Repair of nozzle blades made of heat-resistant nickel alloy ZhS6U

Dobrynin D.A., Alekseeva M.S., Afanasiev-Khodykin A.N.
Dobrynin D.A., Alekseeva M.S., Afanasiev-Khodykin A.N. Repair of nozzle blades made of heat-resistant nickel alloy ZhS6U // Proceedings of VIAM. 2021. No. 5. DOI: 10.18577/2307-6046-2021-0-5-3-13. URL: https://viam-works.ru/en/journal/2021/5/1
Keywords
repair of gas turbine engine nozzle blades, high-temperature nickel alloy ZhS6U, spent diffusion aluminide coating, hot isostatic pressing, thermal, hydrothermal and thermochemical treatment, electrolyt
Abstract

An overview of traditional methods for cleaning the surface of gas turbine engine (GTE) blades from products of gas corrosion and spent coating, methods for restoring the structure and properties of the material of blades using hot isostatic pressing and heat treatment, as well as methods for applying coatings on the inner and outer surfaces of the blades is presented. The main disadvantages of these methods are described, taking into account which the state-of-the-art technology for repairing gas-turbine engine nozzle blades made of ZhS6U alloy has been developed in FSUE «VIAM», which ensures an increase in their resource and a reduction in repair costs.

Reference list
  1. Kablov E.N., Muboyadzhyan S.A. Heat resisting and heat-protective coverings for turbine blades of high pressure of perspective GTE. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 60–70.
  2. Kablov E.N., Muboyadzhyan S.A. Protective coatings for turbine blades of promising gas turbine engines. Gazoturbinnye tekhnologii, 2001, no. 3, pp. 30–32.
  3. Popova S.V., Muboyadzhyan S.A., Budinovskiy S.A., Dobrynin D.A. The feature of electrolytic plasma etching of heat resistant coatings from parts surface of high-temperature nickel alloys. Trudy VIAM, 2016, no. 2 (38), paper no. 04. Available at: http://www.viam-works.ru (accessed: March 15, 2021). DOI: 10.18577/2307-6046-2016-0-2-4-4.
  4. Kablov E.N., Muboyadzhyan S.A., Budinovskiy S.A., Lutsenko A.N. Ion-plasma protective coatings for blades of gas turbine engines. Metally, 2007, no. 5. P. 23–34.
  5. Kosmin A.A., Budinovskiy S.A., Muboyadzhyan S.A. Heat and corrosion resistant coating for working turbine blades from promising high-temperature alloy VZhL21. Aviacionnye materialy i tehnologii, 2017, no. 1 (46), pp. 17–24. DOI: 10.18577/2071-9140-2017-0-1-17-24.
  6. Muboyadzhyan S.A., Budinovskij S.A. Ion-plasma technology: prospective processes, coatings, equipment. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 39–54. DOI: 10.18577/2071-9140-2017-0-S-39-54.
  7. Tikhomirova E.A., Budinovsky S.A., Zhivushkin A.A., Sidokhin E.F. Features of thermal fatigue development in details, produced from heat-resistant alloys with coatings. Aviacionnye materialy i tehnologii, 2017, no. 3 (48), pp. 20–25. DOI: 10.18577/2071-9140-2017-0-3-20-25.
  8. Kablov E.N., Ospennikova O.G., Svetlov I.L. Highly efficient cooling of GTE hot section blades. Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 3–14. DOI: 10.18577/2071-9140-2017-0-2-3-14.
  9. Process for treating the surface of a component, made from a Ni based supperalloy, to be coated: pat. US 6440238B1; filed 09.08.99; publ. 27.08.02.
  10. A method of processing channels for cooling turbine blades of a gas turbine engine: pat. 2417145С2 Rus. Federation; filed 15.07.09; publ. 27.04.11.
  11. Contact solution, method and installation for cleaning the surface of metal alloys, including the surface of cracks and narrow gaps: pat. 2419684С2 Rus. Federation; filed 04.06.09; publ. 27.05.11.
  12. Method for electrochemical cleaning of metal products: pat. 2411310S2 Rus. Federation; filed 20.02.09; publ. 10.02.11.
  13. Method for electrochemical cleaning of metal products: pat. 2099445С1 Rus. Federation; filed 22.07.94; publ. 20.12.97.
  14. Method for cleaning metal surfaces from deposits: pat. 2169794С1 Rus. Federation; filed 15.11.00; publ. 27.06.01.
  15. Method for removing the coating from a metal substrate: pat. 2094546С1 Rus. Federation; filed 15.11.00; publ. 27.06.01.
  16. Method for removing heat-resistant metal coating: pat. 2228396С1 Rus. Federation; filed 19.09.02; publ. 10.05.04.
  17. Device and method for removing the coating: pat. 2215068С2 Rus. Federation; filed 17.12.00; publ. 27.10.03.
  18. Method of removing heat-resistant coating from parts made of heat-resistant nickel alloys: pat. 2339738С1 Rus. Federation; filed 27.03.07; publ. 27.11.08.
  19. Method for removing coatings from parts made of heat-resistant alloys: pat. 2200211C2 Rus. Federation; filed 07.03.01; publ. 10.03.03.
  20. Nickel heat-resistant alloy, a product made of it, and a method of heat treatment of the alloy and products from it: pat. 2220220С1 Rus. Federation; filed 05.08.02; publ. 27.12.03.
  21. Method of heat treatment of parts made of heat-resistant alloys based on nickel: pat. 2232204С2 Rus. Federation; filed 09.09.02; publ. 10.07.04.
  22. Method of regenerative heat treatment of products made of heat-resistant nickel alloys: pat. 2459885С1 Rus. Federation; filed 15.07.11; publ. 27.08.12.
  23. Method of protecting the surface of the blade: pat. 2252110С1 Rus. Federation; filed 09.10.03; publ. 20.05.05.
  24. Method of restoring repair of gas turbine engine parts made of heat-resistant nickel alloys: pat. 2346799С2 Rus. Federation; filed 01.03.07; publ. 20.02.09.
  25. A method of processing castings with a monocrystalline structure from heat-resistant nickel alloys with hot isostatic pressing: pat. 2380454С1 Rus. Federation; filed 11.06.08; publ. 27.01.10.
  26. Method of applying a combined coating: pat. 2244041С1 Rus. Federation; filed 29.04.03; publ. 10.01.05.
  27. The composition of the mixture for multiple chromoalitization: pat. 2266349С1 Rus. Federation; filed 07.06.04; publ. 20.12.05.
  28. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  29. Ospennikova O.G., Orlov M.R., Gubenko L.A. Ensuring the quality of the surface of the blades in the process of hydrothermal leaching of ceramic rods. Liteinoe proizvodstvo, 2007, no. 8, pp. 31–34.
  30. Orlov M.R. Pore formation in monocrystalline turbine rotor blades in the process of directional solidification. Metally, 2008, no. 1, pp. 70–75.
  31. Orlov M.R. Physicochemical features of the formation of pores of thermal origin and the performance of single-crystal turbine blades. Deformatsiya i razrusheniye materialov, 2008, no. 6. P. 43–48.
  32. Orlov M.R., Orlov E.M. Hydrogen brittleness of monocrystalline heat-resistant nickel alloys. Deformatsiya i razrusheniye materialov, 2008, no. 7, pp. 36–41.