Manufacturing of metal-matrix composite materials using additive technologies (review)

Zhabin A.N., Nyafkin A.N.
Zhabin A.N., Nyafkin A.N. Manufacturing of metal-matrix composite materials using additive technologies (review) // Proceedings of VIAM. 2022. No. 2. DOI: 10.18577/2307-6046-2022-0-2-64-74. URL: https://viam-works.ru/en/journal/2022/2/5
Keywords
metal matrix composite material, selective laser fusion, direct laser sintering, SiC particles, aluminum alloy, additive technologies
Abstract

A review of scientific and technical literature in the field of obtaining metal-matrix composite materials (MMCM) reinforced with ceramic particles using additive technologies is presented. The structure, basic physical and mechanical properties and morphology of MMCM are briefly described. The structure and properties of MMCM reinforced with micro- and nano-sized ceramic particles are briefly described. The use of additive technologies for the manufacture of MMKM will make it possible to manufacture parts of a more complex shape, providing high adhesion between powder layers.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Composites: today and Tomorrow. Metally Evrazii, 2015, no. 1, pp. 36–39.
  3. Kablov E.N. Present and future of additive technologies. Metally Evrazii, 2017, no. 1, pp. 2–6.
  4. Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  5. Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
  6. Lopatin A.N., Zverkov I.D. Shaping molding tools production for composite parts by means of additive technologies. Aviacionnye materialy i tehnologii, 2019, no. 2 (55). pp. 53–59. DOI: 10.18577/2071-9140-2019-0-2-53-59.
  7. Evgenov A.G., Shurtakov S.V., Prager S.M., Malinin R.Yu. On the development of a universal calculation method for assessing the degradation of recycled metal powder materials, depending on the cyclicity of use in the selective laser melting process. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 3–11. DOI: 10.18577/2071-9140-2020-0-4-3-11.
  8. Chang F., Gu D., Dai D., Yuan P. Selective laser melting of in-situ Al4SiC4 + SiC hybrid reinforced Al matrix composites: Influence of starting SiC particle size. Surface & Coatings Technology, 2015, vol. 272, pp. 15–24. DOI: 10.1016/j.surfcoat.2015.04.029.
  9. Xue G., Ke L., Zhu H. et al. Influence of processing parameters on selective laser melted SiCp/AlSi10Mg composites: Densification, microstructure and mechanical properties. Materials Science & Engineering A, 2019, vol. 764, pp. 1–10. DOI: 10.1016/j.msea.2019.138155.
  10. Famodimu O.H., Stanford M., Oduoza Ch.F., Zhang L. Effect of process parameters on the density and porosity of laser melted AlSi10Mg/SiC metal matrix composite. Frontiers of Mechanical Engineering, 2018, vol. 13, part 4, pp. 520–527.
  11. Anandkumar R., Almeida A., Vilar R. et al. Influence of powder particle injection velocity on the microstructure of Al–12Si/SiCp coatings produced by laser cladding. Surface & Coatings Technology, 2009, vol. 204, pp. 285–290. DOI: 10.1016/j.surfcoat.2009.07.025.
  12. Gu D., Chang F., Dai D. Selective Laser Melting Additive Manufacturing of Novel Aluminum Based Composites With Multiple Reinforcing Phases. Journal of Manufacturing Science and Engineering, 2015, vol. 137, pp. 1–11. DOI: 10.1115/1.4028925.
  13. Astfalck L.C., Kelly G.K., Li X., Sercombe T.B. On the Breakdown of SiC during the Selective Laser Melting of Aluminum Matrix Composites. Advanced Engineering Materials, 2017, pp. 1–6. DOI: 10.1002/adem.201600835.
  14. Simchi A., Godlinski D. Effect of SiC particles on the laser sintering of Al–7Si–0.3Mg alloy. Scripta Materialia, 2008, vol. 59, pp. 199–202. DOI: 10.1016/j.scriptamat.2008.03.007.
  15. Li X.P., Ji G., Chen Z. et al. Selective laser melting of nano-TiB2 decorated AlSi10Mg alloy with high fracture strength and ductility. Acta Materialia, 2017, vol. 129, pp. 183–193. DOI: 10.1016/j.actamat.2017.02.062.
  16. Aversa A., Marchese G., Lorusso M. et al. Microstructural and Mechanical Characterization of Aluminum Matrix Composites Produced by Laser Powder Bed Fusion. Advanced Engineering Materials, 2017, pp. 1–11. DOI: 10.1002/adem.201700180.