Abstract

The article is devoted to a theoretical study of chemical reactions occurring during thermal decomposition of an isolated methyldichlorosilane molecule. The most probable chemical reactions of methyldichlorosilane decomposition and the mechanisms of their occurrence were determined. Using the quantum chemistry method thermodynamic were calculated characteristics of products and transition structures at different temperatures. The reaction rate constants at different temperatures have been also calculated.

Keywords
methyldichlorosilane, pyrolytic decomposition, transition state, thermodynamic characteristics, quantum chemistry, reaction rate



Reference list
  1. Akchurin R.Kh., Marmalyuk A.A. MOS hydride epitaxy in photonics and electronics materials technology. Moscow: Tekhnosfera, 2018, 488 p.
  2. Latha H., Udayakumar A., Prasad V. Microstructure and electrical properties of nitrogen doped 3C–SiC thin films deposited using methyltrichlorosilane. Materials science in semiconductor processing, 2015, vol. 29, pp. 117–123.
  3. Reznik B., Gerthsen D., Zhang W., Huttinger G. Microstructure of SiC deposited from methyltrichlorosilane. Journal of the European ceramic society, 2003, vol. 23, pp. 1499–1508.
  4. Pakula D., Marciniec B., Przekop R. Direct synthesis of silicon compounds – from the beginning to green chemistry revolution. AppliedChem, 2023, vol. 3, pp. 89–109.
  5. Sidorov D.V., Schavnev A.A., Melentev A.A. Formation of silicon carbide coatings by chemical vapor deposition (review). Part 2. Trudy VIAM, 2022, no. 2 (108), pp. 88–98. Available at: http://www.viam-works.ru (accessed: March 16, 2026). DOI: 10.18577/2307-6046-2022-0-2-88-98.
  6. Zhang W., Huttinger G. CVD of SiC from methyltrichlorosilane. Part II: composition of the gas phase and the deposit. Chemical vapor deposition, 2001, vol. 7, pp. 173–181.
  7. Osterheld T., Allendorf M., Melius C. Unimolecular decomposition of methyltrichlorosilane: RRKM calculatios. Journal of physical chemistry, 1994, vol. 98, p. 6995.
  8. Ge Y., Gordon M., Battaglia F. et al. Theoretical study of the pyrolysis of methyltrichlorosilane in the gas phase. 3. Reaction rate constant calculations. The Journal of Physical Chemistry A, 2010, vol. 114, pp. 2384–2392.
  9. Cagliostro D., Riccitiello S., Carswell M. Analysis of the pyrolysis products of dimethyldichlorosilane in the chemical vapor deposition of silicon carbide in argon. Journal of the American ceramic society, 1990, vol. 73, pp. 607–614.
  10. Cagliostro D., Riccitiello S., Ren J. et al. Comparison of the pyrolysis products of dichlorodimethylsilane in the chemical vapor deposition of silicon carbide on silica in hydrogen or argon. Journal of the American ceramic society, 1994, vol. 77, pp. 2721–2726.
  11. Cagliostro D., Riccitiello S. Model for the formation of silicon carbide from the pyrolysis of dichlorodimethylsilane in hydrogen: I, silicon formation from chlorosilanes. Journal of the American ceramic society, 1993, vol. 76, pp. 39–48.
  12. Shao K., Brunson J., Tian Y., Zhang J. Analysis of the pyrolysis products of dimethyldichlorosilane in the chemical vapor deposition of silicon carbide in argon. Journal of the American ceramic society, 1990, vol. 73, pp. 607–614.
  13. Shao K., Zhang J., Liu X. Thermal Decomposition Mechanism of Tetraethylsilane by Flash Pyrolysis Vacuum Ultraviolet Photoionization Mass Spectrometry and DFT Calculations: The Competition between β-Hydride Elimination and Bond Homolysis. The Journal of Physical Chemistry A, 2023, vol. 127, p. 18. DOI: 10.1021/acs.jpca.2c09081.
  14. Shao K., Tian Y., Zhang J. Thermal decomposition mechanism of allyltrichlorosilane and allyltrimethylsilane. International Journal of Mass Spectrometry, 2021, vol. 460, p. 116476. DOI: 10.1016/j.ijms.2020.116476.
  15. Lemieux J., Zhang J. Thermal decomposition of methyltrichlorosilane, dimethyldichlorosilane and methyldichlorosilane by flash pyrolysis vacuum ultraviolet photoionization time-of-flight mass spectrometry. European journal of mass spectrometry, 2014, vol. 20, pp. 409–417.
  16. Shchegoleva N.E., Evdokimov S.A., Vershinin D.I., Kholodova V.V., Vaganova M.L., Chaynikova A.S. Silicon nitride based ceramics as a promising material for hybrid bearings. Aviation materials and technologies, 2026, no. 2 (83), pp. 145–159. Available at: http://www.journal.viam.ru (accessed: June 01, 2026). DOI: 10.18577/2071-9140-2026-0-2-145-159.
  17. Sidorov D.V., Grunin A.A., Kirilin A.D., Shavnev A.A. The first step of the pyrolytic decomposition of methylchlorosilane. Khimicheskaya tekhnologiya, 2025, vol. 26, no. 1, pp. 26–33.
  18. Sidorov D.V., Grunin А.А., Schavnev А.А. Rate of chemical reaction of formation of 1,2-dimethyldisilene from methylsilylene. Trudy VIAM, 2025, no. 5 (147), pp. 76–87. Available at: http://www.viam-works.ru (accessed: April 14, 2026). DOI: 10.18577/2307-6046-2025-0-5-76-87.
  19. Ochterski J.W. Thermochemistry in Gaussian. Gaussian Inc., 2000, 19 р.
  20. Chorkendorff I., Niemantsverdriet H. Modern Catalysis and Chemical Kinetics. Dolgoprudny: Intellekt, 2010, 504 p.
  21. Bespalov A.S. Aluminum oxide-based catalyst carriers. Trudy VIAM, 2026, no. 6 (160), pp. 108–117. Available at: http://www.viam-works.ru (accessed: June 30, 2026). DOI: 10.18577/2307-6046-2026-0-6-108-117.