MIM technology as a method of manufacturing precision parts from metal-powder compositions, including titanium alloys (review)

Vasilev A.I., Putyrskiy S.V., Korotchenko A.Yu., Anisimova A.Yu.
Vasilev A.I., Putyrskiy S.V., Korotchenko A.Yu., Anisimova A.Yu. MIM technology as a method of manufacturing precision parts from metal-powder compositions, including titanium alloys (review) // Proceedings of VIAM. 2021. No. 3. DOI: 10.18577/2307-6046-2021-0-3-16-27. URL: https://viam-works.ru/en/journal/2021/3/2
Keywords
MIM technology, titanium alloys, powder technologies, additive manufacturing, microstructure, feedstock.
Abstract

The overview of MIM technology application (injection molding technologies for parts based on metal-powder compositions) as a method of manufacturing precision parts from metal-powder compositions is represented in this article. The features of the manufacturing of parts by additive technologies are also considered. The main stages of the technological process are given. Applied industries and using material statistic data are reflected. The focus was made on analyze of opportunity of application MIM technology in the manufacturing parts from titanium alloys.

Reference list
  1. Gamidov G.S., Adeev Z.I., Kuchuv K.A. Features of a systematic approach to assessing the accuracy of manufacturing parts for internal combustion engines. Obrabotka metallov rezaniem, 2008. T. 2, no. 44, pp. 16–18.
  2. Chainov N.D., Myagkov L.L., Moskvichev Yu.P. New structural materials – granular composites and the effectiveness of their application in engine building. Collection of scientific. tr. Int. conf. "Engine-2010", dedicated to 180th anniversary of N.E. Bauman MSTU. Moscow, 2010, pp. 67–70.
  3. Tverskoy M.V., Khilkova A.A., Khilkov D.E. Investigation of the features of injection molding of metal powder mixtures. Politekhnicheskiy molodezhny zhurnal N.E. Baumana MGTU, 2018, no. 11 (28), pp. 406–407.
  4. Ramakrishnan P. Automotive applications of powder metallurgy. Advances in powder metallurgy, 2013, no. 7, pp. 493–519.
  5. Semenov B.I., Semenov A.B., Muranov A.N. Processing and properties of superalloys suitable for MIM. Modern heat-resistant wrought nickel and intermetallic alloys, methods of their processing: collection of articles of conf. Moscow: VIAM, 2015, pp. 10–13.
  6. Hausnerova B. Powder Injection Molding as an Alternative Processing Method for Automotive Items. PIM International, 2011, no. 3, pp. 129–146.
  7. Semenov A.B., Muranov A.N., Kutsbakh A.A., Semenov B.I. Injection molding of structured multiphase materials. Vestnik RUDN, ser.: Engineering research, 2017, vol. 18, no.4, pp. 407–425.
  8. Semenov A.B., Muranov A.N., Semenov B.I. Thixo- and PIM-technologies in modern engine building. Gruzovik, 2017, no. 10, pp. 3–6.
  9. Public analytical report in the direction of "New production technologies". Moscow: Skolkovo Institute of Science and Technology, 2015, 210 p.
  10. Pogodina E. Casting of powder mixtures. Plastiks. Effektivnye TPA, 2013, no. 6 (124), pp. 34–36.
  11. Parkhomenko A.V. Development of binders in granulates for MIM technology. Vestnik Samarskogo gosudarstvennogo tekhnicheskogo universiteta, ser.: Technical sciences. 2013, no. 2, pp. 91–98.
  12. Starting material for injection molding of metal powder: pat. US 5006164A; filed 02.26.90; publ. 09.04.91.
  13. Peskova A.V., Sukhov D.I., Mazalov P.B. Exami-nation of the formation of the titanium alloy VT6 structure obtained by additive manufacturing. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 38–44. DOI: 10.18577 / 2071-9140-2020-0-1-38-44.
  14. Korotchenko A.Yu., Kotomin S.V., Tverskoy M.V., Khilkov D.E. Development of a new composition of a metal powder mixture for molding under pressure. Liteynoye proizvodstvo, 2018, no. 2, pp. 23–27.
