Electrolyte-plasma polishing of parts made by selective laser sintering from metal powder composition of aluminum alloy grade VAS1
Part 2
UDC
669.018.95:621.791.724
DOI
10.18577/2307-6046-2025-0-3-3-11
Article PDF (Russian)
(740.66 KB)
How to cite
Dobrynin D.A., Pavlova T.V. Electrolyte-plasma polishing of parts made by selective laser sintering from metal powder composition of aluminum alloy grade VAS1. Part 2 // Proceedings of VIAM. 2025. No. 3. DOI: 10.18577/2307-6046-2025-0-3-3-11. URL: https://viam-works.ru/en/journal/2025/3/1
Keywords
electrochemical treatment, electrolyte-plasma polishing, 3D-printing, selective laser sintering, metal powder composition, aluminum alloy grade VAS1, structurally similar sample
Abstract
The influence of additives in the base electrolyte, operating voltage and temperature of the electrolyte on the quality of the process of electrolyte-plasma polishing of parts manufactured by selective laser sintering from a metal powder composition of aluminum alloy grade VAS1 was studied. Electrolyte-plasma polishing of a structurally similar sample of a «bracket» type part was carried out. A technology has been developed for electrolyte-plasma polishing of parts manufactured by the selective laser sintering method from metal powder composition aluminum alloy grade VAS1.
Reference list
- Kablov E.N., Evgenov A.G., Bakradze M.M., Nerush S.V., Krupnina O.A. New generation materials and digital additive technologies for the production of resource parts of FSUE VIAM. Part 1. Materials and synthesis technologies. Elektrometallurgiya, 2022, no. 1, pp. 2–12. DOI: 10.31044/1684-5781-2022-0-1-2-12.
- Kablov E.N., Evgenov A.G., Petrushin N.V., Bazyleva O.A., Mazalov I.S., Dynin N.V. New generation materials and digital additive technologies for the production of resource parts of FSUE VIAM. Part 3. Adaptation and creation of materials. Elektrometallurgiya, 2022, no. 4, pp. 15–25. DOI: 10.31044/1684-5781-2022-0-4-15-25.
- Kablov E.N., Evgenov A.G., Petrushin N.V., Bazyleva O.A., Mazalov I.S. New-generation materials and digital additive technologies for the production of resource parts of FSUE VIAM. Part 4. Development of heat-resistant materials. Elektrometallurgiya, 2022, no. 5, pp. 8–19. DOI: 10.31044/1684-5781-2022-0-5-8-19.
- Shchetinina N.D., Kuznetsova P.E., Dynin N.V., Selivanov A.A. Aluminum alloys with additions of Sc and Zr in additive manufacturing (review). Aviation materials and technologies, 2021, no. 3 (64), paper no. 03. Available at: http://www.journal.viam.ru (accessed: September 10, 2024). DOI: 10.18577/2713-0193-2021-0-3-19-34.
- Peskova A.V., Sukhov D.I., Mazalov P.B. Examination of the formation of the titanium alloy VT6 structure obtained by additive manufacturing. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 38–44. DOI: 10.18577/2071-9140-2020-0-1-38-44.
- Nerush S.V., Sviridov A.V., Afansiev-Khodykin A.N., Galushka I.A., Tarasov S.A. Development of brazing technology for parts obtained by additive technologies from cobalt based metal powder composition. Aviation materials and technologies, 2022, no. 2 (67), paper no. 02. Available at: http://www.journal.viam.ru (accessed: September 10, 2024). DOI: 10.18577/2713-0193-2022-0-2-18-29.
- Marakhovskij P.S., Barinov D.Ya., Shorstov S.Yu., Vorobev N.N. On creation of physical and mathematical models of heat and mass transfer during manufacturing by additive technologies (review). Aviation materials and technologies, 2022, no. 2 (67), paper no. 10. Available at: http://www.journal.viam.ru (accessed: September 10, 2024). DOI: 10.18577/2713-0193-2022-0-2-111-119.
- Galvanic coatings in mechanical engineering: a reference book in 2 vols. Ed. M.A. Shluger. Moscow: Mashinostroenie, 1985, vol. 1, 240 p.
- Mirzoev R.A., Davydov A.D. Anodic processes of electrochemical and chemical processing of metals: a textbook. St. Petersburg: Publ. house of the Polytech. Univ., 2013, 382 p.
- Kulikov I.S., Vaschenko S.V., Kamenev A.Ya. Electrolytic-plasma processing of materials. Minsk: Belarusian Navuka, 2010, 232 p.
- Method of electrolytic-plasma processing of products made of aluminum and aluminum alloys: pat. 7291 Republic of Belarus; appl. 16.07.15; publ. 28.02.17.
- Zakharov S.V., Korotkikh M.T. Electrolyte-plasma polishing of complex-shaped products made of aluminum alloy D16. Vestnik Kontserna VKO «Almaz–Antey», 2017, no. 3, pp. 83–87.
- Pogrebnyak A.D., Tyurin Yu.N., Boyko A.G. et al. Electrolyte-plasma treatment and coating of metals and alloys. Uspekhi fiziki metallov, 2005, vol. 6, pp. 273–344.
- Volenko A.P., Boychenko O.V., Chirkunova N.V. Electrolyte-plasma treatment of metal products. Vektor nauki TGU, 2012, no. 4 (22), pp. 144–147.
- Grilikhes S. Ya. Degreasing, etching and polishing of metals. Ed. P.M. Vyacheslavov. 5th ed., rev. and add. Leningrad: Mashinostroenie, 1983, 101 p.