – comparative study // Steel Research. 1996. Vol. 67. No. 8. P. 343–349.
- Gavrilyuk V. G. Carbon, nitrogen and hydrogen in steels: ductility and brittleness // Izvestiya vysshikh uchebnykh zavedeniy. Chernaya metallurgiya. 2015. Vol. 58. No. 10. P. 761–768. DOI: 10.17073/0368-0797-2015-10-761-768.
- Kostina M. V. Development of principles of alloying Cr-N steels and creation of new-generation corrosion-resistant steels with a structure of nitrogen martensite and austenite for highly loaded products of modern technology: abstract of doctoral thesis. Moscow, 2003. 42 p.
- Berns H., Escher C., Streich W. D. Martensitic high nitrogen steel for applications at elevated temperature // Materials science forum. Transaction Technical Publications Ltd., 1999. Vol. 318. P. 443–448.
- Cottrell A. H., Bilby B. A. Dislocation theory of yielding and strain ageing of iron // Proceedings of the Physical Society A. 1949. Vol. 62. P. 49–62.
- Blinov V. M., Lukin E. I., Blinov E. V., Samoilova M. A., Sevalnev G. S. Features of fracture under tension of corrosion-resistant austenitic steels with super-equilibrium nitrogen content // Deformation and fracture of materials. 2021. No. 4. P. 10–14. DOI: 10.31044/1814-4632-2021-4-10-14.
- Kablov E. N. Innovative developments of FSUE «VIAM» SSC RF for the implementation of «Strategic directions for the development of materials and technologies for their processing for the period up to 2030» // Aviation materials and technologies. 2015. No. 1 (34). P. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.