Methods for measuring and improving the crack resistance of silicon carbide composite materials

Erin K.D., Sorokin O.Ju., Monin S.A., Gorbovets M.A.
Erin K.D., Sorokin O.Ju., Monin S.A., Gorbovets M.A. Methods for measuring and improving the crack resistance of silicon carbide composite materials // Proceedings of VIAM. 2024. No. 11. DOI: 10.18577/2307-6046-2024-0-11-44-70. URL: https://viam-works.ru/en/journal/2024/11/5
Keywords
fracture toughness, crack resistance, ceramic composite materials, silicon carbide, bending, indentation, mechanical properties
Abstract

This literature review discusses methods for determining the fracture toughness of ceramic composite materials. The main methods for increasing crack growth resistance are given. Methods for determining mechanical properties using Vickers pyramid indentation, the three- and four-point bending method, and computer modeling of the crack growth process, including at elevated temperatures, are considered. The main disadvantages of each way of determining mechanical properties are presented.

Reference list
  1. Burkovskaya N.P., Sevostyanov N.V. Cermets for plain bearings (review). Trudy VIAM, 2023, no. 3 (121), paper no. 08. Available at: http://www.viam-works.ru (accessed: January 14, 2024). DOI: 10.18577/2307-6046-2023-0-3-84-94.
  2. Voronov V.A., Chainikova A.S., Lebedeva Yu.E., Zhitnyuk S.V. Production, physico-mechanical and tribotechnical properties of hot-pressed carbon-ceramic composite material on the basis of silicon carbide. Aviation materials and technologies, 2022, no. 2 (67), paper no. 07. Available at: http://www.journal.viam.ru (accessed: January 14, 2024). DOI: 10.18577/2713-0193-2022-0-2-74-84.
  3. Tyutin S.S., Ilyakhinsky I.A., Kamnev M.A., Afrikantov G.G. Comparative evaluation of prototypes of bearing shells for sealed electric pumps for resistance to high-parameter water. Reports Sci.-Pract. Conf. «Nuclear technologies: from research to implementation–2019». N. Novgorod: NSTU named after R.E. Alekseev, 2019, pp. 49–50.
  4. Kablov E.N., Grashchenkov D.V., Isaeva N.V., Solntsev S.S. Promising high-temperature ceramic composite materials. Rossiyskiy khimicheskiy zhurnal, 2010, vol. 54, no. 1, pp. 20–24.
  5. Kablov E.N., Grashchenkov D.V., Isaeva N.V. High-temperature fiber-free ceramic composite material. Abstract Int. Sci.-Tech. conf. «Actual issues of aviation materials science». Moscow: VIAM, 2007, p. 83.
  6. Gnesin G.G. Silicon carbide materials. Moscow: Metallurgiya, 1977, 215 p.
  7. Grinchuk P.S., Kiyashko M.V., Stepkin M.O. et al. Production of dense reaction-bonded ceramics based on silicon carbide. Heat and mass transfer–2017. Minsk, 2017, pp. 56–86.
  8. Kiyashko M.V. Regularities of formation of ceramics based on reaction-bonded silicon carbide in the presence of free silicon: abstract thesis, Cand. Sc. (Phys. & Math). Minsk, 2023, 29 p.
  9. Zhitnyuk S.V., Sorokin O.Yu., Zhuravleva P.L. Silicon carbide ceramics obtained by sintering granular powder. Trudy VIAM, 2020, no. 2 (86), paper no. 06. Available at: http://www.viam-works.ru (accessed: February 05, 2024). DOI: 10.18577/2307-6046-2020-0-2-50-59.
  10. Sevastyanov V.G., Simonenko E.P., Simonenko N.P., Grashchenkov D.V., Solntsev S.S., Ermakova G.V., Prokopchenko G.M., Kablov E.N., Kuznetsov N.T. Production of silicon carbide whiskers using the sol-gel method in the bulk of SiC ceramics. Kompozity i nanostruktury, 2014, vol. 6, no. 4, pp. 198–211.
  11. Yan J., Zhang Zh., Kuriyagawa T. Mechanism for material removal in diamond turning of reaction-bonded silicon carbide. International Journal of Machine Tools & Manufacture, 2009, vol. 49, pp. 366–374. DOI: 10.1016/j.ijmachtools.2008.12.007.
  12. Cook J., Gordon J., Evans C., Marsh D. A mechanism for the control of crack propagation in all-brittle systems. Proceedings of the Royal Society of London A: Mathematical, Physical and Engineering Sciences. The Royal Society, 1964, рр. 508–520.
  13. Clegg W., Kendall K., Alford N.M., Button T., Birchall J. A simple way to make tough ceramics. Nature, 1990, vol. 347, is. 6292, pp. 455–457.
