Features of the formation of the structure, complex of service properties and the use of hybrid laminate alumopolymer composite materials in aircraft construction

Antipov V.V., Astashkin A.I., Selivanov A.A., Tkachenko E.A.
Antipov V.V., Astashkin A.I., Selivanov A.A., Tkachenko E.A. Features of the formation of the structure, complex of service properties and the use of hybrid laminate alumopolymer composite materials in aircraft construction // Proceedings of VIAM. 2026. No. 3. DOI: 10.18577/2307-6046-2026-0-3-97-113. URL: https://viam-works.ru/en/journal/2026/3/8
Keywords
laminate metal-polymer materials, SIAL aluminum-fiberglass, ALOR aluminum-organoplastics, ALCAR, application, structure, properties of metal-polymer composite materials
Abstract

An overview of scientific information on the structure and properties of hybrid fiber metal laminate aluminum-polymer composite materials is given. The advantages of using fiberglass (in SIAL, GLARE) in comparison with aramid fiber (in ALOR, ARALL) and carbon fiber (in ALCAR, CARALL) are shown. The results of the review show that, in comparison with sheets made of monolithic aluminum alloys, aluminum-glass plastics have a unique set of properties: low density, high specific strength, increased crack resistance, resistance to shock loads, fire resistance and good maintainability. 

Reference list
  1. Laurens B.V. Development of a new hybrid material (ARALL) for aircraft structures. Industrial & Engineering Chemistry, 1983, no. 22 (3), pp. 492–496.
  2. Marissen R. Flight simulation behaviour of aramidreinforced aluminium laminates (ARALL). Engineering Frocfure Mechanics, 1984, vol. 19, no. 2, pp. 261–277.
  3. Zhelezina G.F., Shalin R.E., Perov B.V. et al. Layered metal-polymer composite alor. Organoplastics in aviation products: appendix of Aviation Industry. Moscow: Mashinostroinie, 1985, no. 2, pp. 9–12.
  4. Schijve J. Crack stoppers and ARALL laminates. Engineering Fracture Mechanics, 1990, vol. 31, no. 2, pp. 405–421.
  5. Vogelesang L.B., Gunnink J.W. ARALL: A Materials Challenge for the next Generation of Aircraft. Materials and Design, 1986, vol. 7, no. 6, pp. 287–300.
  6. Postnov V.I., Senatorova O.G., Zhelezina G.F., Kazakov I.A., Abramov P.A., Gerasimov V.A., Postnova M.V. Experience of using MPCM ALOR D16/41 in the nose section of the wing of the An-124-100 aircraft. Aviatsionnye materialy i tekhnologii, 2009, no. 4 (13), pp. 8–17.
  7. Layered composite materials – 98: collection of works of the int. conf. Volgograd, 1998, 352 p.
  8. Friflyander I.N., Senatorova O.G., Anihovckaya L.I., Sidelnikov V.V., Dementeva L.A., Startsev O.V. The Structure and Properties of СИАЛ (Glass/Epoxy – Aluminium) Laminates. Proceedings of the 6th International Conference on Aluminum Alloys (ICAA-6). Toyohashi, 1998, vol. 3, pp. 1957–1963.
  9. Vlot A. Glare history of development of a new aircraft material. Kluwer Academic Publishers, 2001, 527 р.
  10. Lin C.T., Kao P.W., Yang F.S. Fatigue behaviour of carbon fibre-reinforced aluminium laminates. Composites, 1991, no. 22 (2), pp. 135–141.
  11. Voynov S.I., Zhelezina G.F., Ilyichev A.V., Solovieva N.A. Study of mechanical characteristics of layered metal-polymer composite material based on aluminum sheets and carbon fiber layers. Voprosy materialovedeniya, 2018, no. 4 (96), рp. 86–96.
  12. Voynov S.I., Zhelezina G.F., Solovieva N.A. Influence of initial components on the mechanical characteristics of layered metal-polymer composite material «aluminum–carbon fiber». Materialovedenie, 2017, no. 5, рp. 38–42.
  13. Voynov S.I., Zhelezina G.F., Pavlovskaya T.G., Volkov I.A. Problem of contact corrosion in the creation of layered metal-polymer composite materials based on aluminum and carbon fiber. Voprosy materialovedeniya, 2016, no. 1 (85), рр. 127–133.
