X-rays diffractometry application at plotting of structure conditions diagrams of deformable alloys of aviation assignment

Kochubey A.Ya., Juravleva P.L.
Kochubey A.Ya., Juravleva P.L. X-rays diffractometry application at plotting of structure conditions diagrams of deformable alloys of aviation assignment // Proceedings of VIAM. 2022. No. 2. DOI: 10.18577/2307-6046-2022-0-2-142-152. URL: https://viam-works.ru/en/journal/2022/2/12
Keywords
hot plastic deformation, axisymmetric compression, recrystallization, structure condition diagrams
Abstract

Axisymmetric hot compression experiments of nickel superalloy ЭП975-ИД, ЭП742-ИД and MA2, MA3 alloy specimens in a wide temperature and rate intervals were carried out. Structure formation was studied by х-ray diffractometry methods. Structure diagrams plotting method is based on using of the test machine which has been adjusted on compression, and structure studying is developed. Diagrams can be used for development and optimization of hot pressure technology parameters, for the purpose receiving preparations with the regulated structure.

Reference list
  1. Kablov E.N. Materials of a new generation and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  2. Kablov E.N., Akinina M.V., Volkova E.F., Mostyaev I.V., Leonov A.A. The research of aspects of phase composition and fine structure of magnesium alloy ML9 in the as-cast and heat-treated conditions. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 17–24. DOI: 10.18577/2071-9140-2020-0-2-17-24.
  3. Kablov E.N. VIAM: new generation materials for PD-14. Krylya Rodiny, 2019, no. 7–8. pp. 54–58.
  4. Kablov E.N. The role of fundamental research in the creation of new generation materials. Reports of the XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, p. 24.
  5. Volkova E.F., Akinina M.V., Mostyaev I.V. The ways of rising of wrought magnesium alloys main mechanical characteristics. Trudy VIAM, 2017, no. 10 (58), paper no. 02. Available at: http://www.viam-works.ru (accessed: October 1, 2021). DOI: 10.18577/2307-6046-2017-0-10-2-2.
  6. Lomberg B.S., Ovsepjan S.V., Bakradze M.M., Letnikov M.N., Mazalov I.S. The application of new wrought nickel alloys for advanced gas turbine engines. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 116–129. DOI: 10.18577/2071-9140-2017-0-S-116-129.
  7. Antipov V.V. Strategy of development of titanium, magnesium, beryllium and aluminum alloys. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 157–167.
  8. Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
  9. Blokhin N.N., Ovechkin B.I. Structure and diagrams of structural states of deformable magnesium alloys // Tsvetnye metally, 1992, no. 11, pp. 56–59.
  10. Filonova E.V., Bakradze M.M., Kochubey A.Ya., Vavilin N.L. Structural-phase evolution of VZH175-alloy during hot deformation and heat treatment. Aviacionnye materialy i tehnologii, 2014, no. 3, pp. 10–13. DOI: 10.18577/2071-9140-2014-0-3-10-13.
  11. Weinblat Yu.M. Diagrams of structural states and maps of the structures of aluminum alloys. Izvestiya AN SSSR. Metally, 1982, no. 2, pp. 82–89.
  12. Bubnov M.V., Sklyarenko V.G. Formation of a regulated structure during deformation of the granular alloy EP741NP. Tekhnologiya legkikh splavov, 2007, no. 2, pp. 54–55.
  13. Razuvaev E.I., Lebedev D.Yu., Bubnov M.V. Forming of ultrafine grained and nanodimensional structure in metals and alloys deformation methods. Aviacionnye materialy i tehnologii, 2010, no. 3, pp. 3–8.
  14. Mazalov I.S., Filonova E.V., Lomberg B.S. Formation of microstructure of nickel weldable VGH172 superalloy in process of deformation and heat treatment of semi-finished products. Trudy VIAM, 2013, no. 12, paper no. 01. Available at: http://www.viam-works.ru (accessed: October 1, 2021).
  15. Gorelik S.S. Recrystallization of metals and alloys. Moscow: Metallurgiya, 1978, 568 p.
  16. Umansky Ya.S., Skakov Yu.A., Ivanov A.N., Rastorguev L.N. Crystallography, radiography and electron microscopy. Moscow: Metallurgiya, 1982. 632 p.
  17. Novikov I.I. Theory of heat treatment of metals. Moscow: Metallurgy, 1978. 392 p.
  18. Kochubey A.Ya., Medvedev P.N. The use of direct pole figures in the study of structure formation processes during heating of deformed metals and alloys. News of Materials Science. Science and technology, 2016, no. 5 (23). Art. 02. Available at: http://www.materialsnews.ru (accessed: October 1, 2021).
  19. Davydov V.G., Ber L.B., Kochubey A.Ya. Influence of grain size on diagrams of structural states of alloy MA2-1. Tekhnologiya legkikh splavov, 2003, no. 2–3, pp. 28.