Phthalic anhydride application for hydroxyl groups contents determination in polyester 24K

Prokopova L.A.
Prokopova L.A. Phthalic anhydride application for hydroxyl groups contents determination in polyester 24K // Proceedings of VIAM. 2022. No. 1. DOI: 10.18577/2307-6046-2022-0-1-35-43. URL: https://viam-works.ru/en/journal/2022/1/4
Keywords
polyester, hydroxyl groups contents, phthalic acid anhydride, IR-spectroscopy, expiry, raw materials control
Abstract

The possibility of replacing acetic anhydride with phthalic anhydride when determining the hydroxyl groups contents in polyester 24K is discussed. Titrimetric analysis method obtained data on the content of these functional groups, consistent with previously analyzes. The reaction completeness was controlled by infrared spectroscopy, the results of which report on the successful process flow. Additionally, the reactivity of the product with an expired shelf life was checked.

Reference list
  1. Raskutin A.E. Development strategy of polymer composite materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
  2. Kablov E.N. Chemistry in Aviation Materials Science. Russian Journal of General Chemistry, 2011, vol. 81, no. 5. P. 967–969.
  3. State standart 22234–76. Polyester 24K. Specifications. Moscow: Publishing house of standards, 1989, 10 p.
  4. Kablov E.N. Aviation materials science: results and prospects. Vestnik RAN, 2002, vol. 72, no. 1, pp. 3–12.
  5. Petrova A.P., Malysheva G.V. Adhesives, adhesive binders and adhesive prepregs. Ed. E.N. Kablov. Moscow: VIAM, 2017, 472 p.
  6. Epoxypolyester paint composition: pat. 2472830 Rus. Federation, no. 2011140686/05; filed 07.10.11; publ. 20.01.13.
  7. Polymer radiotransparent composition: pat. 2570446 Rus. Federation, no. 2014137816/05; filed 18.09.14; publ. 10.12.15.
  8. Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review). Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
  9. Semenova L.V., Nefedov N.I., Belova M.V., Laptev A.B. Systems of paint coatings for helicopter equipment. Aviacionnye materialy i tehnologii, 2017, no. 4 (49), pp. 56–61. DOI: 10.18577/2071-9140-2017-0-4-56-61.
  10. Perov N.S. Design of polymer materials on the molecular principles. I. The development of polymer materials with additional mechanisms of dissipation of mechanical energy at low temperatures. Aviacionnye materialy i tehnologii, 2017, no. 3 (48), pp. 50–55. DOI: 10.18577/2071-9140-2017-0-3-50-55.
  11. Yakovlev A.D. Powder paints. Leningrad: Khimiya, 1987, 216 p.
  12. State Standard 17555–72. Plastics. Methods for determining the content of hydroxyl groups in epoxy resins and epoxidized compounds. Moscow: Publishing house of standards, 1979, 11 p.
  13. Nakanishi K. Infrared spectra and structure of organic compounds. Moscow: Mir, 1965, 219 p.
  14. Siggia S. Instrumental methods for the analysis of functional groups of organic compounds. Moscow: Mir, 1974, 464 p.
  15. Tarasevich B.N. IR spectra of the main classes of organic compounds: reference materials. Moscow: Lomonosov Moscow State University, 2012, 55 p.
  16. Kline G. Analytical chemistry of polymers. Moscow: Publ. of foreign literature, 1963, vol. 1, 592 p.
  17. Kline B.J., Beckman E.J., Russell A.J. One-step biocatalytic synthesis of linear polyesters with pendant hydroxyl groups. Journal of the American chemical society, 1998, vol. 120, no. 37, pp. 9475–9480. DOI: 10.1021/ja9808907.
  18. State Standard 25261–82. Polyethers are simple and complex for polyurethanes. Method for determining the hydroxyl number. Moscow: Publishing house of standards, 1982, 5 p.
  19. ASTM D4274-11. Standard Test Methods for Testing Polyurethane Raw Materials: Determination of Hydroxyl Numbers of Polyols. ASTM International, 2011, 9 p.