Effect of modification of cold cured epoxy adhesives with elastomers on the resource strength of adhesive joints

Isaev A.Yu., Pavlyuk B.Ph., Petrova A.P., Lukina N.F., Balabanova O.S.
Isaev A.Yu., Pavlyuk B.Ph., Petrova A.P., Lukina N.F., Balabanova O.S. Effect of modification of cold cured epoxy adhesives with elastomers on the resource strength of adhesive joints // Proceedings of VIAM. 2020. No. 9. DOI: 10.18577/2307-6046-2020-0-9-27-34. URL: https://viam-works.ru/en/journal/2020/9/3
Keywords
epoxy oligomer, rubber, adhesive joint, VK-9 adhesive, VK-27 adhesive, resource durability, thermal stability, elastic characteristics.
Abstract

Comparative data on characteristics of the adhesive joints executed by epoxy adhesive of cold curing VK-9 (not modified) and VK-27 (modified by rubber) are provided. It is shown that updating of epoxy adhesive of cold curing by rubber leads to increase of strength, deformation and resource characteristics of glued joints, however heat resistance of adhesive joints decreases. Comparison of properties of the adhesive joints executed by adhesives VK-9 and VK-27 is given, at influence of loadings, temperatures, humidity and other factors.

Reference list
  1. Kablov E.N., Chursova L.V., Babin A.N., Mukhametov R.R., Panina N.N. Developments of FSUE «VIAM» in the field of melt binders for polymer composite materials. Polimernye materialy i tekhnologii, 2016, vol. 2, no. 2, pp. 37–42.
  2. Grashhenkov D.V., Chursova L.V. Strategy of development of composite and functional materials. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 231–242.
  3. Lukina N.F., Petrova A.P., Muhametov R.R., Kogtjonkov A.S. New developments in the field of adhesive aviation materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 452–459. DOI: 10.18577/2071-9140-2017-0-S-452-459.
  4. Petrova G.N., Larionov S.A., Platonov M.M., Perfilova D.N. Thermoplastic materials of new generation for aviation. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 420–436. DOI: 10.18577/2071-9140-2017-0-S-420-436.
  5. Gladkikh S.N., Vyalov A.I., Shestakov A.S., Shorokhova D.V. Cold-curing structural adhesives with increased deformation resistance. Klei. Germetiki. Tekhnologii, 2013, no. 3, pp. 10–14.
  6. Pyrikov A.V., Loiko D.P., Kochergin Yu.S. Modification of epoxy resins with polysulfide and carboxylate butadiene rubbers. Klei. Germetiki. Tekhnologii, 2010, no. 1, pp. 28–33.
  7. Pyrikov A.V., Loiko D.P. Changes in the properties of epoxy polymers under the influence of liquid polysulfide and carboxylated butadiene rubbers. Remont, vosstanovleniye, modernizatsiya, 2008, no. 8, pp. 30–32.
  8. Bonding in mechanical engineering. Handbook in 2 volumes. Vol. 1. Ed. G.V. Malysheva. Moscow: Nauka i tekhnologiya, 2005, pp. 435–445.
  9. Kulik T.A., Kochergin Yu.S., Zaitsev Yu.S. et al. Influence of liquid rubbers on the physical and mechanical properties of epoxy polymers. Plasticheskiye massy, 1985, no. 4, pp. 25–26.
  10. Kablov E.N. New generation materials – the basis for innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  11. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  12. Kablov E.N., Chursova L.V., Lukina N.F., Kutsevich K.E., Rubtsova E.V., Petrova A.P. Investigation of epoxy-polysulfone polymer systems as the basis for high-strength adhesives for aviation purposes. Klei. Germetiki. Tekhnologii, 2017, no. 3, pp. 7–12.
  13. Aviation materials: handbook in 13 vols. Ed. E.N. Kablov. Moscow: VIAM, 2019, vol. 10: Adhesives, sealants, rubbers, hydraulic fluids, part 1: Adhesives, adhesive prepregs, 276 p.
  14. Kablov E.N., Minakov V.T., Anikhovskaya L.I. Adhesives and materials based on them for the repair of aircraft structures. Aviacionnye materialy i tehnologii. Moscow: VIAM, 2002, no. 1, pp. 61–65.
  15. Sharova I.A. Cold curing epoxy adhesives for bonding and repairing aircraft parts: thesis, Cand Sc. (Tech.). Moscow: VIAM, 2014, 127 p.
  16. Sharova I.A., Lukina N.F., Aleksashin V.M., Antyufeeva N.V. Influence of the composition of fast-curing epoxy adhesive compositions on their kinetic and strength properties. Klei. Germetiki. Tekhnologii, 2015, no. 2, pp. 2–7.
  17. Petrova A.P., Mukhametov R.R., Akhmadieva K.R. Internal stresses in cured polyester binders for polymer composites. Trudy VIAM, 2019, no. 5 (77), paper no. 02. Available at: http://www.viam-works.ru (accessed: June 16, 2020). DOI: 10.18577/2307-6046 -2019-0-5-12-21.
  18. Kurshubadze I.V., Petrova A.P. Efficiency of adhesive joints in marine subtropics. Klei. Germetiki. Tekhnologii, 2005, no. 12, pp. 14-17.
  19. Lobanov M.V., Gulyaev A.I., Babin A.N. Increasing the impact and crack resistance of epoxy thermosetting plastics and composites based on them with the help of thermoplastic additives as modifiers. Vysokomolekulyarnye soyedineniya, ser: B, 2016, vol. B8, no. 1, pp. 3–15.