Influence of solvents in the composition of the paint and varnish material on the appearance and properties of paint and varnish coatings

Kuznetsova V.A., Ponomarenko S.A., Zheleznyak V.G., Timoshina E.A.
Kuznetsova V.A., Ponomarenko S.A., Zheleznyak V.G., Timoshina E.A. Influence of solvents in the composition of the paint and varnish material on the appearance and properties of paint and varnish coatings // Proceedings of VIAM. 2023. No. 9. DOI: 10.18577/2307-6046-2023-0-9-110-121. URL: https://viam-works.ru/en/journal/2023/9/10
Keywords
paint coatings, solvents, gas chromatography-mass spectrometry method, adhesion, decorative properties, surface roughnes
Abstract

The influence of solvents in the composition of the paintwork material on the properties of coatings was studied. For research, paints and varnishes based on polyurethane film-forming agents cured with an isocyanate hardener were selected. Solvent R-189 from various manufacturers was used to dilute paints and varnishes. Using the method of gas chromatography-mass spectrometry, the qualitative and quantitative composition of the used solventsR-189 was determined. It has been established that the studied solvents from various manufacturers do not comply with TU 6-10-1725–78, and a significant effect of the composition of the R-189 solvent on the properties of the obtained coatings has also been shown.

Reference list
  1. Zhitomirsky G.I. Aircraft design. Moscow: Mashinostroenie, 1991, 400 p.
  2. Kablov E.N., Kutyrev A.E., Vdovin A.I., Kozlov I.A., Afanasyev-Khodykin A.N. The research of possibility of galvanic corrosion in brazed connections used in aviation engine construction. Aviation materials and technologies, 2021, no. 4 (65), paper no. 01. Available at: http://www.journal.viam.ru (accessed: April 10, 2023). DOI: 10.18577/2713-0193-2021-0-4-3-13.
  3. Buznik V.M., Kablov E.N. Materials for the development of the Arctic and cold territories. Reports XXI Mendeleevsky Congress for General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, p. 21.
  4. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  5. Denker I.I., Vladimir V.N. Technology for the coloring of aircraft and helicopters of civil aviation. Moscow: Mashinostroenie, 1988, 124 p.
  6. Kablov E.N. Materials and chemical technologies for aviation technology. Vestnik Rossiyskoy akademii nauk, 2012, vol. 82, no. 6, pp. 520–530.
  7. Kablov E.N. The role of chemistry in the creation of materials of the new generation for complex technical systems. Reports XX Mendeleevsky Congress for General and Applied Chemistry. Ekaterinburg: SB of RAS, 2016, pp. 25–26.
  8. Rosenfeld I.L., Rutinstein F.I., Zhigalova K.A. Protection of metals from corrosion with paint coatings. Moscow: Khimiya, 1987, 224 p.
  9. Chebotarevsky V.V., Kondrashov E.K. Technology of paintwork in mechanical engineering. Moscow: Mashinostroenie, 1978, 295 p.
  10. Zheleznyak V.G. Modern paint and varnish materials for use in aviation equipment products. Trudy VIAM, 2019, no. 5 (77), paper no. 07. Available at: http://www.viam-works.ru. (accessed: April 17, 2023). DOI: 10.18577/2307-6046-2019-0-5-62-67.
  11. Problems of protective LKM. Review of the materials of the European Conference "Protective Coating" (Protective Coating), Dusseldorf. Lakokrasochnyye materialy i ikh primenenie, 2013, no. 9, pp. 33–35.
  12. Kovrizhkina N.A., Kuznetsova V.A., Silaeva A.A., Marchenko S.A. Ways to improve the properties of paint coatings by adding different fillers (review). Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 41–48. DOI: 10.18577/2071-9140-2019-0-4-41-48.
  13. Merkulova Yu.I., Kuznetsova V.A., Kodachenko E.N., Zheleznyak V.G. Study of the influence of the primer layer’s chemical nature on the properties of the coating system based on fluoropolyurethane enamel. Aviation materials and technologies, 2022, no. 1 (66), paper no. 09. Available at: http://www.journal.viam.ru (ассеssed: April 04, 2023). DOI: 10.18577/2713-0193-2022-0-1-110-119.
  14. Serdtselyubova A.S., Merkulova Yu.I., Zagora A.G., Kurshev E.V. Research of film-forming parameters and protective properties of basecoat/clearcoat system. Aviation materials and technologies, 2023, no. 1 (70), paper no. 07. Available at: http://www.journal.viam.ru (accessed: May 17, 2023). DOI: 10.18577/2713-0193-2022-0-1-93-104.
  15. Merkulova Yu.I., Kurshev E.V., Vdovin A.I., Andreeva N.P. Microstructural and electrochemical studies of paint coatings under natural climate tests of tropical climate of North America. Aviation materials and technologies, 2022, no. 2 (67), paper no. 11. Available at: http://www.journal.viam.ru (accessed: April 05, 2023). DOI: 10.18577/2713-0193-2022-0-2-120-130.
  16. Raw materials and semi-products for paint and varnishes: reference. Ed. M.M. Goldberg. Moscow: Khimiya, 1978, 510 p.
  17. Yakovlev A.D. Chemistry and technology of paintwork: textbook for universities. St. Petersburg: Khimiya, 2010, 448 p.
  18. Okhrimenko I.S., Verkholatsev V.V. Chemistry and technology of film-forming substances. Leningrad: Khimiya, 1978, 392 p.
  19. Sorokin M.F., Kochnova Z.A., Shode L.G. Chemistry and technology of film-forming substances. Moscow: Khimiya, 1989, 477 p.
  20. Goldberg M.M. Materials for paintwork. Moscow: Khimiya, 1972, 343 p.
  21. Orlova O.V., Fomicheva T.N., Okunchikov A.Z., Kursk G.R. Technology of varnishes and colors. Moscow: Khimiya, 1980, 392 p.
  22. Denker I.I., Volberg V.V. Technology for painting products in mechanical engineering. Moscow: Vysshaya Shola, 1990, 303 p.
  23. Tag A.A. Physico-chemistry of polymers. Moscow: Khimiya, 1968, 536 p.
  24. Chalyh A.E. Diffusion in polymer systems. Moscow: Khimiya, 1987, 312 p.
  25. Varnish and paint coatings in mechanical engineering: reference. Ed. M.M. Goldberg. Moscow: Mashinostroenie, 1974, 576 p.
  26. Zubov P.M., Sukhareva L.A. The structure and properties of polymer coatings. Moscow: Khimiya, 1982, 256 p.
  27. Brock T., Groteklaus M., Mishka P. European leadership for paint and varnishes and coatings. Ed. L.N. Mashlyakovsky. Moscow: Paint-Media, 2004, 548 p.
  28. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  29. Fundamentals of analytical chemistry. Ed. Yu.A. Zolotov. Moscow: Vysshaya Shola, 2004, vol. 1, 360 p.
  30. Ponomarenko S.A., Shimkin A.A. Chromatographic methods of analysis: the possibilities of application in the aviation industry. Zavodskaya laboratoriya. Diagnostika materialov, 2017, no. 83 (4), pp. 5–13.