Improvement of the chemical composition and structure of castable nickel-based superalloy with low density

Part 2
Petrushin N.V., Visik E.M., Elyutin E.S.
Petrushin N.V., Visik E.M., Elyutin E.S. Improvement of the chemical composition and structure of castable nickel-based superalloy with low density. Part 2 // Proceedings of VIAM. 2021. No. 4. DOI: 10.18577/2307-6046-2021-0-4-3-15. URL: https://viam-works.ru/en/journal/2021/4/1
Keywords
castable nickel-based superalloys, computer design, microstructure, phase stability, density, mechanical properties, long-term strength.
Abstract

Results of design and experimental studies of a nickel-based superalloy VZhL20 with a density of 8.04 g/cm3 for the manufacture of turbine blades with a columnar granular structure and a single-crystal structure are presented. It is shown that alloy VZHL20 with a single-crystal structure of the crystallographic orientation [001] in the heat-treated state possesses high phase stability, and enhanced short-term strength (\( \sigma_{0,2}^{20} = 950 \, \text{МПа} \) и \( \sigma_{\delta}^{20} = 1130 \, \text{МПа} \)) and long-term strength (\( \sigma_{100}^{900} = 340 \, \text{МПа} \) и \( \sigma_{100}^{1000} = 185 \, \text{МПа} \))

