Skupov A.A., Sviridov A.V., Khodakova E.A., Afanasiev-Khodykin A.N.
Skupov A.A., Sviridov A.V., Khodakova E.A., Afanasiev-Khodykin A.N. Creation of joints from intermetallic titanium alloys (review) // Proceedings of VIAM. 2021. No. 7. DOI: 10.18577/2307-6046-2021-0-7-31-38. URL: https://viam-works.ru/en/journal/2021/7/4
Keywords
electron-beam welding, laser welding, argon arc welding, intermetallic titanium alloys, filler materials, brazing, heat-resistant materials.
Abstract

An review of studies on the development of technologies for creating joints of intermetallic titanium alloys is presented. Today, electron beam welding is most common method for producing welded joints of this class of alloys. Brands of filler materials and solders used for intermetallic titanium alloys, as well as the properties that can be obtained when using them, are given. Approaches to the choice of welding technology that ensure the production of high-quality joints with the required characteristics are described.

Reference list
  1. Nochovnaya N.A., Bazyleva O.A., Kablov D.E., Panin P.V. Intermetallic alloys based on titanium and nickel. ed. E.N. Kablov. Moscow: VIAM, 2018, 308 p.
  2. Kablov E.N., Lukin V.I. Intermetallic compounds based on titanium and nickel for new technology products. Avtomaticheskaya svarka, 2008, no. 11, pp. 76–82.
  3. Kablov E.N., Kashapov O.S., Medvedev P.N., Pavlova T.V. Study of a α+β-titanium alloy based on a system of Ti–Al–Sn–Zr–Si–β-stabilizing alloying elements. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 30–37. DOI: 10.18577/2071-9140-2020-0-1-30-37.
  4. Kablov D.E., Panin P.V., Shiryaev A.A., Nochovnaya N.A. The use of ADL VAR L200 vacuum-arc furnace for ingots fabrication of high-temperature titanium aluminides base alloys. Aviacionnye materialy i tehnologii, 2014, no. 2, pp. 27–33. DOI: 10.18577/2071-9140-2014-0-2-27-33.
  5. Antashev V.G., Nochovnaya N.A., Pavlova T.V., Ivanov V.I. Heat-resistant titanium alloys. Vse materialy. Entsiklopedicheskiy spravochnik, 2007, no. 3, pp. 7–8.
  6. Dzunovich D.A., Alekseyev E.B., Panin P.V., Lukina E.A., Novak A.V. Structure and properties of sheet semi-finished products from various wrought intermetallic titanium alloys. Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 17–25. DOI: 10.18577/2071-9140-2018-0-2-17-25.
  7. Cao J., Qi J., Song X., Feng J. Welding and Joining of Titanium Aluminides. Materials, 2014, no.7, pp. 4930–4962.
  8. Bewlay B.P., Nag S., Suzuki A., Weimer M.J. TiAl alloys in commercial aircraft engines. Materials at High Temperatures, 2016, no. 33 (4–5), pp. 549–559.
  9. Loretto M.H., Godfrey A.B., Hu D. et al. The influence of composition and processing on the structure and properties of TiAl-based alloys. Intermetallics, 1998, no. 6 (7–8), pp. 663–666.
  10. Panteleev M.D., Bakradze M.M., Skupov A.A., Scherbakov A.V., Belozor V.E. Technological features of fusion welding of aluminum alloy V-1579. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 11–17. DOI: 10.18577/2071-9140-2018-0-3-11-17.
  11. Skupov A.A., Panteleev M.D., Ioda E.N., Movenko D.A. The efficiency of rare earth metals for filler materials alloying. Aviacionnye materialy i tehnologii, 2017, no. 3 (48), pp. 14–19. DOI: 10.18577/2071-9140-2017-0-3-14-19.
  12. Kablov E.N., Lukin V.I., Ospennikova O.G. Welding and soldering is in the aerospace industry. Proceedings of All-Rus. Scientific and Practical Confference «Welding and safety». Yakutsk: IFTPS SB RAS, 2012, pp. 21–30.
  13. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  14. Chen B., Xiongn H., Sun B. et al. Microstructures and mechanical properties of Ti3Al/Ni-based superalloy joints arc welded with Ti–Nb and Ti–Ni–Nb filler alloys. Progress in Natural Science: Materials International, 2014, no. 24, pp. 313–320.
  15. Liu X.L., Wu S.J., Ji Y.P. et al. Ultrasonic frequency pulse tungsten inert gas welding of Ti2AlNb-based alloy. Chinese Journal of Rare Metals, 2014, vol. 38, no. 4, pp. 541–547.
