Change of parameters of elasto-plastic deformation for LCF testing Ni-base superalloy VZh175
UDC
669.018.44:669.245
DOI
10.18577/2307-6046-2015-0-12-4-4
Article PDF (Russian)
(540.34 KB)
How to cite
Belyaev M.S., Gorbovets M.A., Bakradze M.M. Change of parameters of elasto-plastic deformation for LCF testing Ni-base superalloy VZh175 // Proceedings of VIAM. 2015. No. 12. DOI: 10.18577/2307-6046-2015-0-12-4-4. URL: https://viam-works.ru/en/journal/2015/12/4
Keywords
low-cycle fatigue (LCF), alteration curves of cyclic stress, elastic-plastic hysteresis, Ni-base superalloy VZh175.
Abstract
The LCF behavior for Ni-base superalloy VZh175 was investigated for a given total strain, ratio R=0 and stain amplitude εa=0,4–0,6% at test temperatures 20 and 650°С. Parameters of elastic-plastic strain were observed in this article.
Reference list
- Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokoleniya [Nickel foundry heat resisting alloys of new generation] //Aviacionnye materialy i tehnologii. 2012. №S. C. 36–52.
- Birger I.A., Balashov B.F., Dulnev R.A. i dr. Konstrukcionnaja prochnost materialov i detalej gazoturbinnyh dvigatelej [Constructional durability of materials and details of gas turbine engines]. M.: Mashinostroenie. 1981. 222 s.
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
- Inozemtsev A.A., Ratchiev A.M., Nihamkin M.Sh. i dr. Malociklovaja ustalost i ciklicheskaya treshhinostojkost nikelevogo splava pri nagruzhenii, harakternom dlya diskov turbin [Low-cyclic fatigue and cyclic crack firmness of nickel alloy when loading, characteristic for disks of turbines] //Tuazheloe mashinostroenie. 2011. №4. S. 30–33.
- Schijve J. Fatigue of structures and materials. Berlin Heidelberg: Springer-Verlag. 2009. 185 p.
- Kablov E.N., Lomberg B.S., Ospennikova O.G. Sozdanie sovremennyh zharoprochnyh materialov i tehnologij ih proizvodstva dlya aviacionnogo dvigatelestroeniya [Creation of modern heat resisting materials and technologies of their production for aviation engine building] //Krylya Rodiny. 2012. №3–4. S. 34–38.
- Kablov E.N., Ospennikova O.G., Lomberg B.S., Sidorov V.V. Prioritetnye napravleniya razvitiya tehnologij proizvodstva zharoprochnyh materialov dlya aviacionnogo dvigatelestroeniya [The priority directions of development of production technologies of heat resisting materials for aviation engine building] //Problemy chernoj metallurgii i materialovedenija. 2013. №3. S. 47–54.
- Sposob polucheniya izdeliya iz deformiruemogo zharoprochnogo nikelevogo splava [Way of receiving product from deformable heat resisting nickel alloy]: pat. 2387733 Ros. Federaciya; opubl. 31.03.2009.
- Golubovskij E.R., Svetlov I.L., Petrushin N.V., Cherkasova S.A., Volkov M.E. Malociklovaya ustalost monokristallov zharoprochnyh nikelevyh splavov pri povyshennyh temperaturah [Low-cyclic fatigue of single crystals of heat resisting nickel alloys at elevated temperatures] //Deformaciya i razrushenie materialov. 2009. № 8. S. 41–48.
- Tobias J., Chlupova A., Petrenec M. et al. Low Cycle Fatigue and Analysis of the Cyclic Stress-Strain Response in Superalloy Inconel 738LC /In: 18-th International Conference «Engineering Mechanics 2012». Svratka. 2012. P. 1407–1411.
- Nagesha A., Goyal Sunil, Nandagopal M. at al. Dynamic strain ageing in Inconel Alloy 783 under tension and low cycle fatigue //Mater. Sci. and Eng. A. 2012. V. 546. P. 34–39.
- Levkovitch V., Sievert R., Svendsen B. Simulation of deformation and lifetime behavior of a FCC single cristal superalloy at high temperature under low-cycle fatigue loading //Int. J. Fatigue. 2006. V. 28 (12). P. 1791–1802.
- Wright J.K., Carroll L.J., J.A. Simpson J.A. et al. Low Cycle Fatigue of Alloy 617 at 850°C and 950°C //J. of Eng. Mat. and Tech. 2013. V. 135. №7. P. 031005-1–031005-8.
- Subramanya Sarma V., Sundararaman M., Padmanabhan K.A. Effect of γ size on room temperature low cycle fatigue behavior of a nickel base superalloy //Material Science and Technology. 1998. V. 14. №7. P. 669–675.
- Lomberg B.S., Ovsepyan S.V., Bakradze M.M., Mazalov I.S. Vysokotemperaturnye zharo-prochnye nikelevye splavy dlya detalej gazoturbinnyh dvigatelej [High-temperature heat resisting nickel alloys for details of gas turbine engines] //Aviacionnye materialy i tehnologii. 2012. №S. S. 52–57.
- Bakradze M.M., Ovsepyan S.V., Shugaev S.A., Letnikov M.N. Vliyanie rezhimov zakalki na strukturu i svojstva shtampovok diskov iz zharoprochnogo nikelevogo splava EK151-ID [The influence of quenching on structure and properties nickel-based superalloy EK151-ID forgings] //Trudy VIAM. 2013. №9. St. 01 (viam-works.ru).
- Lomberg B.S., Ovsepyan S.V., Bakradze M.M. Osobennosti legirovaniya i termicheskoj obrabotki zharoprochnyh nikelevyh splavov dlya diskov gazoturbinnyh dvigatelej novogo pokoleniya [Features of alloying and thermal processing of heat resisting nickel alloys for disks of gas turbine engines of new generation] //Aviacionnye materialy i tehnologii. 2010. №2. S. 3–8.
- Kablov E.N., Ospennikova O.G., Lomberg B.S. Kompleksnaya innovacionnaya tehnologiya izotermicheskoj shtampovki na vozduhe v rezhime sverhplastichnosti diskov iz superzharoprochnyh splavov [Complex innovative technology of isothermal punching on air in mode of superplasticity of disks from superhot strength alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 129–141.
- Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Litejnye zharoprochnye nikelevye splavy dlya perspektivnyh aviacionnyh GTD [Cast heat resisting nickel alloys for perspective aviation GTE] //Tehnologiya legkih splavov. 2007. №2. S. 6–16.