Valuation of the effect of prepreg storage time on warping and PCM properties based on it

Savitsky R.S., Galiullin A.R., Mantusova O.Yu., Veshkin E.A
Savitsky R.S., Galiullin A.R., Mantusova O.Yu., Veshkin E.A Valuation of the effect of prepreg storage time on warping and PCM properties based on it // Proceedings of VIAM. 2023. No. 3. DOI: 10.18577/2307-6046-2023-0-3-48-57. URL: https://viam-works.ru/en/journal/2023/3/5
Keywords
polymer composite material, warping of large-sized flat products, autoclave technology, strength, carbon fiber
Abstract

The article is devoted to the study of the effect of the storage time of lined and uncured polymer composite material made of carbon fiber based on a bundle filler, unidirectional carbon fabric and equal-strength carbon fabric before autoclave forming on the occurrence of the warping process of flat monolithic elements. It was found that prolonged (more than five days) storage of the prepreg after laying out before molding negatively affects the warping of the panel. The development of technological recommendations in accordance with the results obtained will ensure a reduction in the share of defective finished products.

Reference list
  1. Kolpachkov E.D., Kurnosov A.O., Petrova A.P., Raskutin A.E. Hybrid polymer composite materials for aviation based on fibrous fillers (review). Voprosy materialovedeniya, 2020, no. 1 (101), pp. 126–138. DOI: 10.22349/1994-6716-2020-101-1-126-138.
  2. Timoshkov P.N., Goncharov V.A., Usacheva M.N., Khrulkov A.V. Features of technology and polymer composite materials for the manufacture of wings of advanced aircraft (review). Trudy VIAM, 2022, no. 1 (107), paper no. 07. Available at: http://www.viam-works.ru (accessed: August 01, 2022). DOI: 10.18577/2307-6046-2022-0-1-66-75.
  3. Valueva M.I., Evdokimov A.A., Klimenko O.N. Carbon fiber in the design of space technology products (review). Vse materialy. Entsiklopedicheskiy spravochnik, 2022, no. 1, pp. 12–21
  4. Raskutin A.E. Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
  5. Kablov E.N. VIAM: new generation materials for PD-14. Krylya Rodiny, 2019, no. 7–8, pp. 54–58.
  6. Gunyaeva A.G., Sidorina A.I., Kurnosov A.O., Klimenko O.N. Polymeric composite materials of new generation on the basis of binder VSE-1212 and the filling agents alternative to ones of Porcher Ind. and Toho Tenax. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 18–26. DOI: 10.18577/2071-9140-2018-0-3-18-26.
  7. Kablov E.N., Antipov V.V., Girsh R.I., Serebrennikova N.Yu., Konovalov A.N. Constructed layered materials based on sheets of aluminum-lithium alloys and fiberglass in the construction of new generation aircraft. Vestnik mashinostroeniya, 2020, no. 12, pp. 46–52.
  8. Kablov E.N., Podzhivotov N.Yu., Lutsenko A.N. On the need to create a unified information and analytical center for aviation materials of the Russian Federation. Problemy mashinostroyeniya i avtomatizatsii, 2019. No. 3. S. 28–34.
  9. Veshkin E.A., Satdinov R.A., Savitsky R.S. Approach to the selection of technological mode for the manufacture of PCM. Trudy VIAM, 2021, no. 11 (105), paper no. 10. Available at: http://www.viam-works.ru (accessed: August 01, 2022). DOI: 10.18577/2307-6046-2021-0-11-103-111.
  10. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  11. Bondarchuk D.A., Fedulov B.N., Fedorenko A.N., Lomakin E.V. Analysis of residual stresses in layered composites on the example of a symmetrical reinforcement scheme [0°/90°]. Vestnik Permskogo natsional'nogo issledovatelskogo politekhnicheskogo universiteta. Mekhanika, 2019, no. 3, pp. 17–26.
  12. Shabalin L.P., Puzyretsky E.A., Sidorov I.N., Girfanova A.M. Technique for calculating technological stresses to prevent warping of composite parts. Problemy mashinostroeniya i nadezhnosti mashin, 2021, no. 2, pp. 52–62. DOI: 10.31857/S0235711921020127.
  13. Bondarchuk D.A., Klemareva M.V., Gadelev R.R., Nazarov E.V. The use of different methods for determining residual stresses and strains in large-sized aircraft parts made of PCM on the example of a stringer panel. Vestnik mashinostroeniya, 2021, no. 12, pp. 63–67. DOI: 10.36652/0042-4633-2021-12-63-67.
  14. Mantusova O.Yu., Postnov V.I. Calculation-experimental method for estimating the fatigue strength of MPCM. Izvestiya Samarskogo nauchnogo tsentra RAN, 2012, vol. 14, no. 4, pp. 847–849.
  15. Bitkina E.V., Pidodnya V.G., Bitkina O.V. Study of the influence of technological factors on residual stresses in a fibrous composite. Vestnik Samarskogo gosudarstvennogo tekhnicheskogo universiteta. Ser.: Physical and mathematical sciences, 2011, no. 4 (25), pp. 59–66.
  16. Korolkov V.I., Nekravtsev E.N., Safonov K.S. et al. Investigation of the processes of eliminating warping of aviation products from polymer-composite materials obtained by high-temperature molding. Izvestiya vysshikh uchebnykh zavedeniy. Mashinostroyenie, 2021, no. 10, pp. 84–94. DOI: 10.18698/0536-1044-2021-10-84-94.
  17. Markin O.V., Kravchenko E.A., Bush A.V., Sviridov A.G. Analysis of the causes of excessive distortion of the composite rib. Colloquium-Journal, 2021, no. 16-1 (103), pp. 19–22.
  18. Guseva M.A., Petrova A.P. Possibilities of rheology in the study of binders for PCM. Vse materialy. Entsiklopedicheskiy spravochnik, 2021, no. 7, pp. 38–44.