  15. Muranov A.N. Investigation of free shrinkage of the main types of polymer-powder mixtures used for the manufacture of parts from powder analogs of 38KhMA (42CrMo4) steel by the MIM method. Mekhanika kompozitsionnykh materialov i konstruktsiy, 2019, vol. 25, no. 1, pp. 76–86.
  16. Yakovlev A.L., Arislanov A.A., Putyrsky S.V., Nochovnaya N.A. Study of mechanical properties and structure of large-sized semi-finished products made of VT6ch titanium alloy. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 12–18. DOI: 10.18577 / 2071-9140-2020-0-4-12-18.
  17. Parkhomenko A.V. Characteristics of MIM granules based on carbonyl iron powder of the NM grade and polyformaldehyde. Intellektualnyj potentsial XXI veka: stupeni poznaniya, 2016, no. 32, pp. 89–93.
  18. Thermoplastic masses for preparing metallic moldings: pat. EP 0465940-B1; filed 15.01.92; publ. 17.05.95.
  19. Semenov A.B. Development of a methodology for mathematical modeling of the process of injection molding of polymers filled with metal powders. Tekhnologiya metallov, 2019, no. 1, pp. 9-16.
  20. Semenov A.B., Semenov B.I. Two paradigms of metal casting technologies. Izvestiya vuzov. Mechanical engineering, 2017, no. 5, pp. 79–98.
  21. Kablov E.N., Evgenov A.G., Ospennikova O.G. et al. Metal-powder compositions of EP648 heat-resistant alloy produced by FSUE "VIAM" State Scientific Center of the Russian Federation in technologies of selective laser alloying, laser gas-powder surfacing and high-precision casting of polymers filled with metal powders. Izvestiya vuzov. Mechanical engineering, 2016, no. 9, pp. 62–80.
  22. Froes (Sam) F.H. Advances in titanium metal injection molding. Powder Metallurgy and Metal Ceramics, 2007, vol. 46, p. 303–310.
  23. German R.M. Powder Metallurgy Science. 2nd ed. New Jersey: MPIF Princeton, 1994. Chap. 6. 192 p.
  24. Froes (Sam) F.H., Yau Te-Lin, Weidenger H.G. Titanium, Zirconium and Hafnium. Chap. 8. Materials Science and Technology – Structure and Properties of Nonferrous Alloys. Ed. K.H. Matucha. Weinheim: VCH, 1996, p. 401.
  25. Froes (Sam) F.H. Titanium. Encyclopedia of Materials Science and Engineering. Oxford: Elsevier, 2000, pp. 328–340.
  26. Froes (Sam) F.H. Titanium Alloys. Handbook of Advanced Materials. Wessel: Wiley Interscience, 2004. P. 271.
  27. Froes (Sam) F.H. Titanium Metal Alloys: Handbook of Chemical Industry Economics, Inorganic. New York: John Wiley and Sons Inc., 2000, pp. 44–50.
  28. Kang L. Ceramic Membranes for Separation and Reaction. London: John Wiley and Sons, 2007, 306 p.
  29. Boljanovic V. Powder metallurgy. Metal Shaping Processes: Casting and Molding, Particulate Processing, Deformation Processes, Metal Removal. New York: Industrial Press Inc., 2009, pp. 325–346.
  30. Gülsah E., Bülent A., Özkan Gülsoy H. Injection molding of micro-porous titanium alloy with space holder technique. Rare Metals, 2011, no. 30, pp. 565–571.
  31. Yakovlev A.L., Nochovnaya N.A., Putyrskij S.V., Krohina V.A. Titanium-polymer laminated materials. Aviacionnye materialy i tehnologii, 2016, no. S2, pp. 56–62. DOI: 10.18577/2071-9140-2016-0-S2-56-62.
  32. Korotchenko A.Yu., Kovalevich E.V., Nuraliev N.F., Kutsy O.Ya. A device for the study of free casting shrinkage of alloys. Liteinoe proizvodstvo, 2020, no. 11, pp. 16–18.
  33. Korotchenko A.Yu., Khilkov D.E., Tverskoy M.V., Khilkova A.A. On the use of additive and hybrid technologies in foundry. Liteinoe proizvodstvo, 2019, no. 6, pp. 26–28.
  34. Kablov E.N., Kashapov O.S., Medvedev P.N., Pavlova T.V. Study of a α+β-titanium alloy based on a system of Ti–Al–Sn–Zr–Si–β-stabilizing alloying elements. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 30–37. DOI: 10.18577/2071-9140-2020-0-1-30-37.
  35. Kablov E.N. The dominant feature of the national technology initiative. Problems of accelerating the development of additive technologies in Russia. Metally Evrazii, 2017, no. 3, pp. 2–6.