Polymer binders in advanced technologies of polymer composite materials production (review)

Afanaseva E.A., Shiryakina Yu.M., Kitaeva N.S., Novikova A.A.
Afanaseva E.A., Shiryakina Yu.M., Kitaeva N.S., Novikova A.A. Polymer binders in advanced technologies of polymer composite materials production (review) // Proceedings of VIAM. 2022. No. 2. DOI: 10.18577/2307-6046-2022-0-2-75-87. URL: https://viam-works.ru/en/journal/2022/2/6
Keywords
VaRTM, polymeric binders, automated tape laying (ALT), automated fiber placement, polymeric composite materials, infusion technology
Abstract

The article analyzes the scientific and patent literature about modern methods of manufacturing polymer composite materials. The main aspects of using automatic filler laying for preforms and the use of various polymer binders for stabilizing filler layers are considered. The requirements for polymer binders, types of production forms and the nature of the chemical structure, as well as their application are described. Methods of activation of polymeric binders by local and general actions are presented.

Reference list
  1. Kablov E.N. The role of fundamental research in the creation of new generation materials. Tez. Reports of the XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, pp. 24.
  2. Polynt Composites - truly high-quality solutions for shipbuilding. Kompozitnyy mir, 2018, no. 1, pp. 44–47.
  3. Panshin A. Evgeny Kablov: Russia's share in the market of composites is negligible. Kompozitnyy mir, 2019, no. 1, pp. 22–23.
  4. Bityukov Yu.I., Deniskin Yu.I. Quality control of structures made of composite materials. Vse materialy. Entsiklopedicheskiy spravochnik, 2017, no. 11, pp. 14–19.
  5. Minibaev M.I., Raskutin A.E, Goncharov V.A. Peculiarities of technology production specimens of PCM on CNC machines (review). Trudy VIAM, 2019, no. 1 (73), paper no. 11. Available at: http://www.viam-works.ru (accessed: September 22, 2021). DOI: 10.18577/2307-6046-2019-0-1-105-114.
  6. Marakhovsky P.S., Barinov D.Ya., Chutskova E.Yu., Melnikov D.A. Curing of multilayer polymeric composite materials. Part 2. Molding of a thick-walled fiberglass plate. Vse materialy. Entsiklopedicheskiy spravochnik, 2018, no. 6, pp. 7–14.
  7. Kablov E.N. Materials of a new generation - the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14). pp. 42–47.
  8. Kudryavtseva A.N., Tkachuk A.I., Grigorieva K.N., Gurevich Ya.M. The use of epoxy resin system VSE-30, processed by the infusion technology, for the manufacture of low and medium loaded structural polymer composite materials. Trudy VIAM, 2019, no. 1 (73), paper no. 04. Available at: http://www.viam-works.ru (accessed: September 22, 2021). DOI: 10.18577/2307-6046-2019-0-1-31-39.
  9. Timoshkov P.N., Goncharov V.A., Usacheva M.N., Khrulkov A.V. Effect of gaps and overlaps when laying prepregs on the mechanical properties of carbon plastics (review). Trudy VIAM, 2018, no. 12 (72), paper no. 08. Available at: http://www.viam-works.ru (accessed: September 22, 2021). DOI: 10.18577/2307-6046-2018-0-12-71-78.
  10. Mosiyuk V.N., Tomchani O.V. Evaluation of properties of glass-fibre-reinforced plastics based on epoxybismaleimide resin, produced by different non-autoclave molding techniques. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 47–52. DOI: 10.18577/2071-9140-2019-0-2-47-52.
  11. Gusev Yu.A., Grigorev M.M., Timoshina L.N. Production of standard polymer composite samples with the set porosity by vacuum infusion. Trudy VIAM, 2014, no. 11, paper no. 06. Available at: http://www.viam-works.ru (accessed: September 22, 2021). DOI: 10.18577/2307-6046-2014-0-11-6-6.
  12. Mosiyuk V.N., Vorvul S.V., Tomchani O.V. Differential vacuum molding as an advanced technology of vacuum molding. Aviacionnye materialy i tehnologii, 2017, no. 4 (49), pp. 37–41. DOI: 10.18577/2071-9140-2017-0-4-37-41.
  13. Timoshkov P.N., Goncharov V.A., Usacheva M.N., Khrulkov A.V. The development of automated laying: from the beginning to our days (review). Part 2. Automat-ed Fiber Placement (AFP). Aviation materials and technologies, 2021, no. 3 (64), paper no. 11. Available at: http://www.journal.viam.ru (accessed: October 2, 2021). DOI: 10.18577/2713-0193-2021-0-3-117-127.
  14. Chursova L.V., Panina N.N., Grebeneva T.A., Terekhov I.V., Donetsky K.I. Thermosetting binders and polymer binders for polymer composite materials obtained by vacuum infusion (review). Plasticheskiye massy, 2018, no. 1–2. pp. 57–64. DOI: 10.18577/2307-6046-2018-0-2-57-64.
  15. Lebel L.L., Trudeau P. Preforming of a Fuselage C-shaped Frame Manufacturing by Resin Transfer Molding. SAE International Journal of Aerospace, 2013, vol. 6, no. 2, pp. 508–512. DOI: 10.4271/2013-01-2214.
  16. Epoxy resin formulations for textiles, mats and other fibrous reinforcements for composite applications: pat. EP2623561A1; filed 06.02.12; publ. 07.08.13.
