V. O. Startsev, A. A. Nechaev Analysis of the correlation of changes in mechanical and diffusion characteristics of fiberglass VPS-53/T-25 during full-scale and accelerated climatic tests // Proceedings of VIAM. 2026. No. 8 (162). С. 195-207. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-8-195-207.
Analysis of the correlation of changes in mechanical and diffusion characteristics of fiberglass VPS-53/T-25 during full-scale and accelerated climatic tests
1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru
Abstract
Climatic testing of VPS-53/T-25 fiberglass was conducted in outdoor, moderate and moderately warm climates for 12 months, as well as laboratory simulation tests in two modes. After all intermediate measurements, flexural strengths were measured, taking into account the reversible effect of moisture. The mass of the specimens was measured during drying and wetting to determine moisture transfer parameters. Correlations between the studied characteristics were calculated during full-scale and accelerated climatic tests.
Keywords
climatic aging, fiberglass, bending strength, diffusion coefficient, mathematical modeling, correlation dependence
Reference list
- Buznik V.M., Kablov E.N. Arctic materials science. Tomsk: Publ. house. house Tomsk. State Univ., 2018, is. 3, 44 p.
- Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Climatic aging of composite aviation materials: 2. Relaxation of the initial structural nonequilibrium and through thickness gradient of properties. Russian Metallurgy (Metally), 2011, no. 10, pp. 1001–1007.
- Startsev O.V., Isupov V.V., Nikishin E.F. The Gradient of Mechanical Characteristics Across the Thickness of Composite Laminates After Exposure to a Low Earth Orbit Environment. Polymer Composites, 1998, vol. 19, no. 1, pp. 65–70.
- Startsev O.V., Nikishin E.F. Aging of polymer composite materials in outer space. Mekhanika kompozitnykh materialov, 1993, no. 4, pp. 457–467.
- Siddiqui M.N., Redhwi H.H., Andrady A.L. et al. Effect of Extensive Solar Ultra-Violet Irradiation on the Durability of High-Density Polyethylene- and Polypropylene-Based Wood– Plastic Composites. Polymers, 2024, vol. 17, no. 1, pp. 74.
- Das S.C., La Rosa A.D., Goutianos S., Grammatikos S. Effect of accelerated weathering on the performance of natural fibre reinforced recyclable polymer composites and comparison with conventional composites. Composites Part C: Open Access, 2023, vol. 12, art. 100378.
- Hashim U.R., Jumahat A., Jawaid M., Dungani R., Alamery S. Effects of Accelerated Weathering on Degradation Behavior of Basalt Fiber Reinforced Polymer Nanocomposites. Polymers, 2020, vol. 12, no. 11, art. 2621.
- Rogha E., Bazli M., Shakiba M. et al. UV-induced transformations and mechanical performance of 3D-printed thermoplastic CFRP, GFRP, and AFRP composites. Composites Communications, 2025, vol. 59, art. 102591.
- Alam L., Piezel B., Sicot O. et al. UV accelerated aging of unidirectional flax composites: Comparative study between recycled and virgin polypropylene matrix. Polymer Degradation and Stability, 2023, vol. 208, art. 110268.
- Xi X., Zhang S., Hao Z. et al. Durability assessment of vacuum-infused GFRP laminates and I-beams in marine environments. Case Studies in Construction Materials, 2025, vol. 22, art. e04743.
- Hassanshahi O., Jorge M., Sena-Cruz J. et al. Durability of GFRP Composites Produced by Pultrusion under Thermal Environments. Procedia Structural Integrity, 2024, vol. 64, pp. 81–88.
- Wang J., Karimi S., Zeinalzad P. et al. Using machine learning and experimental study to correlate and predict accelerated aging with natural aging of GFRP composites in hygrothermal conditions. Construction and Building Materials, 2024, vol. 444, art. 137576.
- Fan J., Zhang Q., Chen X., He Y. Interlaminar Shear Strength Change and Storage Life Prediction of Carbon Fiber/Epoxy Composites with Hygrothermal Accelerated Aging. Polymers, 2024, vol. 16, no. 8, art. 1109.
- Fourari A., Chakkour M., Ould Moussa M., Khay I., Ben Zineb T. A Comprehensive Review on Thermal and Hygro/Hydrothermal Aging of Plant Fiber Composites: Properties, Degradation Mechanisms, and Service Life Prediction. Polymer Composites, 2025, vol. 46, no. 16, pp. 14576-14620.
- Zhelezina G.F., Kulagina G.S., Sidorina A.I., Soloveva N.A. Fatigue of constructional organoplastics. Aviacionnye materialy i tehnologii, 2014, no. 1, pp. 89-100. Available at: http://www.journal.viam.ru (accessed: April 10, 2026). DOI: 10.18577/2713-0193-2024-0-1-89-100.
- Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), pp. 70-80. Available at: http://www.journal.viam.ru (accessed: April 10, 2026). DOI: 10.18577/2713-0193-2021-0-4-70-80.
- Erofeev V.T., Smirnov I.V., Voronov P.V., Afonin V.V., Kablov E.N., Startsev O.V., Startsev V.O., Medvedev I.M. Study of the durability of polymer coatings under the influence of climatic factors of the Black Sea coast. Fundamentalnye issledovaniya, 2016, no. 11, pp. 911-924.