  14. Laminated aluminum-fiberglass plastic and a product made therefrom: pat. 2600765 Rus. Federation; appl. 10.06.15; publ. 04.10.16.
  15. Zichenkov M.Ch., Shanygin A.N. New-generation hybrid aircraft structures for advanced civil aircraft. Polet, 2018, no. 11, pp. 106–114.
  16. Shestov V.V., Antipov V.V., Serebrennikova N.Yu., Nefedova Yu.N. High-strength layered material based on aluminum-lithium alloy sheets. Tekhnologiya legkikh splavov, 2016, no. 1, pp. 119–123.
  17. Lavrov A.V., Erasov V.S., Podzhivotov N.Yu., Avtaev V.V. Optimization of structure of hybrid composition materials for aircraft. Trudy VIAM, 2016, no. 11 (47), pp. 56–62. Available at: http://www.viam-works.ru (accessed: September 07, 2025). DOI: 10.18577/2307-6046-2016-0-11-7-7.
  18. Kablov E.N., Antipov V.V., Senatorova O.G. Layered aluminum-fiberglass plastics SIAL-1441 and cooperation with Airbus and TU Delft. Tsvetnye metally, 2013, no. 9, pp. 50–53.
  19. Antipov V.V. Scientific and technological foundations for the development of layered hybrid composite materials of the SIAL type with variable physical and mechanical properties based on sheets of aluminum-lithium alloys and fiberglass: thesis, Dr Sc. (Tech.). Samara, 2021, 316 p.
  20. Duyunova V.A., Kutyrev A.E., Serebrennikova N.Yu., Vdovin A.I., Somov A.V. Examination of the impact of aggressive environmental factors on the development of corrosion damage on samples of laminated glass-reinforced plastic of SIAL class. Aviation materials and technologies, 2021, no. 4 (65), pp. 81–90. Available at: http://www.journal.viam.ru (accessed: December 01, 2025). DOI: 10.18577/2713-0193-2021-0-4-81-90.
  21. Zhelezina G.F., Kulagina G.S., Kan A.Ch., Solovyova N.A. Research of corrosion resistance of the hybrid layered metal polymeric materials. Trudy VIAM, 2024, no. 8 (138), pp. 38–47. Available at: http://www.viam-works.ru (accessed: December 01, 2025). DOI: 10.18577/2307-6046-2024-0-8-38-47.
  22. Antipov V.V., Serebrennikova N.Yu., Senatorova O.G., Morozova L.V., Lukina N.F., Nefedova Yu.N. Hybrid layered materials with a low rate of fatigue crack development. Vestnik mashinostroyeniya, 2016, no. 12, pp. 45–49.
  23. Zhelezina G.F., Kolobkov A.S., Kulagina G.S., Kan A.Ch. Damping properties of hybrid layered metal-polymer materials based on aluminum, titanium alloys and organoplastics layers. Trudy VIAM, 2021, no. 2 (96), pp. 10–19. Available at: http://www.viam-works.ru (accessed: December 01, 2025). DOI: 10.18577/2307-6046-2021-0-2-10-19.
  24. Antipov V.V., Zaitsev M.D., Rodchenko T.S., Stoyda Yu.M., Serebrennikova N.Yu., Sidelnikov V.V. Study of the durability of a structurally similar sample of a fuselage panel with a skin made of SIAL aluminum-fiberglass plastic. Deformatsiya i razrusheniye materialov, 2021, no. 3, pp. 18–24.
  25. Antipov V.V., Oglodkov M.S., Selivanov A.A., Samokhvalov S.V., Nefedova Yu.N. Evaluation of the resistance of laminated aluminum-fiberglass plastics to impact loads. Voprosy materialovedeniya, 2025, no. 4 (124), pp. 130–132.
  26. Qi С., Zhidong G., Zengshan L. et al. Experimental investigation on impact performances of GLARE laminates. Chinese Journal of Aeronautics, 2015, vol. 28, is. 6, pp. 1784–1792.
