The approaches that are used for developed of optimal strain modes of aluminum-lithium alloys (review)

Shchetinina N.D., Rudchenko A.S., Selivanov A.A.
Shchetinina N.D., Rudchenko A.S., Selivanov A.A. The approaches that are used for developed of optimal strain modes of aluminum-lithium alloys (review) // Proceedings of VIAM. 2020. No. 8. DOI: 10.18577/2307-6046-2020-0-8-20-34. URL: https://viam-works.ru/en/journal/2020/8/3
Keywords
aluminum-lithium alloys, hot deformation, Zener–Hollomon parameter, Arrhenius model, dynamic model of materials, processing maps.
Abstract

Рrovides a review of publications in the field of the research of aluminum-lithium alloys deformation processes, which are used in the construction of aircraft and space technology products. The review summarizes the research that are devoted to the influence of parameters of pressure treatment on structure formation processes in aluminum-lithium alloys and the mathematical modeling as applied to hot deformation processes. The article discusses the approaches that are used by researchers in the development of optimal deformation modes of aluminum-lithium alloys.

Reference list
  1. Kablov E.N., Lukin V.I., Antipov V.V., Ioda E.N., Panteleev M.D., Skupov A.A. Efficiency of the use of filler materials in laser welding of high-strength aluminum-lithium alloys. Svarochnoye proizvodstvo, 2016, no. 10, pp. 17–21.
  2. Grigorenko I.B., Zhegina I.P., Fomina M.A., Kablov E.N., Morozova L.V. Investigation of the influence of a corrosive environment on the process of damage accumulation and the nature of destruction of structural aluminum alloys 1441 and B-1469 during tensile tests and low-cycle fatigue. Nauka i tekhnologii, 2017, no. 1, pp. 41–48.
  3. Annin B.D., Fomin V.M., Karpov E.V., Malikov A.G., Orishich A.M. Complex research of laser welding of high-strength alloy V-1469. Aviacionnye materialy i tehnologii, 2016, no. 3 (42), pp. 9–16. DOI: 10.18577/2071-9140-2016-0-3-9-16.
  4. Antipov V.V., Klochkova Yu.Yu., Romanenko V.A. Modern aluminum and aluminum-lithium alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 195–211. DOI: 10.18577/2107-9140-2017-0-S-195-211.
  5. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  6. Knyazev M.I., Betzofen S.Ya., Antipov V.V. Alloys of the Al – Cu – Li and Al – Mg – Li systems: phase composition, texture and anisotropy of mechanical properties (review). Deformatsiya i razrusheniye materialov, 2015, no. 11, pp. 10-26.
  7. Klochkov G.G., Grushko O.E., Klochkova Ju.Ju., Romanenko V.A. Industrial development of strength alloy V-1469 of Al–Cu–Li–Mg. Trudy VIAM, 2014, no. 7, paper no. 01. Available at: http://viam-works.ru (accessed: February 17, 2020). DOI: 10.18577/2307-6046-2014-0-7-1-1.
  8. Oglodkov M.S., Klochkova Yu.Yu., Kolobnev N.I., Khokhlatova L.B. High-strength alloys of the Al – Cu – Li system with increased fracture toughness for aircraft structures. Tsvetnye metally, 2013, no. 9, pp. 66–70.
  9. Oglodkov M.S., Filatov A.A., Popova Yu.A., Khokhlatova L.B., Kolobnev N.I. Prospects for the use of low-density high-strength alloy V-1461 plates in aircraft structures. Vse materialy. Entsiklopedicheskiy spravochnik, 2014, no. 2, pp. 16–22.
  10. Kolobnev N.I. History of development, phase composition and properties of alloys of the Al – Cu – Li system. Tekhnologiya legkikh splavov, 2015, no. 2, pp. 46–52.
  11. Oglodkov M.S., Erisov Ya.A., Grechnikov F.V. Influence of modes of making sheets from alloy V-1461 on crystallography of structure and anisotropy of properties. Izvestiya vuzov. Tsvetnaya metallurgiya, 2015, no. 6, pp. 36–42.
  12. Liu M., Hu Y., Chen Y. et al. Analysis of empirical relation between microstructure, texture evolution and fatigue properties of an Al–Cu–Li alloy during different pre deformation processes. Materials Science and Engineering: A, 2018, vol. 72, pp. 309–319.