- Startsev V.O., Nizina T.A. The modeling of epoxy polymers weathering by the color characteristics measurements. Trudy VIAM, 2015, no. 12, pp. 80-85. Available at: http://www.viam-works.ru (accessed: April 10, 2026). DOI: 10.18577/2307-6046-2015-0-12-10-10.
- Startsev V.O., Frolov A.S. Influence of climatic influence on the color characteristics of paint and varnish coatings. Lakokrasochnye materialy i ikh primenenie, 2015, no. 3, pp. 16-18.
- Shahid A.T., Garrido M., Correia J.R. Durability under natural outdoor weathering of sustainable composites developed with bio-based unsaturated polyester and epoxy resins reinforced with glass, basalt, and carbon fibres. Construction and Building Materials, 2025, vol. 505, p. 144651.
- Haider I., Khan M.A., Aziz S. et al. Exploring the Weathering and Accelerated Environmental Aging of Wave-Transparent Reinforced Composites. Polymers, 2025, vol. 17, no. 3, p. 357.
- Startsev O.V., Veligodsky I.M., Medvedev I.M., Gladkikh A.V., Gorbovets M.A. Measurement of Strength and Fracture Load of Weathered Samples of Polymer Composite Materials. Polymer Science. Series D, 2024, vol. 17, no. 2, pp. 302-310.
- Aging Effects on Natural Fiber-Reinforced Polymer Composites. Eds. C. Muthukumar, S. Krishnasamy, S.M.K. Thiagamani, S. Siengchin. Singapore: Springer Nature Singapore, 2022. 350 p.
- Hao Z.-H., Zeng J.-J., Chen G.-M. et al. Durability of FRP-to-concrete bonded joints subjected to 110 months accelerated laboratory and field exposure. Engineering Structures, 2024, vol. 305, p. 117681.
- Lebedev M.P., Startsev O.V., Kychkin A.K. The effects of aggressive environments on the mechanical properties of basalt plastics. Heliyon, 2020, vol. 6, no. 3, p. e03481.
- Koval T.V., Veligodsky I.M., Gromova A.A. Study of the plasticizing effect of moisture on the properties of VSE-34 binder based PCMS after 5 years exposure in the different climate zones. Trudy VIAM, 2021, no. 9 (103), pp. 105-116. Available at: http://www.viam-works.ru (accessed: April 10, 2026). DOI: 10.18577/2307-6046-2021-0-9-105-116.
- Startsev V.O., Molokov M.V., Postnov V.I., Starostina I.V. Assessment of the influence of climatic exposure on the properties of fiberglass VPS-53K. Izvestiya Samarskogo nauchnogo tsentra Rossiyskoy Akademii nauk, 2017, vol. 19, no. 4 (2), pp. 220-228.
- Kablov E.N., Startsev O.V., Medvedev I.M. Corrosive aggressiveness of the coastal atmosphere. Part 2. New approaches to assessing the corrosivity of coastal atmospheres. Korroziya: materialy, zashchita, 2016, no. 1, pp. 1-15.
- Kornienko G.V., Startsev O.V., Krotov A.S., Koval T.V. Dependence modeling of the CFRP shear modulus on moisture content. Aviation materials and technologies, 2025, no. 3 (80), pp. 161-178. Available at: http://www.journal.viam.ru (accessed: April 10, 2026). DOI: 10.18577/2713-0193-2025-0-3-161-178.
- Startsev V.O., Panin S.V., Startsev O.V. Sorption and diffusion of moisture in polymer composite materials with impact damage. Mekhanika kompozitnykh materialov, 2015, vol. 51, no. 6, pp. 1081–1094.
- Filistovich D.V., Startsev O.V., Kuznetsov A.A. et al. Effect of moisture on the anisotropy of the dynamic shear modulus of glass-reinforced plastics. Doklady Physics, 2003, vol. 48, no. 6, pp. 306–308.
- Startsev O.V., Krotov A.S., Senatorova O.G. et al. Sorption and diffusion of moisture in layered metal-polymer composite materials of the SIAL type. Materialovedenie, 2011, no. 12, pp. 38–44.
- Kablov E.N., Startsev O.V., Panin S.V. Moisture transfer in carbon-fiber-reinforced plastic with degraded surface. Doklady Physical Chemistry, 2015, vol. 461, no. 2, pp. 80–83.
- Startsev O.V., Makhonkov A.Y., Erofeev V., Gudojnikov S. Impact of moisture content on dynamic mechanical properties and transition temperatures of wood. Wood Material Science and Engineering, 2017, vol. 12, no. 1, pp. 55–62.
- Carslow G., Eger D. Thermal Conductivity of Solids. Moscow: Nauka, 1964, 488 p.
- Lykov A.V. Theory of Thermal Conductivity. Moscow: Vysshaya Shkola, 1967, 600 p.
- Crank J. The mathematics of diffusion. Second ed. Oxford: Clarendon press, 1975, 414 p.
The article was submitted
2026-05-12
approved and accepted for publication after reviewing
2026-05-13