  16. Arenas M.F., Acoff V.L. An investigation of the cracking susceptibility of gamma titanium aluminide welds produced by gas tungsten arc welding. High temperature materials processes, 2014, vol. 23, no. 1, pp. 25–34.
  17. Chaturvedi M.C., Richards N.L., Xu Q. Electron beam welding of a Ti–45Al–2Nb–2Mn + 0.8 vol. % TiB2 XD alloy. Material Science and Engineering: A, 1997, vol. 239–240, pp. 605–612.
  18. Reisgen U., Olschok S., Backhaus A. Electron beam welding of titanium aluminides – Influence of the welding parameters on the weld seam and microstructure. Materialwissenschaft und Werkstofftechnik, 2010, vol. 41, no 11, pp. 897–907. DOI: 10.1002/mawe.201000683.
  19. Kuwahara G., Yamaguchi S., Nanri K. et al. CO2 laser welding of titanium aluminide intermetallic compound. Proceedings of SPIE, 2000, vol. 3888, pp. 411–417.
  20. Davies P.D., Davies H.M., Watkins I., Britton D.A. The joining of gamma titanium aluminides via the powder interlayer bonding method. The international journal of advanced manufacturing technology, 2020, no. 109, pp. 2049–2054.
  21. Chen G.Q., Zhang B.G., Liu W., Feng J.C. Crack formation and control upon the electron beam welding of TiAl-based alloys. Intermetallics, 2011, no. 19, pp. 1857–1863.
  22. Chaturvedi M.C., Xu Q., Richards N.L. Development of crack-free welds in a TiAl-based alloy. Journal of Materials Processing Technology, 2001, vol. 118, no. 1, pp. 74–78. DOI: 10.1016/S0924-0136(01)00870-6.
  23. Lei Zh., Dong Zh., Chen Ya. et al. Microstructure and tensile properties of laser beam welded Ti–22Al–27Nb alloys. Materials & Design, 2013, vol. 46, pp. 151–156. DOI: 10.1016/j.mades.2010.10.022.
  24. Auwal S.T., Ramesh S., Yusof F., Manladan S.M. A review on laser beam welding of titanium alloys. The International Journal of Advanced Manufacturing Technology, 2018, vol. 97, no. 1, pp. 1–28. DOI: 10.1007/s00170-018-2030-x.
  25. Arenas M.F., Acoff V.L. Analysis of gamma titanium aluminide welds produced by gas tungsten arc welding. Welding Journal, 2003, no. 5, pp. 110–115.
  26. Wang L., Sun D., Li H. et al. Microstructures and mechanical properties of a laser-welded joint of Ti3Al–Nb alloy using pure Nb filler metal. Metals – Open Access Metallurgy Journal, 2018, vol. 8, no. 10, pp. 785. DOI: 10.3390/met8100785.
  27. Cai X., Sun D., Li H. et al. Microstructure characteristics and mechanical properties of laser-welded joint of γ-TiAl alloy with pure Ti filler metal. Optics & Laser Technology, 2017, vol. 97, pp. 242–247. DOI: 10.1016/j.optlastec.2017.07.011.
  28. Chen X., Xie F.Q., Mab T.J. et al. Microstructure evolution and mechanical properties of linear friction welded Ti2AlNb alloy. Journal of alloys and compounds, 2015, vol. 646, pp. 490–496.
  29. Shapiro A., Rabinkin A. State of the art of titanium-based brazing filler metals. Welding Journal, 2003, vol. 82, no. 10, pp. 36–43.
  30. TiNiNbZr high-temperature brazing filler metal for TiAl alloy, preparation method and brazing method thereof: pat. CN 110605498A; filed 14.05.19; publ. 24.12.19.
  31. Brazing filler metal for brazing titanium-containing material, preparation method and brazing method: pat. CN 110666395A; filed 21.10.19; publ. 10.01.20.
  32. Ti–Zr–Cu–Ni–Co–Mo amorphous brazing filler metal and preparing method thereof: pat. CN 103949802A; filed 23.04.14; publ. 30.07.14.
  33. Ti-based filler alloy compositions: pat. WO 2014169133A1; filed 10.04.14; publ. 16.10.14.
  34. Titanium-based amorphous brazing alloy foil strip for brazing and preparation method for foil strip: pat. CN 102430874A; filed 01.11.11; publ. 02.05.12.