Investigation of impact of vacuum heat treatment on thermophysical properties of composite material of Al–SiC system with high content of reinforcing phase

Nyafkin A.N., Shavnev A.A., Serpova V.M., Razmakhov M.G., Pahomkin S.I.
Nyafkin A.N., Shavnev A.A., Serpova V.M., Razmakhov M.G., Pahomkin S.I. Investigation of impact of vacuum heat treatment on thermophysical properties of composite material of Al–SiC system with high content of reinforcing phase // Proceedings of VIAM. 2020. No. 11. DOI: 10.18577/2307-6046-2020-0-11-60-67. URL: https://viam-works.ru/en/journal/2020/11/7
Keywords
highly filled metal composite material, hot pressing of powders, powders of aluminium alloy, silicon carbide, temperature coefficient of linear expansion, thermal conductivity.
Abstract

The results of investigation of thermal treatment influence on thermophysical properties of metal composite material (MCM) based on aluminium casting alloy АК9ч (АЛ4) grade of Al–Si–Mg system reinforced with silicon carbide particles with content of reinforcing particles of 69±1% (volume) are given. MCM is made by solid-phase method followed by vacuum annealing. There are also presented studies of thermophysical characteristics of the material: thermal conductivity, temperature coefficient of linear expansion in the temperature range from 20 to 400 °C and density. It is shown that thermophysical characteristics depend on structural characteristics of the material.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Composites: Today and Tomorrow. Metally of Evrazii, 2015, no. 1, pp. 36–39.
  3. Kablov E.N., Chibirkin V.V., Vdovin S.M. Manufacturing, properties and application of heat-conducting bases from MMK Al–SiC in power electronics and converting equipment. Aviacionnye materialy i tehnologii, 2012, no. 2, pp. 20–23.
  4. Nyafkin AN, Loshchinin Yu.V., Kurbatkina EI, Kosolapov DV. Investigation of the influence of the fractional composition of silicon carbide on the thermal conductivity of a composite material based on an aluminum alloy. Trudy VIAM, 2019, no. 11 (83), paper no. 06. Available at: http://www.viam-works.ru (accessed: July 30, 2020). DOI: 10.18577/2307-6046-2019-0-11-53-59.
  5. Berezhnoy V.L. Technological principles of maximizing strength in the case of production of press quenched Al–Mg–Si alloy extrusions. Light Metal Age, 2000, vol. 58, no. 5-6, pp. 46–53.
  6. Igarashi T. Characteristics of the flow around a square prism. Bulletin of Journal Series C Me-chanical Systems, 1984, vol. 27, is. 231, pp. 1858–1865. DOI: 10.1299/jsme1958.27.1858.
  7. Crowe C.R., Hasson D.F. Strength Metals and Alloys. Proceedings of the 6th International Conference on Industrial Engineering, 1982, vol. 2, pp. 859–862.
  8. State Standard 8.777–2011. State system for ensuring the uniformity of measurements (GSI). Disperse composition of aerosols and suspensions. Determination of particle size by diffraction of laser radiation. Moscow: Standartinform, 2019, 8 p.
  9. State Standard 22309–2015 (ISO 22309–2011). State system for ensuring uniformity of measurements. Electron probe microanalysis. Quantitative analysis using energy dispersive spectrometry for elements with atomic number 11 (Na) and above. Moscow: Standartinform, 2015, 19 p.
  10. State Standard 18898–89 (ISO 2738–87). Powder products. Methods for determining density, oil content and porosity. Moscow: Publishing house of standards, 1990, 10 p.
  11. ASTM E 1461-01. Standard test method for thermal diffusivity of solids by the flash method. 2001, pp. 1–13. DOI: 10.1520/E1461-01.
  12. Xue J., Taylor R. An evaluation of specific heat measurement methods using the laser flash technique. International Journal of Thermophysics, 1993, vol. 14, vol. 2, pp. 313–320.
  13. State Service Standard Reference Data 65–84. Corundum is synthetic. Isobaric heat capacity in the temperature range 4–2300 K. Moscow: Publishing house of standards, 1985, 6 p.
  14. ASTM E228. Standard test method for linear thermal expansion of solid materials with a push-rod dilatometer. 2017, pp. 1–10. DOI: 10.1520/E0228-17.
  15. ASTM E831. Standard test method for linear thermal expansion of solid materials by thermo-mechanical analysis. 2019, pp. 1–5. DOI: 10.1520/E0831-19.
  16. Parker W.J., Jenkins R.J., Butler C.P., Abbott G.L. Rash method of determining thermal diffu-sivity, heat capacity and thermal conductivity. Journal of Applied Physics, 1961, no. 32, pp. 1679–1684.
  17. Nyafkin A.N., Shavnev A.A., Kurbatkina E.I., Kosolapov D.V. Studying the effect of silicon carbide particle size on the thermal coefficient linear expansion of the composite material based on aluminum alloy. Trudy VIAM, 2020, no. 2 (86), paper no. 05. Available at: http://www.viam-works.ru (accessed: August 05, 2020). DOI: 10.18577/2307-6046-2020-0-2-41-49.
  18. Ogorodov D.V., Trapeznikov A.V., Popov D.A., Pentyukhin S.I. The development of casting heat-resistant aluminum alloys (To the 120th anniversary since the birth of I.F. Kolobnev). Trudy VIAM, 2017, no. 2 (50), paper no. 12. Available at: http://www.viam-works.ru (accessed: August 06, 2020). DOI: 10.18577/2307-6046-2017-0-2-12-12.