  27. Antipov V.V., Senatorova O.G., Sidelnikov V.V. Research of fire firmness layered hybrid aluminum fibreglasses of SIAL’s class. Aviacionnye materialy i tehnologii, 2011, no. 3, pp. 36–41.
  28. Antipov V.V., Konovalov A.N., Serebrennikova N.Yu., Somov A.V., Nefedova Yu.N. Influence of structure on fire resistance and fireproof FMLS SIAL-type and possibility of application of data of materials in aircraft industry. Trudy VIAM, 2019, no. 1 (73), pp. 40–46. Available at: http://www.viam-works.ru (accessed: December 01, 2025). DOI: 18577/2307-6046-2019-0-1-40-46.
  29. Organization Standard 1-595-20-532–2017. Assessment of fire resistance and fire impermeability of materials intended for fire-hazardous zones in aviation equipment. Moscow: VIAM, 2017, 23 p.
  30. Fire-resistant laminated metal-fiberglass plastic and products made from it: pat. 2676637 Rus. Federation; appl. 07.05.18; publ. 09.01.19.
  31. Roebroeks G.H.J.J. GLARE: a structural material for fire resistant aircraft fuselages. Aircraft Fire Safety, AGARD Conference Proceedings, 1996, vol. 587, pp. 26-1–26-13.
  32. Serebrennikova N.Yu., Antipov V.V., Senatorova O.G., Erasov V.S., Kashirin V.V. Hybrid multilayer materials based on aluminum-lithium alloys applied to panels of plane wing. Aviacionnye materialy i tehnologii, 2016, no. 3 (42), pp. 3–8. DOI: 10.18577/2071-9140-2016-0-3-3-8.
  33. Antipov V.V., Somov A.V., Sidelnikov V.V., Nefedova Yu.N., Ogurtsov P.S., Soloviev V.A. Technological features of shaping fire-resistant light laminated material for helicopter engine hood manufacturing. Aviation materials and technologies, 2023, no. 3 (72), pp. 90–100. Available at: http://www.journal.viam.ru (accessed: December 01, 2025). DOI: 10.18577/2713-0193-2023-0-3-90-100.
  34. Method of joining laminated aluminum-fiberglass: pat. 2570469 Rus. Federation; appl. 10.09.14; publ. 10.12.15.
  35. Antipov V.V., Sidelnikov V.V., Samokhvalov S.V., Nefedova Yu.N., Somov A.V. Methods of joining aluminum-fiberglass by splicing for the manufacture of large-sized aircraft skin panels. Vestnik mashinostroeniya, 2022, no. 11, pp. 58–63.
  36. Bucci R.J., Kulak M., Heinimann M.B. et al. Large Panel Validation of Advanced Metallic and Hybrid Structural Concepts for Next-Gen Transport Aircraft. AeroMat 2007. Baltimore, 2007. Available at: https://asm.confex.com/ (accessed: December 01, 2025).
  37. Fredell R.S., Gunnink J.W., Bucci R.J., Hinrichsen J. «Care-free» hybrid wing structures for aging USAF transports: First International Conference on Damage Tolerance of Aircraft Structures. Available at: https://www.researchgate.net/publication/228415487_Carefree_Hybrid_Wing_Structures_for_Aging_USAF_Transports (accessed: December 01, 2025).
  38. Sinmazçelik T., Avcu E., Bora M.Ö., Çoban O. A review: Fibre metal laminates, background, bonding types and applied test methods. Materials and Design, 2011, vol. 32, pp. 3671–3685.
  39. Antipov V.V., Lavro N.A., Sukhoivanenko V.V., Senatorova O.G. Experience of using Al–Li alloy 1441 and layered material based on it in seaplanes. Tsvetnyye metally, 2013, no. 8, pp. 46–50.
  40. Podzhivotov N.Yu., Kablov E.N., Antipov V.V. et al. Layered metal-polymer materials in aircraft structural elements. Perspektivnye materialy, 2016, no. 10, pp. 5–19.
  41. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  42. Antipov V.V., Serebrennikova N.Yu., Konovalov A.N., Nefedova Yu.N. Perspectives of application of fiber metal laminate materials based on aluminum alloys in aircraft design. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 45–53. DOI: 10.18577/2071-9140-2020-0-1-45-53.