Epoxy binders for FR-4 grade dielectric materials

Sarychev I.A. S, Serkova E.A., Mishurov K.S., Payarel S.M.
Sarychev I.A. S, Serkova E.A., Mishurov K.S., Payarel S.M. Epoxy binders for FR-4 grade dielectric materials // Proceedings of VIAM. 2026. No. 1. DOI: 10.18577/2307-6046-2026-0-1-136-149. URL: https://viam-works.ru/en/journal/2026/1/10
Keywords
epoxy resin, hardener, fire retardant, filler, binder, dielectric, fiberglass, flammability
Abstract

The article presents a review of the component base of modern epoxy binders for FR-4 class dielectrics. The main types of resins, hardeners, fire retardants and various functional additives are considered, and their structural formulas are given. The influence of binder components on the properties of dielectrics is described. The possibility of wide modification of the binder to achieve the required properties of the dielectric is indicated. The properties of the VSE-79 epoxy binder and experimental samples of dielectrics based on it are presented.

Reference list
  1. Mylov G.V. Printed circuit boards: selection of base materials. Moscow: Goryachaya Liniya – Telecom, 2015, 176 p.
  2. Halogen-free resin composition, copper clad laminate using the same, and printed circuit board using the same: pat. US20140178697A1; appl. 15.03.13; publ. 26.06.14.
  3. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  4. Petrova A.P., Malysheva G.V. Adhesives, adhesive binders and adhesive prepregs. Ed. E.N. Kablov. Moscow: VIAM, 2017, 472 p.
  5. Goosey M. Plastics for Electronics. Netherlands: Springer, 1999, 408 p.
  6. Epoxy resin compositions for use in electrical laminates: pat. US5405931A; appl. 13.08.93; publ. 11.04.95.
  7. Resin composition for printed wiring board, prepreg, and laminate obtained with the same: pat. EP1637554A1; appl. 03.06.03; publ. 22.03.06.
  8. Peng Y.-R., Qi X. The influence of curing systems on epoxide-based PCB laminate performance. Circuit World, 2005, vol. 31, no. 4, pp. 14–20.
  9. Luda M.P., Balabanovich A.I., Zanetti M. Thermal decomposition of fire retardant brominated epoxy resins cured with different nitrogen containing hardeners. Polymer Degradation and Stability, 2007, vol. 92 (6), pp. 1088–1100.
  10. Thermoset resin composition, and prepreg and laminate for printed circuit board manufactured therefrom: pat. US20150159016A1; appl. 29.12.11; publ. 11.07.15.
  11. Lowdielectric resin composition, copper clad laminate using the same, and printed circuit board using the same: pat. US20140174802A; appl. 26.02.13; publ. 26.06.14.
  12. Kablov E.N., Startsev V.O. Measurement and forecasting of materials samples’ temperature during weathering in different climatic zones. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 47–58. DOI: 10.18577/2071-9140-2020-0-4-47-58.
  13. Epoxy resin composition and prepreg and copper clad laminate manufactured by using the same: pat. US20140342161A1; appl. 28.10.11; publ. 20.11.14.
  14. Resin composition, copper clad laminate and printed circuit board using same: pat. US9850375B2; appl. 23.08.13; publ. 26.12.17.
  15. Barinov D.Ya., Shorstov S.Yu., Razmahov M.G., Gulyaev A.I. Examination of thermophysical characteristics of a heat-protective material based on fiberglass during destruction. Aviation materials and technologies, 2021, no. 4 (65), pp. 91–97. Available at: http://www.journal.viam.ru (accessed: April 17, 2025). DOI: 10.18577/2713-0193-2021-0-4-91-97.
  16. Curing epoxy resins using dicy, imidazole and acid: pat. US5508328; appl. 17.11.94; publ. 16.04.96.
  17. Malysheva G.V., Marakhovskiy P.S., Barinov D.Ya., Nikolaev E.V. Optimization of the curing modes of fiber-glass based on epoxy binder. Aviation materials and technologies, 2023, no. 2 (71), pp. 94–103. Available at: http://www.journal.viam.ru (accessed: April 17, 2025). DOI: 10.18577/2713-0193-2023-0-2-94-103.