  14. Sevostyanova I.N., Han Liang, Buyakova S.P. Formation of the structure and properties of
  15. heteromodular multicomponent ceramic composite materials based on zirconium diboride. Reports Int. Conf. «Physical mesomechanics. Materials with a multilevel hierarchically organized structure and intelligent technologies». Tomsk, 2023, pp. 580–581.
  16. Kablov E.N., Shchetanov B.V., Ivakhnenko Yu.A., Balinova Yu.A. Promising reinforcing high-temperature fibers for metal and ceramic composite materials. Aviacionnye materiay i tehnologii, 2005, no. 2, pp. 3–5.
  17. Popov O., Chornobuk S., Vishnyakov V. Structure formation of TiB2–TiC–B4C–C hetero-modulus ceramics via reaction hot pressing. International Journal of Refractory Metals and Hard Materials, 2017, vol. 64, pp. 106–112. DOI: 10.1016/j.ijrmhm.2017.01.012.
  18. Popov O., Vishnyakov V. Fracture toughness in some hetero-modulus composite carbides: carbon inclusions and voids. Advances in Applied Ceramics, 2017, vol. 116, no. 2, pp. 61–70. DOI: 10.1080/17436753.2016.1208470.
  19. Chakrabarti O.P., Ghosh S., Mukerji J. Influence of grain size, free silicon content and temperature on the strength and toughness of reaction-bonded silicon carbide. Ceramics International, 1994, vol. 20, pp. 283–286. DOI: 10.1016/0272-8842(94)90042-6.
  20. Wilhelm M., Wruss W. Influence of annealing on the mechanical properties of SiC–Si composites with sub-micron SiC microstructures. Journal of the European Ceramic Society, 2000, vol. 20, pp. 1205–1213. DOI: 10.1016/S0955-2219(99)00275-7.
  21. Wang Y., Tan S., Jiang D. The effect of porous carbon preform and the infiltration process on the properties of reaction-formed SiC. Carbon, 2004, vol. 42, pp. 1833–1839. DOI: 10.1016/j.carbon.2004.03.018.
  22. Huang Q.W., Zhu L.H. High-temperature strength and toughness behaviors for reaction-bonded SiC ceramics below 1400 °C. Materials letters, 2005, vol. 59, pp. 1732–1735. DOI: 10.1016/j.matlet.2005.01.049.
  23. Friedman Ya.B. Mechanical properties of metals: in 2 parts. Moscow: Mashinostroenie, 1972, part 2: Mechanical tests. Structural strength, 368 p.
  24. Gnesin B.A. Possibilities of controlling the connectivity of silicon carbide in silicon carbide - molybdenum silicide composite materials. Nauka i obrazovanie, 2014, no. 12, pp. 941–950. DOI: 10.7463/1214.0751844.
  25. Perevislov S.N. Evaluation of crack resistance of reaction-sintered composite materials based on boron carbide. Novye ogneupory, 2019, no. 3, pp. 49–54. DOI: 10.17073/1683-4518-2019-3-49-54.
  26. Chicot D., Tricoteaux A. Mechanical Properties of Ceramic by Indentation: Principle and Applications. Ceramic Materials. InTech, 2010, pp. 116–154.
  27. Oreshko E.I., Erasov V.S., Utkin D.A., Avtayeva Ya.V. The equipment for definition of physicomechanical characteristics of materials by press-in method (review). Aviation materials and technologies, 2021, no. 4 (65), paper no. 12. Available at: http://www.journal.viam.ru (accessed: February 12, 2024). DOI: 10.18577/2713-0193-2021-0-4-107-124.
  28. Rao X., Zhang F., Luo X., Ding F. Characterization of hardness, elastic modulus and fracture toughness of RB–SiC ceramics at elevated temperature by Vickers test. Materials Science and Engineering: A, 2019, vol. 744, pp. 426–435. DOI: 10.1016/j.msea.2018.12.044.
  29. Lapitskaya V.A., Kuznetsova T.A., Chizhik S.A., Grinchuk P.S. Determination of crack resistance using AFM. Reports XIII Int. Conf. «Methodological aspects of scanning probe microscopy». Minsk, 2018, pp. 260–266.
  30. Lynn A. Development and characterization of spiral additions in a ceramic matrix. Materials science and engineering: Masters Theses, 2014, no. 7326, 71 p.
  31. ASTM C1161-13. Standard test method for flexural strength of advanced ceramics at ambient temperature. West Conshohocken: ASTM International, 2013, 19 p.
  32. ASTM C1421-16. Standard test methods for determination of fracture toughness of advanced ceramics. West Conshohocken: ASTM International, 2016, 31 p.
