Laptev A.B., Matishov G.G., Bulysheva N.I., Pavlov M.R., Nikolaev E.V. The effect of the transition of air temperature through zero on the surface integrity of a polymer material. Part 2. Freezing of moisture // Proceedings of VIAM. 2026. No. 5 (159). С. 212–224. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-5-212-224.

The effect of the transition of air temperature through zero on the surface integrity of a polymer material

Part 2. Freezing of moisture
Laptev A.B., Matishov G.G., Bulysheva N.I., Pavlov M.R., Nikolaev E.V.
Abstract

The article considers the effect of the temperature transition of a polymer composite material saturated with moisture through a zero value. The study examines the effect of freezing moisture in the pores of a polymer composite. It is shown that in pores larger than 8 nm, ice forms gradually, with intense nucleation at the «air‒water» interface. This leads to the trapping of water in a confined volume. Upon subsequent cooling to –22°C and below, the pressure pore rises, reaching up to 209,9 MPa due to the water-ice phase transition in a constant volume.

Keywords
climatic factors, temperature transition through zero, polymer composite material, ice freezing
Reference list
  1. Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), pp. 70–80. Available at: http://www.journal.viam.ru (accessed: November 18, 2025). DOI: 10.18577/2713-0193-2021-0-4-70-80.
  2. Kablov E.N., Startsev V.O., Laptev A.B. Aging of polymer composite materials. Moscow: NRC «Kurchatov Institute» – VIAM, 2023, 536 p.
  3. Kablov E.N., Kondrashov S.V., Melnikov A.A., Schur P.A. Application of functional and adaptive materials obtained by 3D printing (review). Trudy VIAM, 2022, no. 2 (108), pp. 32–51. Available at: http://www.viam-works.ru (accessed: November 18, 2025). DOI: 10.18577/2307-6046-2022-0-2-32-51.
  4. Laptev A.B., Pavlov M.R., Novikov A.A., Slavin A.V. Current trends in the development of testing materials for resistance to climate factors (review). Part 1. Testing of new materials. Trudy VIAM, 2021, no. 1 (95), pp. 114–122. Available at: http://www.viam-works.ru (accessed: November 18, 2025). DOI: 10.18577/2307-6046-2021-0-1-114-122.
  5. Whiteside M., Herndon J.M. Unequivocal Detection of Solar Ultraviolet Radiation 250–300 nm (UV-C) at Earth's Surface. European Journal of Applied Sciences, 2023, vol. 11, no. 2, pp. 455–472. DOI: 10.14738/aivp.112.14429.
  6. Laptev A.B., Sadkov V.R., Nikolaev E.V., Zeleneva T.O. Effect of wind on temperature and moisture content of material samples during climatic tests. Trudy VIAM, 2025, no. 2 (144), pp. 112–120. Available at: http://www.viam-works.ru (accessed: November 18, 2025). DOI: 10.18577/2307-6046-2025-0-2-112-120.
  7. Tabazadeh A., Djikaev Y.S., Reiss H. Surface crystallization of supercooled water in clouds. Proceedings of the National Academy of Sciences of the United States of America, 2002, vol. 99, pp. 15873–15878.
  8. Debenedetti P.G., Stanley H.E. Supercooled and Glassy Water. Physics Today, 2003, vol. 56, no. 6, pp. 40–46. DOI: 10.1063/1.1595053.
  9. Sharp R.P. Living Ice: Understanding Glaciers and Glaciation. Cambridge: Cambridge University Press, 1988, 225 p.
  10. Sun G., Tanaka H. Surface-induced water crystallisation driven by precursors formed in negative pressure regions. Nature Communications, 2024, vol. 15, art. 6083. DOI: 10.1038/s41467-024-50188-1.
  11. Kulmala M. How Particles Nucleate and Grow. Science, 2003, vol. 302, no. 5647, pp. 1000–1001. DOI: 10.1126/science.1090848.
  12. Herbert R.J., Murray B.J., Dobbie S.J. et al. Sensitivity of liquid clouds to homogenous freezing parameterizations. Geophysical Research Letters, 2015, vol. 42, pp. 1599–1605.
  13. Djikaev Y.S., Tabazadeh A., Hamill P. et al. Thermodynamic conditions for the surface-stimulated crystallization of atmospheric droplets. The Journal of Physical Chemistry A, 2002, vol. 106, no. 43, pp. 10247–10253. DOI: 10.1021/jp0259234.
  14. Espinosa J.R., Sanz E., Valeriani C. et al. Homogeneous ice nucleation evaluated for several water models. The Journal of Chemical Physics, 2014, vol. 141, is. 18, аrt. 18C529. DOI: 10.1063/1.4897524.
  15. Molinero V., Moore E.B. Water modeled as an intermediate element between carbon and silicon. The Journal of Physical Chemistry B, 2009, vol. 113, no. 13, pp. 4008–4016. DOI: 10.1021/jp805227c.
