Low-molecular organosilicone rubbers in sealant compositions (review)

Gerasimov D.M., Ilyukhina M.A., Glazov P.A.
Gerasimov D.M., Ilyukhina M.A., Glazov P.A. Low-molecular organosilicone rubbers in sealant compositions (review) // Proceedings of VIAM. 2020. No. 8. DOI: 10.18577/2307-6046-2020-0-8-35-45. URL: https://viam-works.ru/en/journal/2020/8/4
Keywords
polymers, sealants, silicone composition, fluorosilicone sealant, polymer composition, low-molecular weight siloxane rubbers, compounds.
Abstract

Being based on a number of sources works on data and synthesis of survey information of the devoted history of development, the comparison of properties of domestic and foreign organosilicon sealant materials and application sealants made on the basis of low-molecular organosilicon and fluorosiloxane rubbers. Features of application of low-molecular weight siloxane rubbers are considered when manufacturing pressurizing materials. The comparative analysis sealants type of VICSINT, compounds and type of VGF.

Reference list
  1. Voronkov M.G., Mileshkevich V.P., Yuzhelevsky Yu.A. Silicone bond. Novosibirsk: Nauka, 1976, p. 12.
  2. Buznik V.M., Kablov E.N. Arctic materials science. Tomsk: Tomsk. State Un-t, 2018, is. 3, 44 p.
  3. Kablov E.N. Formation of domestic space materials science. Vestnik RFFI, 2017, no. 3, pp. 97–105.
  4. Kablov E.N., Semenova L.V., Petrova G.N., Larionov S.A., Perfilova D.N. Polymer composite materials on a thermoplastic matrix. Izvestiya vysshikh uchebnykh zavedeniy. Ser.: Khimiya i khimicheskaya tekhnologiya, 2016, vol. 59, no. 10, pp. 61–71.
  5. Andrianov K.A. Organosilicon polymer compounds. Moscow: GEI, 1946, 136 p.
  6. Bejder E.Ya., Petrova G.N. The thermoplastic binder for polymeric composite materials. Trudy VIAM, 2015, no. 11, paper no. 05. Available at: http://viam-works.ru. (accessed: May 28, 2020). DOI: 10.18577/2307-6046-2015-0-11-5-5.
  7. Bryk Ya.A., Eliseev O.A., Smirnov D.N. Corrosion protection of magnesium alloys polysulphide sealants. Trudy VIAM, 2017, no. 10 (58), paper no. 10. Available at: http://www.viam-works.ru (accessed: May 28, 2020). DOI: 10.18577/2307-6046-2017-0-10-10-10.
  8. Nanushyan S., Semenkova N., Trokhachenkova O., Polivanov A.N. Dispersiveness study of nanosize fillers in organosilicon environment. Conf. 5th European Silicon Days. Venna, 2009, pp. 168.
  9. Bryk Ya.A., Smirnov D.N. Research of frost resistance of aeronautical sealants. Trudy VIAM, 2018, no. 1 (61), paper no. 09. Available at: http://www.viam-works.ru (accessed: May 28, 2020). DOI: 10.18577/2307-6046-2018-0-1-9-9.
  10. Krasnov L.L., Kirina ZV, Venediktova M.A., Bryk Ya.A. Approbation of tape sealant for sealing removable constructive elements operable at temperatures from -60 to +180 °С. Trudy VIAM, 2019, no. 3 (75), paper no. 06. Available at: http://www.viam-works.ru (accessed: May 28, 2020). DOI: 10.18577/2307-6046-2019-0-3-53-60.
  11. Nanushyan S.R. Organosilicon materials of accelerated vulcanization: the history of the creation and development of the direction. Khimicheskaya promyshlennost segodnya, 2015, no. 11, pp. 21.
  12. Semenkova N., Nanushyan S., Polivanov A., Storozhenko P. Divinilpolydiorganosiloxane based composites with nanodispersed fillers. Conf. 5th European Silicon Days. Venna, 2009, pp. 191.
  13. Semenkova N., Nanushyan S., Storozhenko P. et al. Protective insulating Coatings Based on Siloxanes and Submicro- and Nano-Size Fillers. 17th International Symposium on Silicon Chemistry. Berlin, 2014, pp. 236.
  14. Savenkova A.V., Tikhonova I.V., Trebukova E.D. Heat and frost-resistant sealants. Aviation materials at the turn of the XX–XXI centuries. Moscow: VIAM, 1994, pp. 432–439.
  15. Petrova A.P., Donskoy A.A., Chalykh A.E., Shcherbina A.A. Adhesive materials. Sealants: reference book. Saint Petersburg: Professional, 2008, 589 p.
  16. Nikitina A.N., Nightingale V.V. Fuel-resistant sealants. Aviation materials at the turn of the XX–XXI centuries. Moscow: VIAM, 1994, pp. 374–378.
  17. Severny V.V., Minasyan R.M., Makarenko I.A., Biryuzova N.M. Mechanism of «cold» curing of low-molecular polyorgansiloxan rubbers. High molecular weight compounds. Ser.: A. 1976, vol. 18, pp. 1276–1281.
  18. Low-viscosity siloxane composition: pat. 2356117 Rus. Federation; fied 20.06.07; publ. 20.05.09.
  19. Minakov V.T., Savenkova A.V., Donskoy A.A. Organosilicon sealants. Rossiyskiye polimernye novosti, 2003, vol. 8, no. 4, pp. 37–41.
  20. Kornev A.E., Bukanov A.M., Sheverdyaev O.N. Elastomeric materials technology. Moscow: Publ. House Mosk. State Open University, 2000, pp. 64–72.
  21. Khairullin I.K., Pomanskaya M.P., Serebrennikova N.D. and others. New domestic one-pack sealants for installation of main blocks with double-glazed windows. Klei. Germetiki. Tekhnologii, 2006, no. 6, pp. 34–38.
  22. Zaglyadova S.V., Lyusova L.R., Glagolev V.A. et al. Rubber-bitumen sealing mastics. Klei. Germetiki. Tekhnologii, 2005, no. 10, pp. 24–26.
  23. Kablov E.N. Materials for «Buran» spaceship – innovative solutions of formation of the sixth technological mode. Aviacionnye materialy i tehnologii, 2013, no. S1, pp. 3–9.
  24. Kablov E.N. Materials and chemical technologies for aviation technology. Vestnik Rossiyskoy akademii nauk, 2012, vol. 82, no. 6, pp. 520–530.
  25. Khakimullin Yu.N., Gubaidullin L.Yu. Modern approaches to the production of curing sealants. Second Kirpichnikov Readings: plenary reports. Kazan, 2001, pp. 63–68.
  26. Gerasimov D.M., Ilyukhina M.A., Glazov P.A. Features of the use of low-molecular organosilicon rubbers in sealing compositions. All-Russian Scientific and Technical Conf. «Fundamental applied research in the field of sealing, sealing and fire and heat protection materials». Moscow, 2019, pp. 45.
  27. Aronovich D.A., Murokh A.F., Sineokov A.L. Heat-resistant anaerobic sealants and adhesives. Plasticheskiye massy, 2006, no. 6, pp. 37–41.
  28. Mezhikovsky S.M., Irzhak V.I. Chemical physics of oligomer curing. Moscow: Nauka, 2008, 269 p.