UDC
579.26:678.8
DOI
10.18577/2307-6046-2026-0-11-180-188
Article PDF (Russian)
(951.27 KB)
How to cite
A. A. Krivushina, D. N. Mosunova, Yu. S. Goryashnik, T. V. Yakovenko Microscopic fungi on polymeric materials in different climatic zones // Proceedings of VIAM. 2026. No. 11 (165). С. 180-188. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-11-180-188.
Microscopic fungi on polymeric materials in different climatic zones
1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru
Abstract
Data on the species composition of microscopic fungi isolated from polymeric materials in various climatic regions were analyzed and summarized. More than 250 microscopic fungal strains belonging to 98 species and 36 genera were isolated, most of them anamorphs of the Ascomycota phylum. The isolated strains hold promise for studies of the microbiological stability of materials and the effectiveness of biocidal agents used in various climatic regions.
Keywords
biodeterioration, climatic zones, micromycetes-destructors, micromycetes-contaminants, microscopic fungi, polymers
Reference list
- Krivushina A.A., Startsev V.O. Micromycetes-destructors of polymeric materials among extremophilic microorganisms (review). Trudy VIAM, 2022, no. 1 (107), pp. 123–134. Available at: http://www.viam-works.ru (accessed: March 29, 2026). DOI: 10.18577/2307-6046-2022-0-1-123-134.
- Laptev A.B., Zheleznyak V.G., Tourova T.P., Sokolova D.Sh., Nazina T.N. The effect of the presence of toxic additives in the polymer material on the processes of its biodegradation in seawater. Trudy VIAM, 2022, no. 12 (118), pp. 121–134. Available at: http://www.viam-works.ru (accessed: March 29, 2026). DOI: 10.18577/2307-6046-2022-0-12-121-134.
- Zakirova L.I., Afanasyev-Khodykin A.N., Movenko D.A., Laptev A.B. Features of the formation of the Sn–Zn–Fe diffusion layer at the boundary of galvanothermal coating of systems zinc–tin and 30HGSA steel with high protective capability. Aviation materials and technologies, 2022, no. 4 (69), pp. 61–71. Available at: http://www.journal.viam.ru (accessed: March 29, 2026). DOI: 10.18577/2713-0193-2022-0-4-61-71.
- Kurakov A.V., Gevorkyan S.A., Goginyan V.B., Ozerskaya S.M. Diversity and compositional features of microscopic fungi on synthetic polymeric materials. Prikladnaya biokhimiya i mikrobiologiya, 2008, vol. 44, no. 2, pp. 232–235.
- Srikanth M., Sandeep T.S.R.S., Sucharitha K., Godi S. Biodegradation of plastic polymers by fungi: a brief review. Bioresources and Bioprocessing, 2022, vol. 9 (1), p. 42. DOI: 10.1186/s40643-022-00532-4.
- Krivushina A.A., Laptev A.B. Fungicides: application, properties and principles of action. Aviation materials and technologies, 2024, no. 1 (74), pp. 155–168. Available at: http://www.journal.viam.ru (accessed: March 20, 2026). DOI: 10.18577/2713-0193-2024-0-1-155-168.
- Krivushina A.A., Laptev A.B. Methods for testing the efficiency of biocidal agents (review). Aviation materials and technologies, 2026, no. 1 (82), pp. 267–278. Available at: http://www.journal.viam.ru (accessed: March 20, 2026). DOI: 10.18577/2713-0193-2026-0-1-267-278.
- State Standard 16350–80. Climate of the USSR. Zoning and Statistical Parameters of Climatic Factors for Technical Purposes. Moscow: Standards Publ. House, 1981, 140 p.
- Startsev V.O., Startsev O.V., Zeleneva T.O., Vardanyan A.M. Influence of precipitation on changes in the mass of samples of polymeric composite materials in open climatic conditions. Aviation materials and technologies, 2024, no. 1 (74), pp. 136–154. Available at: http://www.journal.viam.ru (accessed: March 20, 2026). DOI: 10.18577/2713-0193-2024-0-1-136-154.
- State Standard 9.915–2023. Unified System for Protection against Corrosion and Aging. Non-metallic Materials and Products Incorporating Them. Test Method for Microbiological Resistance under Natural Atmospheric Conditions. Moscow: RST, 2023, 12 p.
- Kablov E.N., Antipov V.V. The Role of New-Generation Materials in Ensuring the Technological Sovereignty of the Russian Federation. Vestnik Rossiyskoy akademii nauk, 2023, vol. 93, no. 10, pp. 907–916. DOI: 10.31857/S0869587323100055.
- Lugauskas A., Levinskait L., Pečiulyt D. Micromycetes as deterioration agents of polymeric materials. International biodeterioration & biodegradation, 2003, vol. 52 (4), pp. 233–242.
- Domsch K.H., Gams W., Anderson T.H. Compendium of Soil Fungi. 2nd ed. Lubrecht & Cramer Ltd., 2007, 672 p.
- Seifert K., Morgan-Jones G., Gams W., Kendrick B. The Genera of Hyphomycetes. CBS Biodiversity. Series 9. Utrecht, 2011, pp. 1–102.
- Sabev H.A., Barratt S.M., Greenhalgh M. et al. Biodegradation and biodeterioration of man-made polymeric materials. Fungi in biogeochemical cycles. Ed. G.M. Gadd. Cambridge University Press, 2006, pp. 212–235.
- Gao R., Liu R., Sun C. A marine fungus Alternaria alternata FB1 efficiently degrades polyethylene. Journal of Hazardous Materials, 2022, vol. 431, p. 128617. DOI: 10.1016/j.jhazmat.2022.128617.
- Schindler Y., Zucker I. Microplastic Removal and Biodegradation by Native Mediterranean Fungus Alternaria alternate. ACS Environmental Science & Technology Water, 2025, vol. 5, pp. 4079–4088.
- Bensch K., Groenewald J.Z., Dijksterhuis J. et al. Species and ecological diversity within the Cladosporium cladosporioides complex (Davidiellaceae, Capnodiales). Studies in mycology, 2010, vol. 67, pp. 1–94. DOI: 10.3114/sim.2010.67.01.
- Lugauskas A., Prosychevas I., Levinskaitė L., Jaskelevičius B. Physical and chemical aspects of long‐term biodeterioration of some polymers and composites. Environmental Toxicology: An International Journal, 2004, vol. 19 (4), pp. 318–328.
- Stroganov V.F., Kukoleva D.A., Akhmetshin A.S., Stroganov I.V. Biodeterioration of polymers and polymer composite materials. Polymer Science. Series D, 2009, vol. 2 (3), pp. 164–166. DOI: 10.1134/S1995421209030071.
The article was submitted
2026-07-16
approved and accepted for publication after reviewing
2026-08-04