  13. Zhou J., Dang L., Xiao W. et al. Influence of process parameters on deep drawing of 2060 Al–Li alloy under hot stamping process. Journal of Lightweight Materials and Manufacture, 2019, vol. 3, no. 1, pp. 36–42.
  14. Guo X., Zhang S., Ma Y. et al. Strengthening mechanisms, deformation behavior, and anisotropic mechanical properties of Al–Li alloys: a review. Journal of Advanced Research, 2018, vol. 10, pp. 49–67.
  15. Khokhlatova L.B., Oglodkov M.S., Kolobnev N.I., Setiukov O.A. Influence of crystallographic orientations on the properties of plates made of Al–Li alloys B-1461 and 1424. Tekhnologiya legkikh splavov, 2010, no. 1, pp. 100–106.
  16. Knyazev M.I., Oglodkov M.S., Betzofen S.Ya., Antipov V.V. Study of the effect of heat treatment on the phase composition, texture and mechanical properties of the alloy В-1461 systems Al – Cu – Li. Metally, 2015, no. 6, pp. 77–84.
  17. Crooks R.E., Pagan D.C., Tayon W.A., Nygren K.E. In-situ study of planar slip in a commercial aluminum-lithium alloy using high energy x-ray diffraction microscopy. Acta Materialia, 2019, vol. 173, pp. 231–241.
  18. Ponchivalov Yu.I., Panin S.V., Kolobnev N.I., Panin V.E., Kablov E.N. Influence of nanostructuring of the surface layer of aluminum-lithium alloy 1424 on deformation mechanisms, technological characteristics and fatigue life, increasing plasticity and technological characteristics. Fizicheskaya mezomekhanika, 2012, no. 6, pp. 107-111.
  19. Li J.F., Chen Y.L., Zhang X.-H. et al. Flow curve correction and processing map of 2050 Al–Li alloy. Transactions of Nonferrous Metals Society of China, 2018, vol. 28, pp. 404–414.
  20. Nie Y., Jian H., Ou L., Zheng Z. Hot deformation behavior of 2060 alloy. Journal of Alloys and Compounds, 2015, vol. 648, pp. 681–689.
  21. Krishtal M.M. Instability and mesoscopic heterogeneity of plastic deformation (analytical review). Part 1. Fizicheskaya mezomekhanika, 2004, no. 7, pp. 5–29.
  22. Kolupaeva S.N., Popov L.E., Starenchenko V.A. Instabilities of plastic deformation of crystals and the formation of dislocation defect structures. Matematicheskoye modelirovaniye sistem i protsessov, 1995, no. 3, pp. 77–87.
  23. Milevskaya T.V., Ruschits S.V., Tkachenko E.A., Antonov S.M. Deformation behavior of high-strength aluminum alloys in conditions of hot deformation. Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 3–9. DOI: 10.18577/2071-9140-2015-0-2-3-9.
  24. Rajput S.K., Nath S.K., Kumar N., Kumar S. Modelling of flow stress and prediction of workability by processing map for hot compression of 43CrNi steel. ISIJ International, 2017, vol. 573, pp. 497–505.
  25. Saha P. Aluminum extrusion technology. ASM International, 2000, pp. 25.
  26. Soboyejo W.O. Mechanical properties of engineered materials. Marcel Dekker, 2003, pp. 222–228.
  27. Hernandez C.A., Medina S.F. General expression of the Zener-Hollomon parameter as a function of the chemical composition of low alloy and microalloyed steels. Acta Materialia, 1996, vol. 44, pp. 137–148.
  28. Smirnov M.A., Akhmedyanov A.M., Ruschits S.V. Physical and mathematical modeling of hot deformation of steel 20X13. Vestnik YUUrGU, 2013, no. 13, pp. 116-124.
  29. Jonas J.J., Laasraoui A. Prediction of steel flow stresses at high temperatures and strain rates. Metallurgical transactions A, 1991, vol. 22, pp. 1545–1558.
  30. Singh S.B., Pal S.K. Computational Methods and Production Engineering, chapter Finite element modeling of hot rolling: Steady- and unsteady-state analyses. Mechanical Engineering Series, 2017, pp. 83–124.
  31. Nourani M., Sajadifar S.V., Ketabchi M. Modeling of mechanical characteristics in hot deformation of 4130 steel. Transactions of the Metallurgical Society of AIME, 2011, vol. 82, pp. 934–939.
  32. Li C., Wan M., Meng B., Du Z. Constitutive behavior and microstructural evolution in hot deformed 2297 Al–Li alloy. Chinese Journal of Aeronautics, 2019, vol. 11, pp. 77–87.
