Study of the plasticizing effect of moisture on the properties of VSE-34 binder based PCMS after 5 years exposure in the different climate zones

Koval T.V., Veligodsky I.M., Gromova A.A.
Koval T.V., Veligodsky I.M., Gromova A.A. Study of the plasticizing effect of moisture on the properties of VSE-34 binder based PCMS after 5 years exposure in the different climate zones // Proceedings of VIAM. 2021. No. 9. DOI: 10.18577/2307-6046-2021-0-9-105-116. URL: https://viam-works.ru/en/journal/2021/9/11
Keywords
polymer composite materials, natural weathering, epoxy diane resin, CFRP, GFRP, moisture content, glass transition temperature, diffusion coefficient, strength.
Abstract

The plasticizing effect of moisture on the glass transition temperature of VSE-34 solvent-free epoxy binder based polymer composite materials (PCMs) with different reinforcement was studied. Natural weathering was performed in three climatic regions of Russia: Moscow, Gelendzhik, Sochi. It was shown that the glass transition temperature is significantly reduced after 1 year of exposure and then is gradually increased after 3 and 5 years of exposure. Samples were studied in «as-received» state as well as after drying and saturation by water till mass stabilization in order to investigate the moisture influence on PCMs’ glass transition temperature. Linear relationship between glass transition temperature and moisture content was observed.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Raskutin A.E. Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
  3. Popov Yu.O., Kolokoltseva T.V., Khrulkov A.V. The new generation of materials and technologies for helicopter blade spars. Aviacionnye materialy i tehnologii, 2014, no. S2, pp. 5–9. DOI: 10.18577/2071-9140-2014-0-S2-5-9.
  4. Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review). Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58.
  5. Startsev V.O., Plotnikov V.I., Antipov Yu.V. Reversible influence of moisture on the mechanical properties of PCM after weathering. Trudy VIAM, 2018, no. 5 (65), paper no. 12. Available at: http://www.viam-works.ru (accessed: June 18, 2021). DOI: 10.18577/2307-6046-2018-0-5-110-118.
  6. Soles C.L., Yee A.F. A discussion of the molecular mechanisms of moisture transport in epoxy resins. Journal of Polymer Science. Part B: Polymer Physics, 2000, vol. 38, no. 5, pp. 792–802.
  7. Startsev V.O., Lebedev M.P., Khrulev K. et al. Effect of outdoor exposure on the moisture diffusion and mechanical properties of epoxy polymers. Polymer Testing, 2018, vol. 65, pp. 281–296. DOI: 10.1016/j.polymertesting.2017.12.007.
  8. Neuser S., Michaud V. Effect of aging on the performance of solvent-based self-healing materials. Polymer Chemistry, 2013, vol. 4, no. 18, pp. 4993–4999. DOI: 10.1039/c3py00064h.
  9. Startsev V.O., Slavin A.V. Carbon and glass reinforced polymer based on solvent-free binders resistance to the impact of a moderate cold and moderate warm climate. Trudy VIAM, 2021, no. 5 (99), paper no. 12. Available at: http://www.viam-works.ru (accessed: June 18, 2021). DOI: 10.18577/2307-6046-2021-0-5-114-126.
  10. Sharp N., Li C., Strachan A., Adams D., Pipes R.B. Effects of water on epoxy cure kinetics and glass transition temperature utilizing molecular dynamics simulations. Journal of Polymer Science. Part B: Polymer Physics, 2017, vol. 55, no. 15, pp. 1150–1159. DOI: 10.1002/polb.24357.
  11. Lu M.G., Shim M.J., Kim S.W. Effects of moisture on properties of epoxy molding compounds. Journal of Applied Polymer Science, 2001, vol. 81, no. 9, pp. 2253–2259. DOI: 10.1002/app.1664.
  12. Zhou J., Lucas J.P. Hygrothermal effects of epoxy resin. Part II: variations of glass transition temperature. Polymer, 1999, vol. 40, no. 20, pp. 5513–5522. DOI: 10.1016s0032-3861(98)00791-5.
