Change of parameters of elasto-plastic deformation for LCF testing Ni-base superalloy VZh175

Belyaev M.S., Gorbovets M.A., Bakradze M.M.
Belyaev M.S., Gorbovets M.A., Bakradze M.M. Change of parameters of elasto-plastic deformation for LCF testing Ni-base superalloy VZh175 // Proceedings of VIAM. 2015. No. 12. DOI: 10.18577/2307-6046-2015-0-12-4-4. URL: https://viam-works.ru/en/journal/2015/12/4
Keywords
low-cycle fatigue (LCF), alteration curves of cyclic stress, elastic-plastic hysteresis, Ni-base superalloy VZh175.
Abstract

The LCF behavior for Ni-base superalloy VZh175 was investigated for a given total strain, ratio R=0 and stain amplitude εa=0,4–0,6% at test temperatures 20 and 650°С. Parameters of elastic-plastic strain were observed in this article.

Reference list
  1. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokoleniya [Nickel foundry heat resisting alloys of new generation] //Aviacionnye materialy i tehnologii. 2012. №S. C. 36–52.
  2. Birger I.A., Balashov B.F., Dulnev R.A. i dr. Konstrukcionnaja prochnost materialov i detalej gazoturbinnyh dvigatelej [Constructional durability of materials and details of gas turbine engines]. M.: Mashinostroenie. 1981. 222 s.
  3. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  4. Inozemtsev A.A., Ratchiev A.M., Nihamkin M.Sh. i dr. Malociklovaja ustalost i ciklicheskaya treshhinostojkost nikelevogo splava pri nagruzhenii, harakternom dlya diskov turbin [Low-cyclic fatigue and cyclic crack firmness of nickel alloy when loading, characteristic for disks of turbines] //Tuazheloe mashinostroenie. 2011. №4. S. 30–33.
  5. Schijve J. Fatigue of structures and materials. Berlin Heidelberg: Springer-Verlag. 2009. 185 p.
  6. Kablov E.N., Lomberg B.S., Ospennikova O.G. Sozdanie sovremennyh zharoprochnyh materialov i tehnologij ih proizvodstva dlya aviacionnogo dvigatelestroeniya [Creation of modern heat resisting materials and technologies of their production for aviation engine building] //Krylya Rodiny. 2012. №3–4. S. 34–38.
  7. Kablov E.N., Ospennikova O.G., Lomberg B.S., Sidorov V.V. Prioritetnye napravleniya razvitiya tehnologij proizvodstva zharoprochnyh materialov dlya aviacionnogo dvigatelestroeniya [The priority directions of development of production technologies of heat resisting materials for aviation engine building] //Problemy chernoj metallurgii i materialovedenija. 2013. №3. S. 47–54.
  8. Sposob polucheniya izdeliya iz deformiruemogo zharoprochnogo nikelevogo splava [Way of receiving product from deformable heat resisting nickel alloy]: pat. 2387733 Ros. Federaciya; opubl. 31.03.2009.
  9. Golubovskij E.R., Svetlov I.L., Petrushin N.V., Cherkasova S.A., Volkov M.E. Malociklovaya ustalost monokristallov zharoprochnyh nikelevyh splavov pri povyshennyh temperaturah [Low-cyclic fatigue of single crystals of heat resisting nickel alloys at elevated temperatures] //Deformaciya i razrushenie materialov. 2009. № 8. S. 41–48.
  10. Tobias J., Chlupova A., Petrenec M. et al. Low Cycle Fatigue and Analysis of the Cyclic Stress-Strain Response in Superalloy Inconel 738LC /In: 18-th International Conference «Engineering Mechanics 2012». Svratka. 2012. P. 1407–1411.
  11. Nagesha A., Goyal Sunil, Nandagopal M. at al. Dynamic strain ageing in Inconel Alloy 783 under tension and low cycle fatigue //Mater. Sci. and Eng. A. 2012. V. 546. P. 34–39.
  12. Levkovitch V., Sievert R., Svendsen B. Simulation of deformation and lifetime behavior of a FCC single cristal superalloy at high temperature under low-cycle fatigue loading //Int. J. Fatigue. 2006. V. 28 (12). P. 1791–1802.
  13. Wright J.K., Carroll L.J., J.A. Simpson J.A. et al. Low Cycle Fatigue of Alloy 617 at 850°C and 950°C //J. of Eng. Mat. and Tech. 2013. V. 135. №7. P. 031005-1–031005-8.
  14. Subramanya Sarma V., Sundararaman M., Padmanabhan K.A. Effect of γ size on room temperature low cycle fatigue behavior of a nickel base superalloy //Material Science and Technology. 1998. V. 14. №7. P. 669–675.
  15. Lomberg B.S., Ovsepyan S.V., Bakradze M.M., Mazalov I.S. Vysokotemperaturnye zharo-prochnye nikelevye splavy dlya detalej gazoturbinnyh dvigatelej [High-temperature heat resisting nickel alloys for details of gas turbine engines] //Aviacionnye materialy i tehnologii. 2012. №S. S. 52–57.
  16. Bakradze M.M., Ovsepyan S.V., Shugaev S.A., Letnikov M.N. Vliyanie rezhimov zakalki na strukturu i svojstva shtampovok diskov iz zharoprochnogo nikelevogo splava EK151-ID [The influence of quenching on structure and properties nickel-based superalloy EK151-ID forgings] //Trudy VIAM. 2013. №9. St. 01 (viam-works.ru).
  17. Lomberg B.S., Ovsepyan S.V., Bakradze M.M. Osobennosti legirovaniya i termicheskoj obrabotki zharoprochnyh nikelevyh splavov dlya diskov gazoturbinnyh dvigatelej novogo pokoleniya [Features of alloying and thermal processing of heat resisting nickel alloys for disks of gas turbine engines of new generation] //Aviacionnye materialy i tehnologii. 2010. №2. S. 3–8.
  18. Kablov E.N., Ospennikova O.G., Lomberg B.S. Kompleksnaya innovacionnaya tehnologiya izotermicheskoj shtampovki na vozduhe v rezhime sverhplastichnosti diskov iz superzharoprochnyh splavov [Complex innovative technology of isothermal punching on air in mode of superplasticity of disks from superhot strength alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 129–141.
  19. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Litejnye zharoprochnye nikelevye splavy dlya perspektivnyh aviacionnyh GTD [Cast heat resisting nickel alloys for perspective aviation GTE] //Tehnologiya legkih splavov. 2007. №2. S. 6–16.