D. I. Sukhov, V. D. Gogoleva, D. A. Movenko Analysis of selective laser melting modes of nickel alloys using thermodynamic modeling // Proceedings of VIAM. 2026. No. 8 (162). С. 3-16. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-8-3-16.

Analysis of selective laser melting modes of nickel alloys using thermodynamic modeling

D. I. Sukhov1, V. D. Gogoleva1, D. A. Movenko1

1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru

Abstract

In this paper the stages of constructing a map of the selective laser melting process for nickel alloys presented: initially, the map was initially constructed using thermodynamic modeling, then refined and empirically verified. The optimal range of linear energy density for nickel alloys is established, regardless of the hatching type. For the nickel alloys considered in this work the curves for porosity, average and maximum pore size on linear energy density in the optimal range are parabolic.


 

Keywords
additive manufacturing, heat-resistant nickel alloys, selective laser melting, SLM parameters, thermodynamic modeling, energy density
Reference list
  1. Herzog D., Seyda V., Wycisk E., Emmelmann C. Additive manufacturing of metals. Acta Materialia, 2016, vol. 117, pp. 371–392. DOI: 10.1016/j.actamat.2016.07.019.
  2. Kablov E.N., Evgenov A.G., Petrushin N.V., Bazyleva O.A., Mazalov I.S., Dynin N.V. New generation materials and digital additive technologies for the production of resource parts of FSUE VIAM. Part 3. Adaptation and creation of materials. Electrometallurgiya, 2022, no. 4, pp. 15–25.
  3. Zhang D., Sun S., Qiu D. et al. Additive manufacturing of superalloys: A review. Materials & Design, 2018, vol. 158, pp. 198-210. DOI: 10.1016/j.matdes.2018.04.046.
  4. DebRoy T., Wei H.L., Zuback J.S. et al. Additive manufacturing of metallic components - Process, structure and properties. Progress in Materials Science, 2018, vol. 92, pp. 112-224. DOI: 10.1016/j.pmatsci.2017.10.001.
  5. Nerush S.V., Chubov D.G., Kaplanskiy Yu.Yu., Suhov D.I. Investigation of experimental nickelbased heat-resistant alloy obtained by selective laser melting method. Trudy VIAM, 2025, no. 7 (149), pp. 3-12. Available at: http://www.viam-works.ru (accessed: November 17, 2025). DOI: 10.18577/2307-6046-2025-0-7-3-12.
  6. Ospennikova O.G., Naprienko S.A., Medvedev P.N., Zaitsev D.V., Rogalev A.M. Features of the formation of the structural-phase state of the EP648 alloy during selective laser manufacture. Trudy VIAM, 2021, no.8 (102), pp. 3-11. Available at: http://www.viam-works.ru (accessed: November 18, 2025). DOI: 10.18557/2307-6046-2021-0-8-3-11.
  7. Movenko D.A., Shurtakov S.V. Microcrack formation and controlling in nickel superalloys processed by selective laser melting (review). Aviation materials and technologies, 2022, no. 2 (67), pp. 43-51. Available at: http://www.journal.viam.ru (accessed: November 18, 2025). DOI: 10.18577/2713-0193-2022-0-2-43-51.
  8. Wang X., Carter L.N., Pang B. et al. Microstructure and yield strength of SLM-fabricated CM247LC Ni-Superalloy. Acta Materialia, 2017, vol. 128, pp. 87-95. DOI: 10.1016/j.actamat.2017.02.007.
  9. Zhao Y., Li K., Gargani M., Xiong W. A comparative analysis of Inconel 718 made by additive manufacturing and suction casting: Microstructure evolution in homogenization. Additive Manufacturing, 2020, vol. 36, pp. 1-28. DOI: 10.1016/j.addma.2020.101404.
  10. Xinxu L., Chonglin J., Yong Z. et al. Segregation and homogenization for a new nickel-based superalloy. Vacuum, 2020, vol. 177, p. 109379. DOI: 10.1016/j.vacuum.2020.109379.
  11. Sukhov D.I., Mazalov P.B., Nerush S.V., Khodirev N.A. The influence of SLS parameters on pores formation in stainless steel material. Trudy VIAM, 2017, no. 8 (56), pp. 34-44. Available at: http://www.viam-works.ru (accessed: November 19, 2025). DOI: 10.18577/2307-6046-2017-0-8-4-4.
  12. Gu H., Gong H., Pal D. et al. Influences of Energy Density on Porosity and Microstructure of Selective Laser Melted 17-4PH Stainless Steel. Proceeding of Solid Freeform Fabrication Symposium. Texas, 2013, pp. 474-489.