  33. Luo A., Miao J., Sutton S. Microstructure and hot deformation behavior of a new aluminum–lithium–copper based aa2070 alloy. Materials Science Engineering, 2020, vol. A777, pp. 2–14.
  34. Murty N.S.V.S., Jha A.K., Pant B. et al. Microstructure and micro-texture evolution during large strain deformation of an aluminium–copper–lithium alloy aa2195. Materials and Design, 2015, vol. 65, pp. 862–868.
  35. Du R., Zhao M., Wang Z. et al. Characteristic constitution model and microstructure of an Al–3.5C–1.5Li alloy subjected to thermal deformation. Materials Characterization, 2018, vol. 145, pp. 53–64.
  36. Chhangani S., Prakash A., Prasad M.J.N.V. et al. Effect of temperature and strain rate on hot deformation behavior and microstructure of Al–Cu–Li alloy. Journal of Alloys and Compounds, 2017, vol. 723, pp. 548–558.
  37. Li G.-A., Wang X.-M., Sun J. et al. Effects of coarse Al2CuLi phase on the hot deformation behavior of Al–Li alloy. Journal of Alloys and Compounds, 2020, vol. 815, pp. 77–87.
  38. Uvira J.J., Jonas J.L. Hot compression of ARMCO iron and silicon steel. Transactions of the Metallurgical Society of AIME, 1969, vol. 242, pp. 1619–1626.
  39. Antonov S.M., Akhmedyanov A.M., Ruschits S.V. Investigation of the deformation behavior of 20Kh13 steel under hot upsetting conditions. Vestnik YUUrGU, 2012, no. 19, pp. 89–93.
  40. Doraivelu S.M., Malas J.C., Morgan J.T. et al. Modeling of dynamic material behavior in hot deformation: Forging of Ti-6242. Metallurgical transactions A, 1984, vol. 15A, pp. 1883–1892.
  41. Seshacharyulu T., Prasad Y.V.R.K. Processing maps for hot working of titanium alloys. Materials Science and Engineering, 1998, vol. A243, pp. 82–88.
  42. Vargasov N.R., Rybin V.V. Optimization of temperature and rate regimes of plastic deformation by the criterion of dissipation of mechanical energy. Metal Science and Heat Treatment, 1999, vol. 41, pp. 9–10.
  43. Feng Z., Lu Z., Zhu C. et al. Hot deformation characterization of as-homogenized Al–Cu–Li X2A66 alloy through processing maps and microstructural evolution. Journal of Materials Science Technology, 2019, vol. 35, pp. 2409–2421.
  44. Nemets A.M., Khlusova E.I., Barakhtin B.K., Vargasov N.R. The choice of modes of thermo-mechanical treatment of steels and alloys based on system analysis of the structure and simulation. Materials Physics and Mechanics, 2011, no. 12, pp. 30–42.
  45. Li J., Xiang S., Chen Y. et al. Dynamic restoration mechanism and physically based constitutive model of 2050 Al–Li alloy during hot compression. Journal of Alloys and Compounds, 2015, vol. 650, pp. 75–85.
  46. Song M., Liang X., Guo F. et al. Hot deformation behavior and microstructural evolution of Ag-containing 2519 aluminum alloy. Materials and Design, 2010, vol. 31, pp. 2171–2176.
  47. Liu G., Sun L., Chen L. et al. Microstructure evolution and mechanical properties of 2196 Al–Li alloy in hot extrusion process. Journal of Materials Processing Technology, 2020, vol. 275, pp. 2–14.
  48. Kokovikhin E.A., Salikhyanov D.R., Dvoynikov D.A. et al. Determining the plastic strain resistance of metallic materials on an automated plastometric complex. Diagnostics, Resource and Mechanics of materials and structures, 2015, vol. 2, pp. 24–43.
  49. Galkin A.M., Polukhin P.I., Gun G.Ya. Resistance to plastic deformation of metals and alloys: reference book. Moscow: Metallurgiya, 1983, pp. 82–88.
  50. Stefani N., Blackwell P., Bylya O., Gomez-Gallegos A. Al–Li alloys – the industrial analysis hot of material during forging behavior during industrial hot forging. Procedia Engineering, 2017, vol. 207, pp. 7–12.
  51. Liu J., Li C., Li Z. et al. Hot stamping of an Al–Li alloy: a feasibility study. Manufacturing Review, 2016, vol. 9, pp. 2–5.