  18. Kablov E.N., Chursova L.V., Lukina N.F., Kutsevich K.E., Rubtsova E.V., Petrova A.P. Study of epoxy-polysulfone polymer systems as the basis for high-strength adhesives for aviation purposes. Klei. Germetiki. Tekhnologii, 2017, no. 3, pp. 7–12.
  19. Zastrogina O.B., Serkova E.А., Sarychev I.A., Vavilova M.I. Influence of Russian and Chinese vinyflex on the properties of the VFT binder and fiberglass based on it. Aviacionnye materialy i tehnologii, 2020, no. 3 (60), pp. 3–9. DOI: 10.18577/2071-9140-2020-0-3-3-9.
  20. SMA resin formulation: pat. US11365282B2; appl. 25.07.17; publ. 21.06.22.
  21. Flame retardants in printed circuit boards. Available at: https://www.epa.gov/sites/default/files/2015-08/documents/pcb_ch3.pdf (accessed: April 17, 2025)
  22. An Overwie of Flame Retardants in Printed Circuit Boards for LEDs and other Electronic Devices. Journal of Materials and Environmental Science, 2023, vol. 14 (04), pp. 410–420.
  23. Stunning Reversal: EU Axes RoHS Directive’s TBBP-A and MCCPs Restriction Proposals. Available at: https://www.cirs-group.com/en/chemicals/stunning-reversal-eu-axes-rohs-directive-tbbp-a-and-mccps-restriction-proposals (accessed: April 17, 2025).
  24. Flame retardants in printed circuit boards. Available at: https://www.epa.gov/sites/default/files/2015-08/documents/pcb_ch2.pdf (accessed: April 17, 2025).
  25. Schartel B. Phosphorus-based Flame Retardancy Mechanisms-Old Hat or a Starting Point for Future Development? Materials, 2010, vol. 3 (10), pp. 4710–4745.
  26. IEC 61249-2-21 for Halogen Free. Available at: https://www.masterbond.com/certifications/halogen-free (accessed: April 17, 2025).
  27. Halogen-free flame retardant epoxy resin composition, prepreg, and copper clad lamination: pat. US20080241578A1; appl. 29.08.07; publ. 02.10.08.
  28. Copper clad laminate and method for manufacturing the same: pat. US20150266267А1; appl. 21.03.13; publ. 24.09.15.
  29. Halogen-free resin composition, copper clad laminate using the same, and printed circuit board using the same: pat. US20140322541А1; appl. 10.08.13; publ. 30.10.14.
  30. Startsev O.V., Kablov E.N., Makhonkov A.Yu. Regularities of the α-transition of epoxy binders of composite materials according to the data of dynamic mechanical analysis. Bulletin of Bauman MSTU. Ser.: Mechanical Engineering, 2011, no. SP2, pp. 104–113.
  31. Composite and copper clad laminate made therefrom: pat. US20220022314А1; appl. 21.03.21; publ. 20.06.22.
  32. Sho S., Arefazar A., Khosrokhavar R. Silane Coupling Agents in Polymer-based Reinforced Composites: A Review. Journal of Reinforced Plastics and Composites, 2008, vol. 27 (5), pp. 473–485.
  33. Nakamura T., Tabuchi H., Hirai T. et al. Effects of silane coupling agent hydrophobicity and loading method on water absorption and mechanical strength of silica particle-filled epoxy resin. Journal of Applied Polymer Science, 2019, vol. 137 (17), no. 48615, pp. 1–11.
  34. Copper clad laminate, prepreg and method of reducing signal loss: pat. US20100248569А1; appl. 05.02.10; publ. 30.09.10.
  35. Homogeneousbsmalemde trazine-epoxy compositions useful for the manufacture of electrical laminates: pat. US20110247756А1; appl. 11.12.09; publ. 13.10.11.
  36. Olin-Epoxy-Asia-Pacific-Product-Brochure. Available at: https://olinepoxy.com/wp-content/uploads/2018/05/Olin-Epoxy-Asia-Pacific-Product-Brochure.pdf (accessed: 17.04.2025).
  37. Isola DE104. Available at: https://www.isola-group.com/pcb-laminates-prepreg/de104-laminate-and-prepreg (accessed: April 17, 2025).