Influence of the spatial structure of reinforcing fillers on the properties of the paint coatings
UDC
629.7.023.222
DOI
10.18577/2307-6046-2020-0-9-96-104
Article PDF (Russian)
(617.31 KB)
How to cite
Kuznetsova V.A., Marchenko S.A., Zheleznyak V.G., Emelyanov V.V. Influence of the spatial structure of reinforcing fillers on the properties of the paint coatings // Proceedings of VIAM. 2020. No. 9. DOI: 10.18577/2307-6046-2020-0-9-96-104. URL: https://viam-works.ru/en/journal/2020/9/11
Keywords
epoxy oligomer, reinforcing filler, filamentous crystals, paint coating, erosion resistance, adhesion, elasticity, water absorption.
Abstract
The influence of the spatial structure of reinforcing fillers, such as ZnO and BN filamentous crystals of zinc oxide, as well as their content in an epoxy-polyamide polymer matrix on adhesion, physical and mechanical properties, water absorption and erosion resistance, was studied. It is shown that coatings containing ZnO filamentous crystals in their composition, which are clear spatial tetrahedra of four single crystals emerging from a single center, have a higher elastic coating under tension, as well as resistance to erosion compared to similar coatings containing BN filamentous crystals with a needle-like structure.
Reference list
- Kablov E.N. Aviation materials science: results and prospects. Vestnik Rossiyskoy akademii nauk, 2002, vol. 72, no. 1, pp. 3-12.
- Zheleznyak V.G. Modern paint and varnish materials for use in aviation equipment products. Trudy VIAM, 2019, no. 5 (77), paper no. 07. Available at: http://www.viam-works.ru. (accessed: October 17, 2019). DOI: 10.18577/2307-6046-2019-0-5-62-67.
- History of Aviation Materials Science. VIAM – 80 years: years and people. Ed. E.N. Kablov. Moscow: VIAM, 2012, 520 p.
- Kablov E.N. The key problem is materials. Trends and guidelines for innovative development in Russia. Moscow: VIAM, 2015, pp. 458–464.
- Kondrashov E.K., Kuznetsova V.A., Semenova L.V., Lebedeva T.A. The main directions of improving the operational, technological and environmental characteristics of paint and varnish coatings for aviation technology. Rossiyskiy khimicheskiy zhurnal, 2010, vol. LIV, no. 1, pp. 96-102.
- Pavlyuk B.Ph. The main directions in the field of development of polymeric functional materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 388–392. DOI: 10.18577/2071-9140-2017-0-S-388-392.
- Semenova L.V., Nefedov N.I., Belova M.V., Laptev A.B. Systems of paint coatings for helicopter equipment. Aviacionnye materialy i tehnologii, 2017, no. 4 (49), pp. 56–61. DOI: 10.18577/2071-9140-2017-0-4-56-61.
- Kablov E.N. The role of chemistry in the creation of new generation materials for complex technical systems. Abstracts of the XX Mendeleev Congress on General and Applied Chemistry. Ekaterinburg: Ural Branch of the Russian Academy of Sciences, 2016. pp. 25–26.
- Ivanov A.A., Botvin V.V., Filimoshkin A.G. Adhesive strength of filled polyaluminosilicates on an aluminum surface. Zhurnal prikladnoy khimii, 2014, vol. 87, no. 2, pp. 158.
- Kondrashov E.K., Kuznetsova V.A., Semenova L.V., Lebedeva T.A., Malova N.Ye. Development of aviation paints and varnishes. Vse materialy. Entsiklopedicheskiy spravochnik, 2012, no. 5, pp. 49–54.
- Filichkina V.N. Current state and development trends in the production and consumption of epoxy resins. Khimicheskaya promyshlennost za rubezhom. Moscow: NIITEKhIM, 1988, is. 8, pp. 18.
- Moshinsky L.Ya. Epoxy resins and hardeners (structure, properties, chemistry and topology of curing). Tel Aviv: Arcadia Press Ltd, 1995, 370 p.
- Mostovoy A.S., Panova L.G. Investigation of the possibility of using low molecular weight polyamide PO-300 as a cold hardener for epoxy oligomers. Plasticheskiye massy, 2016, no. 1–2, pp. 16–18.
- Noskov A.M., Novikov N.I. Curing of glycidyl ethers with amines in the presence of hydroxyl groups. Zhurnal prikladnoy khimii, 2008, vol. 81, no. 12, pp. 2733–2737.
- Zinoviev V.E. To the question of the relationship between adhesion and the quality of the surface layer of the substrate of the adhesive joint. Vestnik RGUPS, 2010, no. 4, pp. 5–9.
- Pestov A.V., Puzyrev I.S., Mekhaev A.V., Gorbunova T.I., Saloutin V.I., Smirnov S.V., Vichuzhanin D.I., Matafonov P.P. Modification of adhesive materials based on epoxy oligomers with fluorine-containing organic compounds. Zhurnal prikladnoy khimii, 2014, vol. 87, no. 4, pp. 482.
- Lipatov Yu.S. Physical chemistry of filled polymers. Moscow: Khimiya, 1977, 603 p.
- Lipatov Yu.S., Sergeeva L.M. Adsorption of polymers. Kiev: Naukova Dumka, 1972, 196 p.
- Fabulyak F.G. Molecular mobility in surface layers. Kiev: Naukova Dumka, 1983, 144 p.
- Lipatov Yu.S. Interfacial phenomena in polymers. Kiev: Naukova Dumka, 1980, 260 p.
- Semenovich G.M., Lipatov Yu.S. The structure and properties of boundary layers of polymers. Physical chemistry of multicomponent polymer systems. Kiev: Naukova Dumka, 1986, vol. 1, pp. 186–221.
- Shishelova T.I., Stepanova N.E., Plynskaya D.A., Belyaeva M.A. Thread-like crystals. Uspekhi sovremennogo yestestvoznaniya, 2009, no. 8, pp. 12–13.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kuznetsova V.A., Kuznetsov G.V., Shapovalov G.G. Investigation of epoxy resin molecular mass influence by physiomechanical property and erosive resistant of coatings. Trudy VIAM, 2014, no. 8, paper no. 08. Available at: http://www.viam-works.ru (accessed: November 19, 2019). DOI: 10.18577/2307-6046-2014-0-8-8-8.
- Yakovlev A.D., Yakovlev S.A. Functional paintwork. Saint Petersburg: Khimizdat, 2016, 272 p.
- Kuznetsova V.A., Kondrashov E.K., Vladimirsky V.N. Prediction of erosion resistance of paint and varnish coatings taking into account dynamic parameters. Aviacionnye materialy i tehnologii, 2003, no. 2, pp. 50–53.
- Kuznetsova V.A., Kondrashov E.K., Semenova L.V., Kuznetsov G.V. On the influence of the shape of zinc oxide particles on the operational properties of polymer coatings. Materialovedeniye, 2012, no. 12, pp. 12–14.
- Kuznetsova V.A., Kondrashov E.K., Vladimirsky V.N., Kuznetsov G.V. Dispersed-reinforced erosion-resistant coatings. Aviacionnye materialy i tehnologii, 2003, is.: Paints and varnishes and coatings, pp. 53–56.
- Kuznetsova V.A., Deev I.S., Kuznetsov G.V., Kondrashov E.K. Influence of filler on fatigue strength and microstructure of free polymer films of coatings under cyclic tension. Zavodskaya laboratoriya, 2015, vol. 80, no. 5, pp. 35–39.