Research of properties of glues and glue binding, made with use of modern domestic component base

Isaev A.Yu., Rubtsova E.V., Kotova E.V., Sutyagin M.N.
Isaev A.Yu., Rubtsova E.V., Kotova E.V., Sutyagin M.N. Research of properties of glues and glue binding, made with use of modern domestic component base // Proceedings of VIAM. 2021. No. 3. DOI: 10.18577/2307-6046-2021-0-3-58-67. URL: https://viam-works.ru/en/journal/2021/3/5
Keywords
glue, epoxy glue of the cold curing, foaming glue, film glue, glue binding, filler, curing, strength characteristics, heat resistance, utilization properties.
Abstract

Properties of epoxy glues of cold curing VK-9 and VKV-9, the components received with use which are let out by modern producers, depending on the filler used in their structure are considered. Tests of glued joints on VK-9 glue in wider interval of temperatures are carried out. Properties of VK-36 glue and its updating’s on the basis of components let out now are shown. Properties of glue binding brands VSK-14-1, VSK-14-2, VSK-14-4, VSK-14-4m and VSK-14-4k received, under production conditions by VIAM Federal State Unitary Enterprise are given. It is shown that on the properties they completely meet the requirements of existing normative documentation.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  3. Grashhenkov D.V., Chursova L.V. Strategy of development of composite and functional materials. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 231–242.
  4. Petrova A.P., Malysheva G.V. Adhesives, adhesive binders and adhesive prepregs. Ed. E.N. Kablov. Moscow: VIAM, 2017, 472 p.
  5. Petrova A.P., Donskoy A.A., Chalykh A.E., Shcherbina A.A. Adhesive materials. Sealants: a reference book. Saint Peterburg: Professional, 2008. 589 p.
  6. Sharova I. A. Domestic and foreign experience in area of cold curing epoxy adhesive development. Trudy VIAM, 2014, no. 7, paper no. 05. Available at: http://viam-works.ru (accessed: October 21, 2020). DOI: 10.18577/2307-6046-2014-0-7-5-5.
  7. Sharova I.A. Epoxy cold curing adhesives for bonding and repairing aircraft parts: thesis abstract, Cand. Sc. (Tech.). Moscow: VIAM, 2015, 26 p.
  8. Sharova I.A., Lukina N.F., Aleksashin V.M., Antyufeeva N.V. Influence of the composition on the kinetic and strength properties of rapidly hardening epoxy adhesive compositions. Klei. Germetiki. Tekhnologii, 2015, no. 2, pp. 1–5.
  9. Petrova A.P. Foaming adhesives and their use in aircraft construction. Klei. Germetiki. Tekhnologii, 2015, no. 1, pp. 2–5.
  10. Petrova A.P., Lukina N.F. Foaming adhesives. Klei. Germetiki. Tekhnologii, 2006, no. 9, pp. 2–5.
  11. Lukina N.F., Petrova A.P., Muhametov R.R., Kogtjonkov A.S. New developments in the field of adhesive aviation materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 452–459. DOI: 10.18577/2071-9140-2017-0-S-452-459.
  12. Dementyeva L.A., Kutsevich K.E., Lukina N.F., Petrova A.P. Properties of epoxy structural adhesives modified with polysulfones. Klei. Germetiki. Tekhnologii, 2016, no. 11, pp. 13–18.
  13. Kablov E.N., Chursova L.V., Lukina N.F., Kutsevich K.E., Rubtsova E.V., Petrova A.P. Investigation of epoxy-polysulfone polymer systems as a basis for high-strength adhesives for aviation purposes. Sealants. Technologies. 2017, no. 3, pp. 7–12.
  14. Petrova A.P., Dementyeva L.A., Lukina N.F., Anikhovskaya L.I. Film construction adhesives. Klei. Germetiki. Tekhnologii, 2014, no. 10, pp. 7–12.
  15. Lukina N.F., Dementeva L.A., Petrova A.P., Anihovskaya L.I. Gluing materials in the design of blades of helicopters. Trudy VIAM, 2016, no. 7, paper no. 07. Available at: http://www.viam-works.ru (accessed: November 6, 2021). DOI: 10.18577/2307-6046-2016-0-7-7-7.
  16. Lukina N.F., Dementeva L.A., Petrova A.P., Serezhenkov A.A. Constructional and heat-resistant glues. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 328–335.
  17. Lukina N.F., Dementyeva L.A., Petrova A.P., Tyumeneva T.Yu. Properties of adhesives and adhesives for aircraft products. Klei. Germetiki. Tekhnologii, 2009, no. 1, pp. 14–24.
  18. Petrova A.P., Lukina N.F., Dementyeva L.A., Tyumeneva T.Yu., Avdonina I.A., Zhadova N.S. Adhesives for aviation technology. Rossiyskiy khimicheskiy zhurnal, 2010, vol. LIV, no.1, pp. 46–52.
  19. Rubtsova E.V., Sharova I.A., Petrova A.P. High-strength film adhesive VK-36T based on epoxy-polysulfone system. Novosti materialovedeniya. Nauka i tekhnika, 2016, no. 6, paper no. 08. URL: http://materialsnews.ru (accessed: October 13, 2020)
  20. Kutsevich K.E., Dementyeva L.A., Lukina N.F., Chursova L.V. Properties and purposes of VK-36RM glue for aviation technology. Klei. Germetiki. Tekhnologii, 2013, no. 8, pp. 5–6.
  21. Kutsevich K.E. Adhesive prepregs and carbon composites based on them: thesis, Cand. Sc. (Tech.). Moscow: VIAM, 2014, 102 p.
  22. Lukina N.F., Dementeva L.A., Kutsevich K.E. Adhesive prepregs based on tissue Porsher – perspective materials for parts and units out of polymeric composite materials. Trudy VIAM, 2014, no. 6, paper no. 10. Available at: http://www.viam-works.ru (accessed: October 13, 2020). DOI: 10.18577/2307-6046-2014-0-6-10-10.
  23. Petrovа A.P., Dementyevа L.A., Lukina N.F., Chursova L.V. Adhesive binders for polymer composite materials based on carbon- and glass fillers. Trudy VIAM, 2015, no. 9, paper no. 11. Available at: http://www.viam-works.ru (accessed: October 19, 2020). DOI: 10.18577/2307-6046-2015-0-9-11-11.