  33. Mirov Yu.A., Burlachenko A.G., Buyakova S.P. Study of crack resistance of heteromodular ZrC/C composites by the SEVNB method. Reports conf. «Physical mesomechanics. Materials with a multilevel hierarchically organized structure and intelligent manufacturing technologies». Tomsk, 2020, pp. 330–331. DOI: 10.17223/9785946219242/212.
  34. Mirov Yu.A. Ceramic composite materials with high crack resistance based on zirconium carbide, oxide and boride: thesis, Cand. Sc. (Tech.). Tomsk, 2023, 145 p.
  35. Ferraro C. Bio-inspired ceramic based composites. London, 2016, 246 p. DOI: 10.25560/45538.
  36. Munz D., Fett T. Ceramics: mechanical properties, failure behavior, material selection. Springer, 1999, 298 р.
  37. Hubner H., Jillek W. Sub-critical crack extension and crack resistance in polycrystalline alumina. Journal of Materials Science, 1977, vol. 12, pp. 117–125. DOI: 10.1007/BF00738476.
  38. Nose T., Fujii T. Evaluation of fracture toughness for ceramic materials by a singleedge-precracked-beam method. Journal of the American Ceramic Society, 1988, vol. 71, pp. 328–333. DOI: 10.1111/j.1151-2916.1988.tb05049.x.
  39. Cui W., Li M., Liu J. et al. A Strong Integrated Strength and Toughness Artificial Nacre Based on Dopamine Cross-Linked Graphene Oxide. ACS Nano, 2014, vol. 8, pp. 9511–9517. DOI: 10.1021/nn503755c.
  40. ASTM E1820-15a. Standard Test Method for Measurement of Fracture Toughness. West Conshohocken: ASTM International, 2015, 48 p.
  41. Zimmermann J.W., Hilmas G.E., Fahrenholtz W.G. Thermal Shock Resistance and Fracture Behavior of ZrB2–Based Fibrous Monolith Ceramics. Journal of the American Ceramic Society, 2009, vol. 92, is. 1, pp. 161–166.
  42. Kamiya A., Nakano K., Kondoh A. Fabrication and properties of hot-pressed SiC whisker-reinforced TiB2 and TiC composities. Journal of Materials Science Letters, 1989, vol. 8, pp. 566–568. DOI: 10.1007/BF00720300.
  43. Munro R.G. Material Properties of a Sintered α-SiC. Journal of Physical and Chemical Reference Data, 1997, vol. 26, is. 5, pp. 1195–1203. DOI: 10.1063/1.556000.
  44. Luo Z., Zhou X., Yu J. Mechanical properties of SiC/SiC composites by PIP process with a new precursor at elevated temperature. Materials Science and Engineering: A, 2014, vol. 607, pp. 155–161. DOI: 10.1016/j.msea.2014.03.011.
  45. Magley D., Winholtz F., Faber K. Residual Stresses in a Two-Phase Microcracking Ceramic. Journal of the American Ceramic Society, 1990, vol. 73, is. 6, pp. 1641–1644. DOI: 10.1111/j.1151-2916.1990.tb09808.x.
  46. Teague M. Modeling and Measurement of Thermal Residual Stresses and Isotope Effects on Thermo Physical Properties of ZrB2–SiC Ceramics. Materials Science and Engineering: Master Thesis. Missouri, 2008, no. 4624, 111 p.
  47. A Method for Toughening via the Production of Spiral Architectures through Powder Loaded Polymer Extrusion and Toughened Materials Formed Thereby: pat. US8192853; appl. 12.09.08; publ. 19.03.09.
  48. King D.S., Fahrenholtz W.G., Hilmas G.E. Silicon carbide-titanium diboride ceramic composites. Journal of the European Ceramic Society, 2013, vol. 33, is. 15–16, pp. 2943–2951. DOI: 10.1016/j.jeurceramsoc.2013.03.031.
  49. Yu L., Zhao J., Yue X.Y. et al. Microstructure and Properties of Graphite Embedded SiC Composite by Coating Method. Advanced Materials Research, 2010, vol. 105–106, pp. 855–858. DOI: 10.4028/www.scientific.net/AMR.105-106.855.
  50. Sieber N., Seyller Th., Ley L. et al. Synchrotron x-ray photoelectron spectroscopy study of hydrogen-terminated 6H-SiC {0001} surfaces. Physical Review B, 2003, vol. 67, is. 20, р. 205304. DOI: 10.1103/PhysRevB67.205304.
  51. Emdadi A., Watts J., Fahrenholtz W.G. et al. Predicting effective fracture toughness of ZrB2-based ultra-high temperature ceramics by phase-field modeling. Materials & Design, 2020, vol. 192, p. 11. DOI: 10.1016/j.matdes.2020.108713.