Analysis of aluminum-based cathodes by X-ray fluorescence spectroscopy

Alekseev A.V., Orlov G.V., Petrov P.S.
Alekseev A.V., Orlov G.V., Petrov P.S. Analysis of aluminum-based cathodes by X-ray fluorescence spectroscopy // Proceedings of VIAM. 2022. No. 2. DOI: 10.18577/2307-6046-2022-0-2-133-141. URL: https://viam-works.ru/en/journal/2022/2/11
Keywords
determination of silicon, aluminum alloys, cathodes, aluminum analysis, ion-plasma technology, heat-resistant alloys
Abstract

The determination of Si, Y, Fe, Ni, Cu, Mg, Cr and Co in the cathodes of the VSDP-11 and VSDP-16 brands based on aluminum by the method of х-ray fluorescence spectroscopy was carried out. The calibration dependences are corrected taking into account the superposition of signals from interfering elements on the analytical signal and changes in intensity caused by inter-element influences in the matrix. A standard-free analysis was carried out using the method of fundamental parameters. The correctness of the results obtained was confirmed by a comparative analysis by atomic emission spectroscopy and high-resolution mass spectrometry with a glow discharge.

Reference list
  1. Kablov E.N., Ospennikova O.G., Svetlov I.L. Highly efficient cooling of GTE hot section blades. Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 3–14. DOI: 10.18577/2071-9140-2017-0-2-3-14.
  2. Kablov E.N., Bondarenko Yu.A., Echin A.B. Development of technology of cast superalloys directional solidification with variable controlled temperature gradient. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 24–38. DOI: 10.18577/2071-9140-2017-0-S-24-38.
  3. Muboyadzhyan S.A., Budinovskij S.A. Ion-plasma technology: prospective processes, coatings, equipment. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 39–54. DOI: 10.18577/2071-9140-2017-0-S-39-54.
  4. Konokotin S. P., Yatsyuk I. V., Dobrynin D. A., Azarovsky E. N. Influence of yttrium on the quality of cast billets from alloys based on aluminum. Trudy VIAM, 2020, no. 3 (87), paper no. 03. Available at: http://www.viam-works.ru (accessed: December 10, 2021). DOI: 10.18577/2307-6046-2020-0-3-30-40.
  5. Farafonov D.P., Leshchev N.E., Afanasiev-Khody- kin A.N., Artemenko N.I. Abrasive wear-resistant seal materials of the gas turbine engine flow section. Aviacionnye materialy i tehnologii, 2019, No. 3 (56), pp. 67–74. DOI: 10.18577/2071-9140-2019-0-3-67-74.
  6. Kablov E.N., Chabina E.B., Morozov G.A., Muravskaya N.P. Conformity assessment of new materials using high-level RM and MI. Kompetentnost, 2017, no. 2, pp. 40–46.
  7. State Standard 11739.7–99. Alloys aluminum casting and deformable. Methods for the determination of silicon. Moscow: Publishing house of standards, 1999, pp. 6–8.
  8. State Standard 11739.21–90. Alloys aluminum casting and deformable. Methods for the determination of chromium. Moscow: Publishing house of standards, 1990, pp. 1–3.
  9. State Standard 11739.6–99. Alloys aluminum casting and deformable. Methods for the determination of iron. Moscow: Publishing house of standards, 1999, pp. 1–4.
  10. State Standard 11739.13–98. Alloys aluminum casting and deformable. Methods for the determination of copper. Moscow: Publishing house of standards, 1998, pp. 6–8.
  11. ASTME E3061-17. Standard Test Method for Analysis of Aluminum and Aluminum Alloys by Inductively Coupled Plasma Atomic Emission Spectrometry. ASTM International, 2017, p. 2.
  12. Blokhin M.A. Methods of x-ray spectral studies. Moscow: State Publishing house of Phys.-Math. Lit., 1959, 388 p.
  13. Handbook of x-ray spectrometry. Ed. by R.E. van Grieken, A.A. Marcowicz. 2nd ed., rev. and exp. New York: Marcel Dekker Inc., 2001. pp. 14–56.
  14. Criss J.W., Birks L.S. Calculation methods for fluorescent X-ray spectrometry. Empirical coefficients vs. fundamental parameters. Analytical Chemistry, 1968, vol. 40, pp. 1080–1086.
  15. Mashin N.I., Lebedeva R.V., Tumanova A.N. X-ray fluorescence analysis of Ni–Fe–Mn–Cr systems. Analitika i kontrol, 2004, no. 2, vol. 8, pp. 160–164.