  17. Toughened binder compositions for use in advance processes: pat. WO2008063611A3; filed 19.11.07; publ. 14.08.08.
  18. Binder resin for resin transfer molding preforms, preforms made therewith, and a method for preparing such preforms: pat. US5432010; filed 23.09.94; publ. 11.07.95.
  19. Method of fabricating fiber reinforced composite articles by resin transfer molding: pat. US4988469A; filed 16.02.90; publ. 29.01.91.
  20. Epoxy composite: pat. GB2460050; filed 14.05.08; publ. 18.11.09.
  21. Methods and preforms for forming composite members with interlayers formed of nonwoven, continuous materials: pat. US8246882; filed 27.10.04; publ. 21.08.12.
  22. Dry fibrous material for subsequent resin infusion: pat. WO2013096377A3; filed 19.12.12; publ. 27.02.14.
  23. Epoxy binder for polymer composite materials: pat. RU25227086; filed 22.11.12; publ. 27.08.14.
  24. Liquid binder composition for binding fibrous materials: pat. US20140179187A1; filed 11.07.13; publ. 26.06.14.
  25. Timoshkov P.N. Equipment and materials for the technology of automated calculations prepregs. Aviacionnye materialy i tehnologii, 2016, no. 2 (41), pp. 35–39. DOI: 10.18577/2071-9140-2016-0-2-35-39.
  26. Timoshkov P.N., Goncharov V.A., Usacheva M.N., Khrulkov A.V. The development of automated laying: from the beginning to our days (review). Part 1. Automated Tape Laying (ATL). Aviation materials and technologies, 2021, no. 2 (63), paper no. 06. Available at: http://www.journal.viam.ru (accessed October 2, 2021). DOI: 10.18577/2713-0193-2021-0-2-51-61.
  27. VaRTM Processing of Tackified Fiber/Fabric Composites: pat. US2014120332; filed 21.03.13; publ. 01.05.14.
  28. Gusev Yu.A., Borshhev A.V., Khrulkov A.V. Features of prepregs intended for automated laying by ATL and AFP technologies. Trudy VIAM, 2015, no. 3, paper no. 06. Available at: http://www.viam-works.ru (accessed: September 22, 2021). DOI: 10.18577/2307-6046-2015-0-3-6-6.
  29. Rakhmatullin A.E., Postnov V.I., Strelnikov S.V. Development and application experience of software for carrying out the formation process of structures from PCM on the heated equipment. Trudy VIAM, 2019, no. 4 (76), paper no. 06. Available at: http://viam-works.ru (accessed: September 22, 2021). DOI: 10.18577/2307-6046-2019-0-4-48-56.
  30. Savin S.P. The use of modern polymer composite materials in the airframe design of aircraft of the MS-21 family. Izvestiya Samarskogo nauchnogo tsentra Rossiyskoy akademii nauk, 2012, vol. 14, no. 4 (2). pp. 686–693.
  31. Epoxy film former string binder: pat. US6828024B1; filed 30.06.03; publ. 07.12.04.
  32. Veshkin E.A. Technologies of autoclave-free molding of low-porous polymer composite materials and large-sized structures from them: thesis, Cand. Sc. (Tech.). Mosocw, 2016. 146 p.
  33. Rohatgi V., Lee L.J. Moldability of Tackified Fiber Preforms in Liquid Composite. Journal of Composite Materials, 2018, vol. 31 (7), pp. 720–744. DOI: 10.1177/002199839703100705.
  34. Schmidt S., Mahrholz T., Kühn A., Wierach P. Powder binders used for the manufacturing of wind turbine rotor blades. Part 2. Investigation of binder effects on the mechanical performance of glass fiber reinforced polymers. Journal of Composite Materials, 2017, vol. 53 (16), pp. 2261–2270. DOI: 10.1177/0021998318824784.
  35. Preforms for moulding process and resins therefor: pat. WO1998050211A1; filed 30.04.98; publ. 12.11.98.
  36. Flexible polymer element as toughening agent in prepregs: pat. EP1317501B1; filed 16.08.01; publ. 22.11.06.
  37. Estrada G., Vieux-Pernon C., Advani S.G. Experimental Characterization of the Influence of Tackifier Material on Preform Permeability. Journal of Composite Materials, 2020, vol. 36 (19), pp. 2297–2310. DOI: 10.1177/0021998302036019542.
  38. Thermally stable binder resin composition and method for binding fibres: pat. EP1341850B2; filed 06.11.01; publ. 14.08.13.
  39. Process for producing a reinforcing woven fabric, a preform and a fiber reinforced plastic molded component: pat. US8168106B2; filed 15.12.10; publ. 01.05.12.
  40. Method for preparing preforms for molding processes: pat. WO1995032085A1; filed 16.05.95; publ. 30.11.95.
  41. Laser-assisted placement of veiled composite material: pat. US2006048881; filed 08.09.04; publ. 09.03.06.
  42. Method for making a composite material having at least one twisted thread deposited therein: pat. US8696850; filed 10.06.08; publ. 15.04.14.
  43. Thermally stable binder resin composition and method for bonding fibers: pat. JP2004514758A; filed 06.11.01; publ. 20.05.04.
  44. Improved process for resin transfer molding: pat. WO1994026492A1; filed 15.04.94; publ. 24.11.94.
  45. Heieck F. Binder application methods for textile preforming processes. LTH Faserverbund-Leichtbau. Available at: https://www.researchgate.net (accessed: September 22, 2021). DOI: 10.13140/RG.2.2.14197.73446.