  13. Braun J., Kaserer L., Stajkovic J. et al. Molybdenum and Tungsten Manufactured by Selective Laser Melting: Analysis of Defect Structure and Solidification Mechanism. International Journal of Refractory Metals & Hard Materials, 2019, vol. 84, art. 104999. DOI: 10.1016/j.ijrmhm.2019.104999.
  14. Kempen K., Thijs L., Van Humbeeck J., Kruth J.-P. Processing AlSi10Mg by selective laser melting: parameter optimization and material characterization. Materials Science and Technology, 2015, vol. 31, no. 8, pp. 917-923. DOI: 10.1179/1743284714Y.0000000702.
  15. Kilina P.N., Morozov E.A., Khanov A.M., Sirotenko L.D. Study of modes of selective laser melting of metal powders. Sovremennye problemy nauki i obrazovaniya, 2014, no. 6. Available at: https://science-education.ru/ru/article/view?id=16035 (accessed: January 23, 2026).
  16. Nerush S.V., Kaplanskii Yu.Yu., Dynin N.V., Benarieb I., Savichev I.D. Development of laser powder bed fusion parameters, structure and mechanical properties of a high-strength aluminum alloy Al-Ce-Cu. Trudy VIAM, 2023, no. 1 (119), pp. 50-68. Available at: http://www.viam-works.ru (accessed: August 03, 2025). DOI: 10.18577/2307-6046-2023-0-1-50-68.
  17. Sukhov D.I., Aslanyan G.G., Rogalev A.M., Kurkin S.E. Alternative approach to assessing selective laser melting modes for nickel alloys prone to cracking. Tekhnologiya metallov, 2024, no. 3, pp. 9-18. DOI: 10.31044/1684-2499-2024-0-3-9-18.
  18. Thomas M., Baxter G., Todd I. Normalized model-based processing diagrams for additive layer manufacture of engineering alloys. Acta Materialia, 2016, vol. 108, pp. 26-35. DOI: 10.1016/j.actamat.2016.02.025.
  19. Leis A., Weber R., Graf T. Process Window for Highly Efficient Laser-Based Powder Bed Fusion of AlSi10Mg with Reduced Pore Formation. Materials, 2021, vol. 14 (18), p. 5255. DOI: 10.3390/ma14185255.
  20. Narra S.P., Rollett A.D., Ngo A. et al. Process qualification of laser powder bed fusion based on processing-defect structure-fatigue properties in Ti-6Al-4V. Journal of Materials Processing Technology, 2023, vol. 311, art. 117775. DOI: 10.1016/j.jmatprotec.2022.117775.
  21. Chen Y., Böhm J., Wahlmann B. et al. Rapid processing window development of Mo–Si–B alloy for electron beam powder bed fusion. Progress in Additive Manufacturing, 2025, vol. 10, pp. 8311–8320. DOI: 10.1007/s40964-025-01119-z.
  22. Park J.M., Jung J., Lee S. et al. Data-driven Approach to Explore the Contribution of Process Parameters for Laser Powder Bed Fusion of a Ti-6Al-4V Alloy. Journal of Powder Materials, 2024, vol. 31 (2), pp. 137–145. DOI: 10.4150/jpm.2024.00038.
  23. Trask M.E., Bishop D.P. Investigating the process parameter window for laser powder bed fusion of copper chrome zirconium. Canadian Metallurgical Quarterly, 2025, vol. 64 (4), pp. 2589–2610. DOI: 10.1080/00084433.2024.2396639.
  24. Jeronen J., Tuovinen T., Kurki M. One-Dimensional Thermomechanical Model for Additive Manufacturing Using Laser-Based Powder Bed Fusion. Computation, 2022, vol. 10 (6), art. 83. DOI: 10.3390/computation10060083.
  25. Psihoyos H.O., Lampeas G.N. Efficient thermomechanical modelling of Laser Powder Bed Fusion additive manufacturing process with emphasis on parts residual stress fields. AIMS Materials Science, 2022, vol. 9 (3), pp. 455–480. DOI: 10.3934/matersci.2022027.
  26. Wang S., Shen Y. A new model framework of laser powder bed fusion by integrating a powder-scale model with a thermodynamic database. Chemical Engineering Science, 2025, vol. 302, part A, art. 120788. DOI: 10.1016/j.ces.2024.120788.
  27. Hu Z., Nagarajan B., Song X. et al. Formation of SS316L Single Tracks in Micro Selective Laser Melting: Surface, Geometry, and Defects. Advances in Materials Science and Engineering, 2019, vol. 2019, pp. 1–9. DOI: 10.1155/2019/9451406.
  28. Bustillos J., Kim J., Moridi A. Exploiting lack of fusion defects for microstructural engineering in additive manufacturing. Additive Manufacturing, 2021, vol. 48, part A, art. 102399. DOI: 10.1016/j.addma.2021.102399.
  29. Wang L., Zhang Y., Chia H.Y., Yan W. Mechanism of keyhole pore formation in metal additive manufacturing. NPJ Computational Materials, 2022, vol. 8, art. 22. DOI: 10.1038/s41524-022-00699-6.