To the question of elasticity modulus of fibers from refractory oxides

Zimichev A.M., Balinova Yu.A., Varrik N.M.
Zimichev A.M., Balinova Yu.A., Varrik N.M. To the question of elasticity modulus of fibers from refractory oxides // Proceedings of VIAM. 2014. No. 10. DOI: 10.18577/2307-6046-2014-0-10-6-6. URL: https://viam-works.ru/en/journal/2014/10/6
Abstract

Results of tests by acoustic method of continuous fibers on a base of refractory oxides meant for production of flexible sealing thermal insulation are given. X-ray phase structure and elasticity modulus were defined for samples of Al2O3–SiO2 fibers after heat treatment at 700, 900 and 1200°С. Results showed that a full crystallization of ceramic structure at high-temperature burning leads to increasing of elasticity modulus of oxide fi-bers.

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  3. Ivahnenko Ju.A., Babashov V.G., Zimichev A.M., Tinjakova E.V. Vysokotemperaturnye teploizoljacionnye i teplozashhitnye materialy na osnove volokon tugoplavkih soedinenij [High-temperature and heat-insulating materials based on fibers of refractory compounds] //Aviacionnye materialy i tehnologii. 2012. №S. S. 380–385.
  4. Tinjakova E.V., Grashhenkov D.V. Teploizoljacionnyj material na osnove mullito-korundovyh i kvarcevyh volokon [Thermal insulation material on the basis of mullite-corundum and quartz fibers] //Aviacionnye materialy i tehnologii. 2012. №3. S. 43–46.
  5. Kablov E.N., Shhetanov B.V., Abuzin Ju.A., Ivahnenko Ju.A. Metallicheskie i keramicheskie kompozicionnye materialy [Metallic and ceramic composite materials] /V sb. materialov Mezhdunarodnoj nauch.-praktich. konf. «Sovremennye tehnologii – kljuchevoe zveno v vozrozhdenii otechestvennogo aviastroenija». T. 1. Kazan'. 2008.
  6. S. 181–188.
  7. Kablov E.N., Grashhenkov D.V., Isaeva N.V., Solncev S.S. Perspektivnye vysokotemperaturnye keramicheskie kompozicionnye materialy [Promising high-temperature ceramic composites] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 20–24.
  8. Kablov E.N., Shhetanov B.V., Ivahnenko Ju.A., Balinova Ju.A. Perspektivnye armirujushhie vysokotemperaturnye volokna dlja metallicheskih i keramicheskih kompozicionnyh materialov [Promising reinforcing fibers for high temperature metal and ceramic composite materials] //Trudy VIAM. 2013. №2. St. 05 (viam-works.ru).
  9. Dospehi dlja «Burana». Materialy i tehnologii VIAM dlja MKS «Jenergija–Buran» [Armor for the «Buran». Materials and technologies for the ISS VIAM «Energiya–Buran»] /Pod obshh. red. E.N. Kablova. M.: Fond «Nauka i zhizn'». 2013. S. 36–39.
  10. Shhetanov B.V., Ivahnenko Ju.A., Babashov V.G. Teplozashhitnye materialy [Heat-proof materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 12–20.
  11. Krenkel W., Lamon J. Hight-Temperature Ceramic Materials and Composites /In: 7-th Internatiolal Conference on Ceramic Matrix Composites (HT-CMC 7). 2010. Р. 467–472.
  12. Ceramic Fibers and Coatings. Advanced Materials for the Twenty-First Century Committee on Advanced Fibers for High-Temperature Ceramic Composites. Washington: National Academy Press. 1998. 95 р.
  13. Wilson D.M., Visser L.R. High performance oxide fibers for metal and ceramic composites /In: Processing of fibers & composites. 2000. Barga. 31 p.
  14. Parlier M., Ritti M.-H., Jankowiak A. Potential and Perspectives for Oxide-Oxide Composites //Journal Aerospacelab. 2011. №3. Р. 1–12.
  15. Jessen T., Ustundag E. /In: 24-th Annual Conference on Composites, Advanced Ceramics, Materials and Structures //Ceramic Engineering and Science Proceedings. B. 2000. V. 21. №4. P. 549–557.
  16. Zimichev A.M., Varrik N.M. Termogravimetricheskie issledovanija nitej na osnove oksida aljuminija [Thermogravimetric studies strands of the alumina] //Trudy VIAM. 2014. №6. St. 06 (viam-works.ru).
  17. Zimichev A.M., Varrik N.M., Dalin M.A. Izmerenie modulja uprugosti volokon iz tugoplavkih oksidov [Measurement of modulus fibers of refractory oxides] //Trudy VIAM. 2014. №6. St. 05 (viam-works.ru).
  18. Dalin M.A., Generalov A.S., Bojchuk A.S., Lozhkova D.S. Osnovnye tendencii razvitija akusticheskih metodov nerazrushajushhego kontrolja [The main trends in the development of acoustic methods of non-destructive testing] //Aviacionnye materialy i tehnologii. 2013. №1. S. 64–69.
  19. Generalov A.S., Murashov V.V., Dalin M.A., Bojchuk A.S. Diagnostika polimernyh kompozitov ul'trazvukovym reverberacionno-skvoznym metodom [Diagnosis of polymer composites ultrasonic cross-cutting method of reverberation] //Aviacionnye materialy i tehnologii. 2012. №1. S. 42–47.
  20. Sposob poluchenija vysokotemperaturnogo volokna na osnove oksida aljuminija [Method of obtaining high fiber based on alumina]: pat. 2212388 Ros. Federacija; opubl. 20.09.2003. Bjul. №34. 6 s.
  21. Bunsell A.R., Miner J. Oxide Fibers for High-Temperature Reinforcement and Insulation //Metalls and Mater. Sci. 2005. V. 57. Р. 48–51.