Reference list
  1. Ospennikova O.G. Strategy of development of hot strength alloys and steels special purpose, protective and heat-protective coverings Aviacionnye materialy i tehnologii, 2012, no. S, pp. 19–36.
  2. Bondarenko Yu.A. Trends in the development of high-temperature metal materials and technologies in the production of modern aircraft gas turbine engines. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 3–11. DOI: 10.18577 / 2071-9140-2019-0-2-3-11.
  3. Kablov E.N. Casting heat-resistant alloys. Mechanical engineering: encyclopedia in 40 vols. Moscow: Mashinostroyenie, 2001, vol. II-3: Non-ferrous metals and alloys. Composite materials, pp. 519−552.
  4. Nazarkin R.M., Kolodochkina V.G., Ospennikova O.G., Orlov. M.R. The microstructure modifications of single crystals of Ni-based superalloys in time-tested turbine blades. Aviacionnye materialy i tehnologii, 2016, no. 4 (45), pp. 9–17. DOI: 10.18577/2071-9140-2016-0-4-9-17.
  5. Walston W.S., O'Hara K.S., Ross E.W., Pollock T.M., Murphy W.H. René N6: Third generation single crystal superalloy. Superalloys. Pennsylvania: Minerals, Metals and Materials Society, 1996, pp. 27–34.
  6. Jo C.-Y., Jones N., Choe S.-J., Knowles D. High temperature mechanical properties and creep crack initiation of DS CM186LC for nozzle guide vane. Metals and Materials, 1998, vol. 4, no. 5, pp. 1017-1025.
  7. Kablov E.N., Ospennikova O.G., Petrushin N.V., Visik E.M. Single-crystal nickel-based superalloy of a new generation with low-density. Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 14–25. DOI: 10.18577/2071-9140-2015-0-2-14-25.
  8. Toloraya V.N., Kablov E.N., Orekhov N.G. Casting technologies for single-crystal turbine blades of GTE and GTU. Aviacionnye materialy i tehnologii, 2003, no. 1, pp. 63–79.
  9. Low carbon directional solidification alloy – CM186LC: pat. US 5069873; filed 14.08.89; publ. 03.12.91.
  10. Ross E.W., O'Hara K.S. RENÉ N4: A first generation single crystal turbine airfoil alloy with improved oxidation resistance, low angle boundary strength and superior long time rupture strength. Superalloys. Pennsylvania: Minerals, Metals and Materials Society, 1996, pp. 19–25.
  11. Kablov E.N., Petrushin N.V. Computer-aided design method for casting heat-resistant nickel alloys. Foundry heat-resistant alloys. The effect of S.T. Kishkina. Moscow: Nauka, 2006, pp. 56–78.
  12. Gerasimov V.V., Petrushin N.V., Visik E.M. Improvement of casting technology and composition of single crystal blades made of heat-resistant intermetallic alloy. Trudy VIAM, 2015, no. 3, paper no. 01. Available at: http://www.viam-works.ru (accessed: December 21, 2020). DOI: 10.18577/2307-6046-2015-0-3-1-1.
  13. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  14. Petrushin N.V., Visik E.M., Elyutin E.S. Improvement of the chemical composition and structure of castable nickel-base superalloy with low density. Part 1. Trudy VIAM, 2021, no. 3 (97), paper no. Available at: http://www.viam-works.ru (date of access: March 15, 2021). DOI: 10.18577/2307-6046-2021-0-3-3-15.
  15. Zadgenidze I.G. Planning an experiment for the study of multicomponent systems. Moscow: Nauka, 1976, 390 p.
  16. Kablov E.N., Petrushin N.V., Parfenovich P.I. Construction of cast heat-resistant nickel alloys with polycrystalline structure. Metallovedenie i termicheskaya obrabotka metallov, 2018, no. 2 (752), pp. 47–55.
  17. Morozova G.I. Regularity of the formation of the chemical composition of γʹ/γ-matrices of multicomponent nickel alloys. Doklady Akademii nauk SSSR, 1991, vol. 320, no. 6, pp. 1413–1416.
  18. Morozova G.I. The importance of physicochemical phase analysis technique in the development of aviation metallic material science and creation of Ni-based superalloys. Trudy VIAM, 2016, no. 1 (37), paper no. 7. Available at: http://www.viam-works.ru (accessed: December 10, 2020). DOI: 10.18577/2307-6046-2016-0-1-50-55.
  19. Yukawa N., Morinaga M., Ezaki H., Murata Y. Alloy design of superalloys by the d-electrons concept. High temperature alloys for gas turbines and other applications: Proceedings of Conference. Dordrecht: CRM, 1986, pp. 935–944.
  20. Argence D., Vernault C., Desvallees Y., Fournier D. MC-NG: a 4th generation single-crystal superalloy for future aeronautical turbine blades and vanes. Superalloys. Pennsylvania: Minerals, Metals & Materials Society, 2000, pp. 829–837.
  21. Visik E.M., Gerasimov V.V., Petrushin N.V., Kolyadov E.V., Filonova E.V. Technological testing of casting of monocrystalline blades from a heat-resistant nickel alloy VZhL20 of low density. Liteyshchik Rossii, 2018, no. 5, pp. 17–22.
  22. Toloraya V.N., Kablov E.N., Orekhov N.G., Demonis I.M., Ostroukhova G.A., Chubarova E.N. Methods of obtaining single crystals of nickel heat-resistant alloys. Proceedings of the Mezhdunar. scientific and technical conf. “Scientific ideas of S.T. Kishkina and modern materials science”. Moscow: VIAM, 2006, pp. 270–279.
  23. Kuzmina N.A., Pyankova L.A. Control of crystallographic orientation of monocrystalline nickel castings heat-resistant alloys by х-ray diffractometry. Trudy VIAM, 2019, no. 12 (84), paper no. 02. Available at: http://www.viam-works.ru (accessed: August 12, 2020). DOI: 10.18577/2307-6046-2019-0-12-11-19.
  24. Nazarkin R.M. X-ray diffraction techniques for precise determination of lattice constants in Ni-based superalloys: a brief review. Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 41–48. DOI: 10.18577/2071-9140-2015-0-1-41-48
  25. Kablov E.N., Golubovsky E.R. Heat resistance of nickel alloys. Moscow: Mashinostroenie, 1998, 464 p.
  26. Golikov I.N., Maslenkov S.B. Dendritic segregation in steels and alloys. Moscow: Metallurgiya, 1977, 224 p.
  27. Reed R.C. The Superalloys. Fundamentals and Applications. Cambridge: United Kingdom at University Press, 2006, 372 p.
  28. Gabb T.P., Dreshfill R.L. Properties of superalloys. Superalloys II. Heat-resistant materials for aerospace and industrial power plants: in 2 vols. Ed. Ch.T. Sims, N.S. Stoloff, W.C. Hagel. Moscow: Metallurgy, 1995, book 2, pp. 352–371.