  13. Kovalenko A.V., Gurevich Ya.M., Lukina A.I., Sokolov I.I. Investigation of a complex of technological and operational properties of a spheroplastic based on an epoxy binder. Plasticheskiye massy, 2020. N, no. 5-6, pp. 52–54.
  14. Kolobkov A.S. Polymer composite materials for various aircraft structures (review). Trudy VIAM, 2020, no. 6–7 (89), paper no. 05. Available at: http://www.viam-works.ru (accessed: June 18, 2021). DOI: 10.18577/2307-6046-2020-0-67-38-44.
  15. Ivanov N.V., Gurevich Ya.M., Khaskov M.A., Akmeev A.R. Mode studying curing binding VSE-34 and its influences on mechanical properties. Aviacionnyye materialy i tehnologii, 2017, no. 2, pp. 50–55. DOI: 10.18577 / 2071-9140-2017-0-2-50-55.
  16. Markevich M.A., Kuzaev A.I., Sakhonenko L.S., Vladimorov L.V., Pekarskii V.A., Brusilov-
  17. skii M.G. Synthesis, Structure and Properties of Epoxydiane Polymers. Polymer Science U.S.S.R., 1984, vol. 26, no. 3, pp. 687–695. DOI: 10.1016/0032-3950(84)90408-8.
  18. Gunyaeva A.G., Sidorina A.I., Kurnosov A.O., Klimenko O.N. Polymeric composite materials of new generation on the basis of binder VSE-1212 and the filling agents alternative to ones of Porcher Ind. and Toho Tenax. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 18–26. DOI: 10.18577/2071-9140-2018-0-3-18-26.
  19. Molchanov E.S., Yudin V.E., Kydralieva K.A., Elokhovskii V.Y. Comparison of the thermomechanical characteristics of porcher carbon fabric-based composites for orthopaedic applications. Mechanics of Composite Materials, 2012, vol. 48, no. 3, pp. 343–350. DOI: 10.1007/s11029-012-9281-7.
  20. Timoshkov P.N., Khrulkov A.V., Yazvenko L.N. Composite materials in automotive industry (review). Trudy VIAM, 2017, no. 6 (54), paper no. 07. Available at: http://www.viam-works.ru (accessed: June 18, 2021). DOI: 10.18577/2307-6046-2017-0-6-7-7.
  21. Startsev O.V., Kablov E.N., Makhonkov A.Yu. Regularities of the transition of epoxy binder composite materials according to dynamic mechanical analysis. Vestnik Moskovskogo gosudarstvennogo tekhnicheskogo universiteta im. N.E. Baumana, ser.: Mechanical engineering. 2011, no. SP2, pp. 104–113.
  22. Panin S.V., Startsev O.V., Krotov A.S. Initial stage environmental degradation of the polymer matrix composites evaluated by Water diffusion coefficient. Trudy VIAM, 2014, no. 7, paper no. 09. Available at: http://viam-works.ru (accessed: June 18, 2021). DOI: 10.18577/2307-6046-2014-0-7-9-9.
  23. Koretskaya L., Aleksandrova T. Structural changes are inevitable. Influence of water on the properties of fiberglass. Polimernye truby, 2011, no. 1 (31), pp. 38–41.
  24. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Climatic aging of composite aviation materials: 1. Aging mechanisms. Russian Metallurgy (Metally), 2011, no. 10, pp. 993–1000. DOI: 10.1134/S0036029520100110.
  25. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Climatic aging of composite aviation materials: 2. Relaxation of the initial structural nenequilibrium and through thickness gradient of properties. Russian Metallurgy (Metally), 2011, no. 10, pp. 1001–1007. DOI: 10.1134/S0036029511100077.
  26. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Climatic aging of composite aviation materials: 3. Significant aging factors. Russian Metallurgy (Metally), 2012, no. 4, pp. 323–329. DOI: 10.1134/S0036029512040040.