  16. Russo J., Romano F., Tanaka H. New metastable form of ice and its role in the homogeneous crystallization of water. Nature Materials, 2014, vol. 13, pp. 733–739. DOI: 10.1038/nmat3977.
  17. Hayton J.A., Davies M.B., Whale T.F. et al. The limit of macroscopic homogeneous ice nucleation at the nanoscale. Faraday Discussions, 2024, vol. 249, pp. 210–228. DOI: 10.1039/D3FD00118J.
  18. Abascal J.L.F., Sanz E., García Fernández R. et al. A potential model for the study of ices and amorphous water: TIP4P/Ice. The Journal of Chemical Physics, 2005, vol. 122, is. 23, art. 234511. DOI: 10.1063/1.1931662.
  19. Odendahl N.L., Geissler P.L. Local ice-like structure at the liquid water surface. Journal of the American Chemical Society, 2022, vol. 144, no. 25, pp. 11178–11188. DOI: 10.1021/jacs.2c01739.
  20. Ma R., Cao D., Zhu Ch. et al. Atomic imaging of the edge structure and growth of a two-dimensional hexagonal ice. Nature, 2020, vol. 577, pp. 60–63. DOI: 10.1038/s41586-019-1853-4.
  21. Lü Y., Zhang X., Chen M. Size effect on nucleation rate for homogeneous crystallization of nanoscale water film. The Journal of Physical Chemistry B, 2013, vol. 117, no. 35, pp. 10241–10249. DOI: 10.1021/jp405585d.
  22. Fitzner M., Sosso G.C., Cox S.J. et al. Ice is born in low-mobility regions of supercooled liquid water. Proceedings of the National Academy of Sciences of the United States of America, 2019, vol. 116, no. 5, pp. 2009–2014. DOI: 10.1073/pnas.1817135116.
  23. Russo J., Tanaka H. Crystal nucleation as the ordering of multiple order parameters. The Journal of Chemical Physics, 2016, vol. 145, is. 21, art. 211801. DOI: 10.1063/1.4962166.
  24. Russo J., Romano F., Tanaka H. Glass forming ability in systems with competing orderings. Physical Review X, 2018, vol. 8, is. 2, art. 021040. DOI: 10.1103/PhysRevX.8.021040.
  25. Powell-Palm M.J., Rubinsky B., Sun W. Freezing water at constant volume and under confinement. Communications Physics, 2020, vol. 3, art. 39. DOI: 10.1038/s42005-020-0303-9.
  26. Falenty A., Hansen T.C., Kuhs W.F. Formation and properties of ice XVI obtained by emptying a type sII clathrate hydrate. Nature, 2014, vol. 516, no. 7530, pp. 231–233. DOI: 10.1038/nature14014.
  27. Strobel T.A., Somayazulu M., Sinogeikin S.V. et al. Hydrogen-Stuffed, Quartz-like Water Ice. Journal of the American Chemical Society, 2016, vol. 138, no. 42, pp. 13786–13789. DOI: 10.1021/jacs.6b06986.
  28. Laptev A.B., Matishov G.G., Krivushina A.A., Pavlov M.R., Nikolaev E.V. The effect of the transition of air temperature through zero on the surface integrity of a polymer material. Part 1. Moistening. Trudy VIAM, 2025, no. 11 (153), pp. 147–156. Available at: http://www.viam-works.ru (accessed: November 26, 2025). DOI: 10.18577/2307-6046-2025-0-11-147-156.
  29. Lobanov D.S., Vildeman V.E., Babin A.D. et al. Experimental study of the influence of external factors and operational contaminants on the performance of polymer fiber composite materials. Mekhanika kompozitnykh materialov, 2015, vol. 51, no. 1, pp. 97–108.
  30. Kolobkov A.S. Polymer composite materials for various aircraft structures (review). Trudy VIAM, 2020, no. 6–7 (89), pp. 38–44. Available at: http://www.viam-works.ru (accessed: November 18, 2025). DOI: 10.18577/2307-6046-2020-0-67-38-44.
  31. Startsev O.V., Kychkin A.K., Lebedev M.P. et al. Effects of moisture on aging of polymer composite materials in a cold climate. Procedia Structural Integrity, 2020, vol. 30, pp. 162–166. DOI: 10.1016/j.prostr.2020.12.025.
  32. Abdelmola F., Carlsson L.A. State of Water in Void-Free and Void-Containing Epoxy Samples. Journal of Reinforced Plastics and Composites, 2019, vol. 26, pp. 556–566.
  33. Karbhari V.M. Response of Fiber-Reinforced Polymer Concrete Subjected to Freezing and Freeze-Thaw Cycles. Construction and Building Composites, 2002, vol. 6, pp. 35–40.
  34. Heshmati M., Haghani R., Al-Emrani M. Durability of GFRP/Steel under Cyclic Wet-Dry and Freeze-Thaw Conditions. Composites Part B: Engineering, 2017, vol. 126, pp. 211–226.
  35. Jeddí J., Jacquemin F., Vautrin A. Accelerated Hygrothermal Cyclic Tests for Carbon-Epoxy Laminates. Composites Part A: Applied Science and Manufacturing, 2006, vol. 37, pp. 636–645.