Fractographic study of bearing steel fracture

Yakovlev N.O., Sedov O.V., Gulina I.V., Grinevich A.V.
Yakovlev N.O., Sedov O.V., Gulina I.V., Grinevich A.V. Fractographic study of bearing steel fracture // Proceedings of VIAM. 2020. No. 2. DOI: 10.18577/2307-6046-2020-0-2-91-100. URL: https://viam-works.ru/en/journal/2020/2/10
Keywords
spallation, fractography, double fracture, fracture surface, tension, stress-strain state.
Abstract

The article is devoted to the fractographic study of double fracture surfaces during standard tensile tests of samples of ball-bearing steel developed by FSUE VIAM. Double destruction occurred simultaneously either in two fillets, or in the working part of the sample with the formation of a thin plate. Such an unexpected failure was never realized when testing structural alloys with ultimate strength characteristics. A hypothesis was put forward about possible destruction by the spallation mechanism, but the version of multiple destruction was not rejected either. The fractographic analysis of the surface of fractures with high reliability confirms the hypothesis of spall fracture.

Reference list
  1. Zaitsev A.M., Korostashevsky R.V. Operation of aircraft rolling bearings. Moscow: Transport, 1968, 222 p.
  2. Korostashevsky R.V., Zaitsev A.M. Aircraft rolling bearings. Moscow: Oborongiz, 1963, 340 p.
  3. Conter L.Ya. Steel for heat-resistant bearings (overview). Moscow: NIINAutoprom, 1978, ser.: XII, 78 p.
  4. Gromov V.I., Voznesenskaya N.M., Pokrovskaya N.G., Tonysheva O.A. High-strength constructional and corrosion-resistant steels developed by VIAM for aviation engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 159–174. DOI: 10.18577/2071-9140-2017-0-S-159-174.
  5. Metallurgy and heat treatment of steel and cast iron: reference book / ed. N.T. Gudtsova. Moscow: State sc. and techn. publ. house lit. by black and color metal., 1956, pp. 821–828.
  6. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  7. Kablov E.N. Trends and guidelines for the innovative development of Russia: collection scientific-inform. materials. 3rd ed. Moscow: VIAM, 2015, 720 p.
  8. Krylov S.A., Markova E.S., Shcherbakov A.I., Yakusheva N.A. Metallurgical features of smelting process of high-strength maraging steel VKS180-ID microalloyed by REM. Aviacionnye materialy i tehnologii, 2015, no. 4 (37), pp. 14–20. DOI: 10.18577/2071-9140-2015-0-4-14-20.
  9. Kablov E.N. Structural and functional materials are the basis of the economic, scientific and technological development of Russia. Voprosy materialovedeniya, 2006, no. 1, pp. 64–67.
  10. Kablov E.N. Without new materials, there is no future. Metallurg, 2013, no. 12, pp. 4-8.
  11. Gromov V.I., Kurpyakova N.A., Korobova E.N., Sedov O.V. New heat resistant steel for aircraft bearings. Trudy VIAM, 2019, no. 2 (74), paper no. 02. Available at: http://www.viam-works.ru (accessed: November 22, 2019). DOI: 10.18577/2307-6046-2019-0-2-17-23.
  12. Gulina I.V., Sedov O.V., Yakovlev N.O., Grinevich A.V. Features of the tested bearing steel. Trudy VIAM, 2019, no. 10 (82), paper no. 07. Available at: http://www/viam-works.ru (accessed: November 22, 2019). DOI: 10.18577/2307-6046-2019-0-10-76-83.
  13. Kola G., Raider D. Waves of stress and destruction. Destruction. Moscow: Mir, 1973, vol. 1, pp. 570-608.
  14. Nicholas T. Elastoplastic stress waves. Impact dynamics. Moscow: Mir, 1985, 296 p.
  15. Novikov S.A. The destruction of materials when exposed to intense shock loads. Sorovskiy obrazovatelnyj zhurnal, 1999, no. 8, pp. 116–121.
  16. Smirnov I.V., Utkin A.A. Spall fracture effects in the nanosecond range of exposure durations. Vestnik Nizhegorod. un-ta im. N.I. Lobachevskogo, 2011, no. 4, pp. 1776–1777.