Determination of characteristics of radiographic films

Osiyanenko N.V., Kosarina E.I., Demidov A.A., Grimova A.P.
Osiyanenko N.V., Kosarina E.I., Demidov A.A., Grimova A.P. Determination of characteristics of radiographic films // Proceedings of VIAM. 2025. No. 7. DOI: 10.18577/2307-6046-2025-0-7-119-129. URL: https://viam-works.ru/en/journal/2025/7/9
Keywords
radiographic film, optical density, characteristic curve, sensitometric characteristics, gradient, speed to radiation
Abstract

The article describes the testing of radiographic technical films according to the regulations of GOST R ISO 11699-1–2023 and according to the method developed at NRC «Kurchatov Institute» – VIAM. The obtained informative characteristics of radiographic films are compared. The article shows that obtaining a characteristic curve according to the requirements of GOST R ISO 11699-1–2023 does not take into account the influence of X-ray radiation energy. The properties of the analog of the characteristic curve according to the developed method take into account its dependence on the radiation energy, i.e. it determines not only its sensitometric properties, but also its flaw detection properties.

Reference list
  1. Kablov E.N., Antipov V.V., Oglodkova Yu.S., Oglodkov M.S. Experience and prospects for the use of aluminum-lithium alloys in aviation and space technology. Metallurg, 2021, no. 1, pp. 62–70.
  2. Kablov E.N., Ospennikova O.G., Kudinov I.I., Golovkov A.N., Generalov A.S., Knyazev A.V. Assessment of the probability of detecting operational defects in aircraft parts made of heat-resistant alloys using flaw detection fluids of domestic and foreign production. Defektoskopiya, 2021, no. 1, pp. 64–71.
  3. Kablov E.N., Belov E.V., Trapeznikov A.V., Leonov A.A., Zaitsev D.V. Strengthening features and aging kinetics of high-strength cast aluminum alloy AL4MS based on Al–Si–Cu–Mg system. Aviation materials and technologies, 2021, no. 2 (63), paper no. 03. Available at: http://www.journal.viam.ru (accessed: March 21, 2024). DOI: 10.18577/2713-0193-2021-0-2-24-34.
  4. State Standard R ISO 11699-1‒2023. Non-destructive testing. Radiographic films for industrial radiography. Part 1. Classification of film systems for industrial radiography. Moscow: RST, 2023, 12 p.
  5. Kosarina E.I., Stepanov A.V., Demidov A.A., Krupnina O.A. Testing methods for radiographic films. Vestnik MGTU im. Baumana. Ser.: Mashinostroenie, 2015, no. 3, pp. 80–89.
  6. Rashchupkin V.P., Korytov M.S. Metal defects: textbook. Omsk: SibADI Publ. House, 2006, 38 p.
  7. Klyuev V.V., Sosnin F.R. Theory and Practice of Radiation Monitoring: A Textbook for University Students. Moscow: Mashinostroenie, 1998, 170 p.
  8. Kuleshov V.K., Sertakov Yu.I., Efimov P.V., Shumikhin V.F. Radiographic Testing Practice: A Manual. Tomsk: Tomsk Polytech. Univ. Publ. House, 2009, 288 p.
  9. Gnedin M.M., Shablov S.V. Requirements of Regulatory Documentation for Selecting Radiographic Film. V mire nerazrushayushchego kontrolya, 2019, no. 1, pp. 14–19.
  10. Velichko V.Ya. Quality Parameters of Radiographic Images of Welded Joints According to the New Standards GOST ISO 17636-1.2–2017. V mire nerazrushayushchego kontrolya, 2018, no. 3, pp. 46–55.
  11. Demidov A.A., Kosarina E.I., Kourova N.V., Mikhailova N.A. Sensitometer for building characteristic curves of x-ray films and determining the sensitivity to radiation and gradient in accordance with ISO 11699-1:2008 requirements. Trudy VIAM, 2020, no. 6-7 (89), paper no. 09. Available at: http://www.viam-works.ru (accessed: December 12, 2024). DOI: 10.18577/2307-6046-2020-0-67-81-90.
  12. Makarov A.V. Chemical and photographic processing of radiographic films. V mire nerazrushayushchego kontrolya, 2021, no. 1, pp. 60–68.
  13. Kovalenko T.S. «Burned» type defect on cast billets of heat-resistant nickel alloys (type ZhS32). Aviation materials and technologies, 2023, no. 4 (73), paper no. 02. Available at: http://www.journal.viam.ru (accessed: December 19, 2024). DOI: 10.18577/2713-0193-2023-0-4-14-22.
  14. Leonov A.A., Trofimov N.V., Panaetov V.G., Kudasov S.V., Shirokozhukov А.V. Magnesium alloys in the design of navigation system products. Aviation materials and technologies, 2024, no. 3 (76), paper no. 03. Available at: http://www.journal.viam.ru (accessed: December 15, 2024). DOI: 10.18577/2713-0193-2024-0-3-25-34.
  15. Svetlov I.L., Petrushin N.V., Epishin A.I., Karashaew M.M., Elyutin E.S. Single crystals of nickel-based superalloys alloyed with rhenium and ruthenium (review). Part 1. Aviation materials and technologies, 2023, no. 1 (70), paper no. 03. Available at: http://www.journal.viam.ru (accessed: December 20, 2024). DOI: 10.18577/2713-0193-2023-0-1-30-50.
  16. Makarov A.V. New documents on non-destructive testing in the field of nuclear energy. Radiographic testing. V mire nerazrushayushchego kontrolya, 2020, no. 2, pp. 46–51.