Influence of phase structure polymeric filmformer on physical mechanical and water resistant properties of coatings

Kuznetsova V.A., Kurshev E.V., Silaeva A.A., Marchenko S.A.
Kuznetsova V.A., Kurshev E.V., Silaeva A.A., Marchenko S.A. Influence of phase structure polymeric filmformer on physical mechanical and water resistant properties of coatings // Proceedings of VIAM. 2021. No. 10. DOI: 10.18577/2307-6046-2021-0-10-87-96. URL: https://viam-works.ru/en/journal/2021/10/9
Keywords
phase structure, polymeric filmformer, adhesion, water absorption, physical mechanical properties.
Abstract

The phase structure, adhesion and physical mechanical properties, water resistance of varnish coatings on the basis of the modified and not modified epoxy filmformers, with organic silicon ammine «AСOT-2» and low-molecular «ПO-200» polyamide as curing agents. It is established that the process of structurization of unfilled epoxy compositions depends on each component of polymeric system. The received results of determination of adhesion, physical mechanical properties, water resistance correlate with results of researches of phase structure of the coatings received on the basis of modified and not modified epoxy compositions, with organic silicon ammine «AСOT-2» and low-molecular «ПO-200» polyamide as curing agents.

Reference list
  1. Kablov E.N. Aviation materials science: results and prospects. Vestnik Rossiyskoy akademii nauk, 2002, vol. 72, no. 1, pp. 3–12.
  2. Kablov E.N. The role of chemistry in the creation of new generation materials for complex technical systems. Reports of XX Mendeleev Congress on General and Applied Chemistry. Ekaterinburg: UB RAS, 2016, pp. 25–26.
  3. Zhitomirskiy G.I. Aircraft design. Moscow: Mashinostroyenie, 1991, 400 p.
  4. Kablov E.N., Startsev O.V., Medvedev I.M. Review of international experience on corrosion and corrosion protection. Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87.
  5. Lutsenko A.N., Slavin A.V., Erasov V.S., Khvackij K.K. Strength tests and researches of aviation materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 527–546. DOI: 10.18577/2071-9140-2017-0-S-527-546.
  6. Pavlyuk B.Ph. The main directions in the field of development of polymeric functional materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 388–392. DOI: 10.18577/2071-9140-2017-0-S-388-392.
  7. Chebotarevsky V.V., Kondrashov E.K. Technology of paint and varnish coatings in mechanical engineering. Moscow: Mashinostroyenie, 1978, 295 p.
  8. Semenova L.V., Nefedov N.I., Belova M.V., Laptev A.B. Systems of paint coatings for helicopter equipment. Aviacionnye materialy i tehnologii, 2017, no. 4 (49), pp. 56–61. DOI: 10.18577/2071-9140-2017-0-4-56-61.
  9. Kvasnikov M.Yu., Zamshin V.A., Kudlo V.L., Ilina N.S., Chinov V.V., Nepochatov V.M. New technology for production of electrophoretic coatings on the parts of a helicopter operating in fretting-corrosion conditions. Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 49–55. DOI: 10.18577 / 2071-9140-2019-0-4-49-55.
  10. Zheleznyak V.G. Modern paint and varnish materials for use in aviation equipment products. Trudy VIAM, 2019, no. 5 (77), paper no. 07. Available at: http://www.viam-works.ru. (accessed: January 18, 2021). DOI: 10.18577/2307-6046-2019-0-5-62-67.
  11. Yakovlev A.D., Yakovlev S.A. Functional paintwork. Saint Petersburg: Khimizdat, 2016, 272 p.
  12. Kochnova Z.A., Sorokin M.F., Zakharova A.A., Cherebylo I.A. Coatings with increased adhesion to anodized aluminum and its alloys. Lakokrasochnye pokrytiya i ikh primenenie, 1980, no. 4, pp. 32–34.
  13. Kondrashov E.K., Kuznetsova V.A., Semenova L.V., Lebedeva T.A., Malova N.E. Development of aviation paints and varnishes. Vse materialy. Entsiklopedicheskiy spravochnik, 2012, no. 5, pp. 49–54.
  14. Filichkina V.N. Current state and development trends in the production and consumption of epoxy resins. Moscow: NIITEKhIM, 1988, is. 8.18 p.
  15. Moshinsky L.Ya. Epoxy resins and hardeners (structure, properties, chemistry and topology of curing). Tel Aviv, 1995, 370 p.
  16. Mostovoy A.S., Panova L.G. Investigation of the possibility of using low molecular weight polyamide PO-300 as a "cold" hardener for epoxy oligomers. Plasticheskiye massy, 2016, no. 1–2, pp.16–18.
  17. Noskov A.M., Novikov N.I. Curing of glycidyl ethers with amines in the presence of hydroxyl groups. Zhurnal prikladnoy khimii, 2008, vol. LW, no. 12, pp. 2733–2737.
  18. Petrov G.N., Sinaisky A.G., Dalgren I.V. Liquid hydrocarbon rubbers and their areas of application. Klei. Germetiki. Tekhnologii, 2009, no. 10, PP. 24–27.
  19. Yulovskaya V.D. Oligomers. Rubber-oligomeric compositions, structure and properties: textbook. Moscow, 2008, 46 p.
  20. Chalykh A.E., Kochnova Z.A., Lark E.S. Compatibility and diffusion in epoxy oligomer – liquid carboxylate rubbers systems. Vysokomolekulyarnye soedineniya. Ser. A, 2001, vol. 43, no. 12, pp. 2147–2155.
  21. Kablov V.F. System technology of rubber-oligomeric compositions. Oligomers-2009. Moscow, 2009, pp. 162–191.
  22. Kondrashov E.K., Kuznetsova V.A., Semenova L.V., Lebedeva T.A. The main directions of improving the operational, technological and environmental characteristics of paint and varnish coatings for aviation technology. Rossiyskiy khimicheskiy zhurnal, 2010, vol. LIV, no. 1, pp. 96–102.
  23. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  24. Pyrikov A.V., Loiko D.P., Kochergin Yu.S. Modification of epoxy resins with liquid polysulfide and carboxylated butadiene rubbers. Klei. Germetiki. Tekhnologii, 2010, no. 1. P. 28–33.
  25. Kuznetsova V.A., Marchenko S.A., Zhelez-nyak V.G., Emelyanov V.V. Influence of the spatial structure of reinforcing fillers on the properties of the paint coatings. Trudy VIAM, 2020, no. 9 (91), paper no. 11. Available at: http://www.viam-works.ru (accessed: July 9, 2021). DOI: 10.18577/2307-6046-2020-0-9-96-104.