D. N. Shafiev, A. I. Tkachuk, E. S. Suvorova, G. B. Eldyaeva, A. V. Kovalenko, N. K. Sidelnikov Study of the kinetic regularities of the curing reaction of spheroplastic VPZ-25 and changes in its physical and mechanical characteristics after heat and humidity exposure // Proceedings of VIAM. 2026. No. 11 (165). С. 99-109. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-11-99-109.

Study of the kinetic regularities of the curing reaction of spheroplastic VPZ-25 and changes in its physical and mechanical characteristics after heat and humidity exposure

D. N. Shafiev1, A. I. Tkachuk1, E. S. Suvorova1, G. B. Eldyaeva1, A. V. Kovalenko1, N. K. Sidelnikov1

1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru

Abstract

The article provides the review of characteristics of the VPZ-25 syntactic polymer filler developed at the NRC «Kurchatov Institute» - VIAM considering climatic tests and kinetics patterns. The paper presents the results of a study of the characteristics of samples of VPZ-25 cold-curing syntactic polymer filler after climatic tests. Kinetic studies were conducted using the differential scanning calorimetry (DSC). Based on the research results, conclusions were drawn regarding the possibility of using this spheroplastic under conditions of elevated humidity and temperature, as well as its application in aircraft interiors.

Keywords
spheroplastic, syntactic filler, epoxy binder, honeycomb panels, cold curing, glass microspheres, aviation, shipbuilding, climatic tests, tropical resistance, fire safety



Reference list
  1. Syntactic foam market forecast and company analysis report 2025‒2030, featuring case studies of AIS, CMT, Europe and Trelleborg. Available at: https://www. Valuespectrum.com/corporate_news/1299852-syntactic-foam-market-forecast-and-company-analysis-report-2025-2030-featuring-case-studies-of-aiscm-Europe-and-relleborg (accessed: August 15, 2026).
  2. Syntactic foam market report 2025‒2030. Available at: https://www.marketsandmarkets.com/Markets-Report/syntactic-foam-market-49852579.html?utm_campaign=Linkedin/RamS/CHSF&utm_medium=RamS/CH/SF&utm_source=Linkedin (accessed: August 15, 2026).
  3. Baykov A.V. Elastic parameters of synact composites based on hollow glass microspheres: thesis, Cand. Sc. (Tech.). Moscow, 2023, 108 p.
  4. Global polymer matrix syntactic foam market 2025 by manufacturers, regions, type and applicatoin, forecast 2031. Available at: https://www.marketresearch.com/GlobalInfoResearchv4117/Global-Polymer-Matrix-Syntactic-Foam-42607736/ (accessed: August 16, 2026).
  5. Zastrogina O.B., Dolmatovsky M.G., Shvets N.I., Minakov V.T., Barbotko S.L. Cold-curing spheroplasts with reduced flammability and smoke generation. Aviatsionnye materialy i tekhnologii, 2005, no. 2, pp. 55–61.
  6. Мodern problems of a scienceand educations. Available at: https://scienceeducation.ru/article/view?id=6547 (accessed: August 16, 2026).
  7. Anirudh S., Jayalakshmi C.G., Anand A. et al. Ismail.Epoxy/hollow glass microsphere syntactic foams for structural and functional application-A review. European Polymer Journal, 2022, vol. 171, p. 111163. DOI: 10.1016/j.eurpolymj.2022.111163.
  8. Galvagnini F., Fredi G., Dorigato A. et al. Mechanical Behaviour of Multifunctional Epoxy/Hollow Glass Microspheres/Paraffin Microcapsules Syntactic Foams for Thermal Management. Plumers, 2021, no. 13 (17), p. 2896. DOI: 10.3390/polym13172896.
  9. Kaur M., Jayakumari L.S. Eco‐friendly cardanol‐based phenalkamine cured epoxy‐cenosphere syntactic foams: Fabrication and characterisation. Journal of Applied Polymer Science, 2016, vol. 133, p. 44189. DOI: 10.1002/app.44189.
  10. Kaur M., Jayakumari L.S. Novel bio-based epoxidized cardanol/cenosphere syntactic foams. High Performance Polymers, 2016, vol. 29 (7), pp. 785–796. DOI: 10.1177/0954008316656923.
  11. Kapustianskaia M.A., Lyubimova A.S., Kovalenko A.V., Sidelnikov N.K., Tkachuk A.I., Slavin A.V. Development of a cold-curing polymer syntatic filler with enhanced physico-mechanical properties. Trudy VIAM, 2024, no. 11 (141), pp. 33–43. Available at: http://www.viam-works.ru (accessed: August 16, 2026). DOI: 10.18577/2307-6046-2024-0-11-33-43.
  12. Kopylov A.V., Kovalenko A.V., Sidelnikov N.K., Kurnosov A.O., Slavin A.V. Studying the characteristics of VPZ-25 cold-curing polymer filler and developing a technology for filling honeycomb panels for aircraft components. Trudy VIAM, 2025, no. 12 (154), pp. 37–52. Available at: http://www.viam-works.ru (accessed: August 16, 2026). DOI: 10.18577/2307-6046-2025-0-12-37-52.
  13. Method for producing a binder for a prepreg (variants), binder for a prepreg (variants), prepreg, and article: pat. 2420547С2 Rus. Federation; appl. 26.03.09; publ. 10.06.11.
  14. Epoxy composition for fiberglass-reinforced plastics: pat. 2172328С2 Rus. Federation; appl. 06.08.99; publ. 20.08.01.
  15. Epoxy resin composition, prepreg, and fiber-reinforced composite material: pat. EP 2154171A1; appl. 12.05.08; publ. 04.05.16.
  16. Quick cure carbon fiber reinforced epoxy resin: pat. US 7005185B2; appl. 27.11.02; publ. 28.02.06.
  17. Epoxy resin composition for carbon-fiber-reinforced composite material, prepreg, integrated molding, fiber-reinforced composite sheet, and casing for electrical/electronic equipment: pat. US 2008166511A1; appl. 24.02.05; publ. 02.10.14.
  18. Manufacturing method of fiber reinforced composite material molded article: pat. JP 4603978B2; appl. 28.11.03; publ. 23.03.06.
  19. Matrix resin composition: pat. GB 2427196A; appl. 24.06.06; publ. 28.10.09.
  20. Kablov E.N., Startsev V.O., Laptev A.B. Aging of Polymer Composite Materials: A Textbook. Moscow: NRC «Kurchatov Institute» – VIAM, 2023, pp. 18–21.
  21. Lyubimova A.S., Tkachuk A.I., Kuznetsova P.A. Shape memory epoxy polymers. Trudy VIAM, 2024, no. 4 (134), pp. 50–63. Available at: http://www.viam-works.ru (accessed: August 18, 2026). DOI: 10.18577/2307-6046-2024-0-4-50-63.
  22. Vakhrusheva Ya.A., Tkachuk A.I., Afanaseva E.A., Kurshev E.V., Lonskii S.L. Perspective epoxy resin system VSE-81 for incoming quality inspection of carbon fiber. Trudy VIAM, 2026, no. 6 (160), pp. 96–107. Available at: http://www.viam-works.ru (accessed: August 18, 2026). DOI: 10.18577/2307-6046-2026-0-6-96-107.