To the question of elasticity modulus of fibers from refractory oxides
Zimichev A.M., Balinova Yu.A., Varrik N.M. To the question of elasticity modulus of fibers from refractory oxides // Proceedings of VIAM. 2014. No. 10. DOI: 10.18577/2307-6046-2014-0-10-6-6. URL: https://viam-works.ru/en/journal/2014/10/6
Abstract
Results of tests by acoustic method of continuous fibers on a base of refractory oxides meant for production of flexible sealing thermal insulation are given. X-ray phase structure and elasticity modulus were defined for samples of Al2O3–SiO2 fibers after heat treatment at 700, 900 and 1200°С. Results showed that a full crystallization of ceramic structure at high-temperature burning leads to increasing of elasticity modulus of oxide fi-bers.
Reference list
- Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
- Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
- Ivahnenko Ju.A., Babashov V.G., Zimichev A.M., Tinjakova E.V. Vysokotemperaturnye teploizoljacionnye i teplozashhitnye materialy na osnove volokon tugoplavkih soedinenij [High-temperature and heat-insulating materials based on fibers of refractory compounds] //Aviacionnye materialy i tehnologii. 2012. №S. S. 380–385.
- Tinjakova E.V., Grashhenkov D.V. Teploizoljacionnyj material na osnove mullito-korundovyh i kvarcevyh volokon [Thermal insulation material on the basis of mullite-corundum and quartz fibers] //Aviacionnye materialy i tehnologii. 2012. №3. S. 43–46.
- Kablov E.N., Shhetanov B.V., Abuzin Ju.A., Ivahnenko Ju.A. Metallicheskie i keramicheskie kompozicionnye materialy [Metallic and ceramic composite materials] /V sb. materialov Mezhdunarodnoj nauch.-praktich. konf. «Sovremennye tehnologii – kljuchevoe zveno v vozrozhdenii otechestvennogo aviastroenija». T. 1. Kazan'. 2008.
- S. 181–188.
- Kablov E.N., Grashhenkov D.V., Isaeva N.V., Solncev S.S. Perspektivnye vysokotemperaturnye keramicheskie kompozicionnye materialy [Promising high-temperature ceramic composites] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 20–24.
- Kablov E.N., Shhetanov B.V., Ivahnenko Ju.A., Balinova Ju.A. Perspektivnye armirujushhie vysokotemperaturnye volokna dlja metallicheskih i keramicheskih kompozicionnyh materialov [Promising reinforcing fibers for high temperature metal and ceramic composite materials] //Trudy VIAM. 2013. №2. St. 05 (viam-works.ru).
- Dospehi dlja «Burana». Materialy i tehnologii VIAM dlja MKS «Jenergija–Buran» [Armor for the «Buran». Materials and technologies for the ISS VIAM «Energiya–Buran»] /Pod obshh. red. E.N. Kablova. M.: Fond «Nauka i zhizn'». 2013. S. 36–39.
- Shhetanov B.V., Ivahnenko Ju.A., Babashov V.G. Teplozashhitnye materialy [Heat-proof materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 12–20.
- Krenkel W., Lamon J. Hight-Temperature Ceramic Materials and Composites /In: 7-th Internatiolal Conference on Ceramic Matrix Composites (HT-CMC 7). 2010. Р. 467–472.
- Ceramic Fibers and Coatings. Advanced Materials for the Twenty-First Century Committee on Advanced Fibers for High-Temperature Ceramic Composites. Washington: National Academy Press. 1998. 95 р.
- Wilson D.M., Visser L.R. High performance oxide fibers for metal and ceramic composites /In: Processing of fibers & composites. 2000. Barga. 31 p.
- Parlier M., Ritti M.-H., Jankowiak A. Potential and Perspectives for Oxide-Oxide Composites //Journal Aerospacelab. 2011. №3. Р. 1–12.
- Jessen T., Ustundag E. /In: 24-th Annual Conference on Composites, Advanced Ceramics, Materials and Structures //Ceramic Engineering and Science Proceedings. B. 2000. V. 21. №4. P. 549–557.
- Zimichev A.M., Varrik N.M. Termogravimetricheskie issledovanija nitej na osnove oksida aljuminija [Thermogravimetric studies strands of the alumina] //Trudy VIAM. 2014. №6. St. 06 (viam-works.ru).
- Zimichev A.M., Varrik N.M., Dalin M.A. Izmerenie modulja uprugosti volokon iz tugoplavkih oksidov [Measurement of modulus fibers of refractory oxides] //Trudy VIAM. 2014. №6. St. 05 (viam-works.ru).
- Dalin M.A., Generalov A.S., Bojchuk A.S., Lozhkova D.S. Osnovnye tendencii razvitija akusticheskih metodov nerazrushajushhego kontrolja [The main trends in the development of acoustic methods of non-destructive testing] //Aviacionnye materialy i tehnologii. 2013. №1. S. 64–69.
- Generalov A.S., Murashov V.V., Dalin M.A., Bojchuk A.S. Diagnostika polimernyh kompozitov ul'trazvukovym reverberacionno-skvoznym metodom [Diagnosis of polymer composites ultrasonic cross-cutting method of reverberation] //Aviacionnye materialy i tehnologii. 2012. №1. S. 42–47.
- Sposob poluchenija vysokotemperaturnogo volokna na osnove oksida aljuminija [Method of obtaining high fiber based on alumina]: pat. 2212388 Ros. Federacija; opubl. 20.09.2003. Bjul. №34. 6 s.
- Bunsell A.R., Miner J. Oxide Fibers for High-Temperature Reinforcement and Insulation //Metalls and Mater. Sci. 2005. V. 57. Р. 48–51.