P. A. Slobodskoy, N. S. Moiseeva, K. V. Dulnev, E. A. Yeliseyev, M. S. Alekseeva Influence of heat treatment parameters on structural-phase composition and properties of high-strength nitrogen-alloyed martensitic steel // Proceedings of VIAM. 2026. No. 11 (165). С. 32-41. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-11-32-41.

Influence of heat treatment parameters on structural-phase composition and properties of high-strength nitrogen-alloyed martensitic steel

P. A. Slobodskoy1, N. S. Moiseeva1, K. V. Dulnev1, E. A. Yeliseyev1, M. S. Alekseeva1

1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru

Abstract

The article presents the results of a study of heat treatment modes on the phase composition, structure and properties of nitrogen-containing steel of the martensitic class. A comprehensive study of the steel phase composition after conducting various heat treatment processes, using thermodynamic modeling and X-ray phase analysis, showed a high degree correlation between calculated and experimental data. It was found that the most favorable combination of hardness and impact toughness is achieved when 3–5 wt.% of the residual austenite is preserved in the structure in the martensitic matrix.

Keywords
research structures, constructional nitrogen-bearing steels, transmission electron microscopy, X-ray diffraction (structural) phase analysis

Reference list
  1. Kablov E. N. The Role of Fundamental Research in the Creation of New-Generation Materials. Abstracts of the XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, pp. 24.
  2. Kablov E. N. Structural and Functional Materials: The Foundation for Russia’s Economic and Scientific-Technological Development. Voprosy materialovedeniya, 2006, no. 1, pp. 64–67.
  3. Kablov E. N., Antipov V. V. The Role of New-Generation Materials in Ensuring the Technological Sovereignty of the Russian Federation. Vestnik Rossiyskoy akademii nauk, 2023, vol. 93, no. 10, pp. 907–916.
  4. Kablov E. N., Bakradze M. M., Gromov V. I., Voznesenskaya N. M., Yakusheva N. A. New high strength structural and corrosion-resistant steels for aerospace equipment developed by FSUE «VIAM» (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 3–11. DOI: 10.18577/2071-9140-2020-0-1-3-11.
  5. Dulnev K. V., Sevalnev G. S. Structure formation and formation of properties during thermal cycling of high-strength high-nitrogen economy-alloyed steel. Aviation materials and technologies, 2026, no. 2 (83), pp. 145–159. Available at: http://www.journal.viam.ru (accessed: June 14, 2026). DOI: 10.18577/2713-0193-2026-0-2-5-14.
  6. Tonysheva O. A., Voznesenskaya N. M., Gromov V. I., Leonov A. V. High strength corrosion resistant steel VNS-74 as applied to aircraft fasteners. Trudy VIAM, 2022, no. 7 (113), pp. 3–12. Available at: http://www.viam-works.ru (accessed: June 10, 2026). DOI: 10.18577/2307-6046-2022-0-7-3-12.
  7. Svyazhin A. G., Kaputkina L. M. Nitrogen-alloyed and high-nitrogen steels: industrial technologies and properties. Izvestiya vysshikh uchebnykh zavedeniy. Chernaya metallurgiya, 2019, vol. 62, no. 3, pp. 173–187.
  8. Gavriluk V. G. Atomicinteraction and mechanisms of strengthening in nitrogen steels. Proceedings of International Conference on High Nitrogen Steels (HNS 2006). Jiuzhaigou Valley, 2006, pp. 3–12.
  9. Gavriluk V. G. Carbon, nitrogen and nydrogen in steels plasticity and brittleness. Proceedings of the 11th Int. Conf. on High Nitrogen Steels and Interstitial Alloys (HNS 2012). Chennai: India VRK Printing House, 2013, p. 23030.
  10. Gavriluk V. G., Berns H. High Nitrogen Steels. Berlin: Springer Verlag, 1999, 378 p.
  11. Lukin E. I. Research and development of nickel and nickel-chromium steels with a nitrogen-martensite structure for highly loaded components: thesis, Dr. Sc. (Tech.). Moscow, 2016, 116 p.
  12. Eliseev E. A., Karpukhin S. D., Druzhinina M. E. The effect of nickel on the structure of the nitrided layer of low-carbon martensitic steels. Aviation materials and technologies, 2025, no. 1 (78), pp. 18–27. Available at: http://www.journal.viam.ru (accessed: June 11, 2026). DOI: 10.18577/2713-0193-2025-0-1-18-27.
  13. Sadovsky V. D., Malyshev K. A., Sazonov B. G. Phase and Structural Transformations During the Heating of Steel. Moscow: Metallurgizdat, 1957, 118 p.
  14. Gromov V. I., Yakusheva N. A., Vostrikov A. V., Cherkashneva N. N. High strength structural steels for gas-turbine engine shafts (review). Aviation materials and technology, 2021, no. 1 (62), pp. 3‒12. Available at: http://www.journal.viam.ru (accessed: June 10, 2026). DOI: 10.18577/2713-0193-2021-0-1-3-12.
  15. Kablov E. N., Grinevich A. V., Slavin A. V., Kabanov I. V., Gromov V. I., Ampilogov A. Yu., Yakovlev N. O., Polyakov A. N., Yakusheva N. A. Design Strength Characteristics of VKS-9M and 300M Steels. Zavodskaya laboratoriya. Diagnostika materialov, 2022, vol. 88, no. 3, pp. 51–60.
  16. Agbalyan S. G., Simonyan V. A. A Review of the Characteristics, Production Methods, and Potential Applications of Maraging Steels. Mezhdunarodnyy nauchno-issledovatelskiy zhurnal, 2022, no. 8, pp. 1–12.
  17. Morozova L. V., Grigorenko V. B., Terekhin А. М. Analysis of defects in parts made of structural steel. Trudy VIAM, 2025, no. 10 (152), pp. 27–39. Available at: http://www.viam-works.ru (accessed: June 10, 2026). DOI: 10.18577/2307-6046-2025-0-10-27-39.