Formation of silicon carbide coatings by chemical vapor deposition (review)

Part 2
Sidorov D.V., Shavnev A.A., Melentev A.A.
Sidorov D.V., Shavnev A.A., Melentev A.A. Formation of silicon carbide coatings by chemical vapor deposition (review). Part 2 // Proceedings of VIAM. 2022. No. 2. DOI: 10.18577/2307-6046-2022-0-2-88-98. URL: https://viam-works.ru/en/journal/2022/2/7
Keywords
chemical vapor deposition, silicon carbide, coating, chemical reaction, reagent, kinetic, thermodynamic
Abstract

The article provides an overview of the scientific and technical literature in the field of the formation of silicon carbide coatings by chemical vapor deposition (CVD). CVD is a complex process, approaches to which vary depending on the tasks being solved. Depending on the technological parameters it is possible to achieve both the deposition of pure silicon carbide and the co-deposition of silicon and carbon, mixed coating In the article attention is paid to the study of CVD from the point of view of the kinetic and parameters for deposition and thermodynamic.

Reference list
  1. Kablov E.N., Echin A.B., Bondarenko Yu.A. History of development of directional crys-tallization technology and equipment for casting blades of gas turbine engines. Trudy VIAM, 2020, no. 3 (87), paper no. 01. Available at: http://www.viam-works.ru (accessed: August 11, 2021). DOI: 10.18577/2307-6046-2020-0-3-3-12.
  2. Kablov E.N., Kutyrev A.E., Vdovin A.I., Kozlov I.A., Afanasyev-Khodykin A.N. The research of possibility of galvanic corrosion in brazed connections used in aviation engine construction. Aviation materials and technologies, 2021, no. 4 (65), paper no. 01. Available at: http://www.journal.viam.ru (accessed: December 21, 2021). DOI: 10.18577/2713-0193-2021-0-4-3-13.
  3. Kablov E.N., Valueva M.I., I.V. Zelenina, Khmelnitskiy V.V., Aleksashin V.M. Carbon plastics based on benzoxazine oligomers – perspective materials. Trudy VIAM, 2020, no. 1, paper no. 07. Available at: http://www.viam-works.ru (accessed: August 11, 2021). DOI: 10.18577/2307-6046-2020-0-1-68-77.
  4. Matovic B., Yano T. Handbook of Advanced Ceramics. Materials, Applications, Processing, and Properties. Oxford, 2013, pp. 225–244.
  5. Sidorov D.V., Storozhenko P.A., Shutova O.G., Kozhevnikov B.E. Obtaining high purity alkylsilanes. Chemical technology, 2006, no. 7, pp. 22–24.
  6. Ashby M., Jones E. Structural materials. Full course. Dolgoprudny: Intellekt, 2010. 672 p.
  7. Choy K. Chemical vapour deposition of coatings. Progress in material science, 2003, vol. 48, pp. 57–170. DOI: 10.1016/S0079-6425(01)00009-3.
  8. Sidorov D.V., Schavnev A.A., Melentev A.A. Formation of silicon carbide coatings by chemical vapor deposition (review). Part 1. Trudy VIAM, 2021, no. 6 (100), paper no. 10. 09. Available at: http://www.viam-works.ru (accessed: September 6, 2021). DOI: 10.18577/2307-6046-2021-0-6-100-111.
  9. Loumagne F., Langlais F., Naslain R. Reactional mechanisms of the chemical vapour deposition of SiC-based ceramics from CH3SiC3/H2 gas precursor. Journal of Crystal Growth, 1995, vol. 155, pp. 205–213.
  10. Huo Y., Chen Y. Effects of Deposition Temperature on the Growth Characteristics of CVD SiC Coatings. Key Engineering Materials, 2008, vol. 368–372, pp. 846–848.
  11. Deng J.G., Su K., Wang X. Thermodynamics of the Production of Condensed Phases in the CVD of Methyltrichlorosilane Pyrolysis. Chemical vapor deposition, 2009, vol. 15, pp. 281–290.
  12. Shulberg M., Allendorf M., Outka D. The adsorption of hydrogen chloride on polycrystalline silicon carbide. Surface Science, 1995, vol. 341, pp. 262–272.
  13. Pons M., Meziere J., Kuan S. Heat and mass transfer modeling for a better knowledge of the large-area growth of homoepitaxial SiC by CVD. Materials Research Society Symposium Proceedings, 2001, vol. 640, pp. H.5.6.1–H.5.6.1.6.
  14. Vorob’ev А.N., Karpov S.Yu., Bord O.V. Modeling of gas phase nucleation during silicon carbide chemical vapor deposition. Diamond and Related Materials, 2000, vol. 9, pp. 472–475.
  15. Takeuchi T., Egashira Y., Komiyama H. A design policy of the SiC CVD reactor based on the chemical reaction kinetics of diclorodimethylsilane. Journal of Materials Science, 1997, vol. 97-25, pp. 447–454.
  16. Herlin N., Lefebvre M., Pealat M. Investigation of the Chemical vapor deposition of silicon carbide from tetramethylsilane by in situ temperature and gas composition measurements. Journal of Physical Chemistry, 1992, vol. 96, pp. 7063–7072.
  17. Shirvan M., Ellahi R., Sheikholeslami T., Behzadmehr А. Numerical investigation of heat and mass transfer flow under the influence of silicon carbide by means of plasma enhanced chemical vapor deposition vertical reactor. Neural Computing & Application, 2017, vol. 96, pp. 7063–7072.
  18. Ding J., Zhao Y., Yan N., Shubo M. Effect of electrode architecture and process parameters on distribution of SiH3 in a PECVD system. Vacuum, 2011, vol. 86, pp. 344–349.
  19. Soong C., Chyuan C., Tzong R. Thermo-flow structure and epitaxial uniformity in large-scale metalorganic chemical vapor deposition reactors with rotating susceptor and inlet flow control. Japanese Journal of Applied Physics, 1998, vol. 37, pp. 5823–5834.
  20. Lu C., Cheng L., Zhao C. Kinetics of chemical vapor deposition of SiC from methyltrichlorosilane and hydrogen. Applied Surface Science, 2009, vol. 255, pp. 7495–7499.