The contribution of phases to the magnetization of sintered materials Nd–Dy–Fe-Co–B

Valeev R.A., Korolev D.V., Morgunov R.B., Piskorsky V.P.
Valeev R.A., Korolev D.V., Morgunov R.B., Piskorsky V.P. The contribution of phases to the magnetization of sintered materials Nd–Dy–Fe-Co–B // Proceedings of VIAM. 2022. No. 11. DOI: 10.18577/2307-6046-2022-0-11-60-68. URL: https://viam-works.ru/en/journal/2022/11/6
Keywords
rare earth magnets, main magnetic phase, residual induction, coercive force, cobalt alloying, secondary phases
Abstract

The need to manufacture permanent magnets based on rare-earth metals of complex shape and with increased thermal stability of magnetic properties forces the use of heavy rare-earth metal dysprosium and transition metal cobalt in the chemical composition of the alloy. In this regard, the phase composition of the permanent magnet material changes. The study of the magnetic properties of secondary phases and their contribution to the magnetic properties of permanent magnets is necessary to find the optimal composition that allows to obtain permanent magnets with the necessary level of properties.

Reference list
  1. Raspopov V.Ya. Micromechanical devices: textbook. Tula: Tula State Univ., 2002, 392 p.
  2. Arnold R.R. Calculation and design of magnetic systems with permanent magnets. Moscow: Energiya, 1969, 184 p.
  3. Kablov E.N., Piskorsky V.P., Burkhanov G.S., Valeev R.A., Moiseeva N.S., Stepanova S.V., Petrakov A.F., Tereshina I.S., Repina M.V. Thermally stable ring magnets with radial texture based on Nd(Pr)–Dy–Fe–Co–B. Fizika i khimiya obrabotki materialov, 2011, no. 3, pp. 43–47.
  4. Kablov E.N., Petrakov A.F., Piskorsky V.P., Valeev R.A., Nazarova N.V. Influence of dysprosium and cobalt on the temperature dependence of magnetization and phase composition of the material of the Nd–Dy–Fe–Co–B system. Metallovedenie i termicheskaya obrabotka metallov, 2007, no. 4, pp. 3–10.
  5. Christodoulou C.N., Wallace W.E., Massalski T.B. Magnetic hardening of Pr–Co–B sintered magnets. Journal of Applied Physics, 1989, vol. 66, pp. 2749–2751.
  6. Gros Y., Hartmann-Boutron F., Meyer C. et al. Mossbauer study of compounds RCo4–xFexB and RFe4B. Journal de Physique, 1988, vol. 49, pp. C8-547–C8-548.
  7. Gros Y., Hartmann-Boutron F., Meyer C. et al. Preparation and 57Fe Mossbauer study of PrCo3FeB, NdCo3FeB, SmCo3FeB and SmCo2Fe2B. Journal of Magnetism and Magnetic Materials, 1988, vol. 74, pp. 319–326.
  8. Herve M., Oliver I., Fernande G., Gary J.L. A structural magnetic and Mossbauer spectral study of the DyCo4–xFexB compounds with x = 0–3. Faculty Research Creative Works. Available at: http//scholarsmine.mst.edu/faculty_work/39 (accessed: June 15, 2022).
  9. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  10. Morgunov R.B., Piskorskiy V.P., Valeev R.A., Korolev D.V. The thermal stability of rare-earth magnets supported by means of the magnetocaloric effect. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 88–94. DOI: 10.18577/2071-9140-2019-0-1-88-94.
  11. Piskorsky V.P., Valeev R.A., Korolev D.V., Morgunov R.B., Rezchikova I.I. Terbium and gadolinium dopin g influence on thermal stability and magnetic properties of sintered magnets Pr–Tb–Gd–Fe–Co–B. Trudy VIAM, 2019, no. 7 (79), paper no. 07. Available at: http://www.viam-works.ru (accessed: June 15, 2022). DOI: 10.18577/2307-6046-2019-0-7-59-66.
  12. Koplak O.V., Kunitsyna E.I., Valeev R.A., Korolev D.V., Piskorskii V.P., Morgunov R.B. Ferromagnetic microwires α-Fe/(PrDy)(FeCo)B for micromanipulators and polymer composites. Trudy VIAM, 2019, no. 11 (83), paper no. 7. Available at: http://www.viam-works.ru (accessed: June 15, 2022). DOI: 10.18577/2307-6046-2019-0-11-60-67.
  13. Morgunov R.B., Koplak O.V., Talantsev A.D., Korolev D.V., Piskorskij V.P., Valeev R.A. The phenomenology of the magnetic hysteresis loops in multilayer microwires α-Fe/DyPrFeCoB. Trudy VIAM, 2019, no. 7 (79), paper no. 08. Available at: http://www.viam-works.ru (accessed: June 15, 2022). DOI: 10.18577/2307-6046-2019-0-7-67-75.
  14. Pedziwiatr A.T., Jiang S.Y., Wallace W.E. et al. Magnetic properties of RCo4B compounds where R = Y, Pr, Nd, Gd and Er. Journal of Magnetism and Magnetic Materials, 1987, vol. 66, pp. 69–73.
  15. Liao L.X., Altounian Z., Ryan D.H. Cobalt site preferences in iron rare-earth-based compounds. Physical Review B, 1993, vol. 47, no. 17, pp. 11230–11241.
  16. Bolzoni F., Leccabue F., Moze O. et al. 3d and 4f magnetism in Nd2Fe14–xCoxB and Y2Fe14–xCoxB compounds. Journal of Applied Physics, 1987, vol. 61, pp. 5369–5373.
  17. Buschow K.H.J., de Mooij D.B., Sinnema S. et al. Magnetic and crystallographic properties of ternary rare earth compounds of the type R2Co14B. Journal of Magnetism and Magnetic Materials, 1985, vol. 51, pp. 211–217.
  18. Ende M.V., Jung I., Kim Y.H., Kim T. Thermodynamic optimization of the Dy–Nd–Fe–B system and application in the recovery and recycling of rare earth metals from NdFeB magnet. Green Chemistry, 2015, vol. 17, pp. 2246–2261.