Silicon nitride ceramic materials for aviation GTE bearings and methods of manufacturing (review)

Belyachenkov I.O., Shchegoleva N.E., Chaynikova A.S., Vaganova M.L., Shavnev A.A.
Belyachenkov I.O., Shchegoleva N.E., Chaynikova A.S., Vaganova M.L., Shavnev A.A. Silicon nitride ceramic materials for aviation GTE bearings and methods of manufacturing (review) // Proceedings of VIAM. 2019. No. 7. DOI: 10.18577/2307-6046-2019-0-7-42-49. URL: https://viam-works.ru/en/journal/2019/7/5
Keywords
gas turbine engines, rolling bearings, hybrid bearings, ceramics, silicon nitride, dry lubricants.
Abstract

Considered materials applicable to the creation of bearings of aircraft gas turbine engines (GTE). The advantages of using ceramic materials are shown in comparison with traditional steels and alloys. The methods of obtaining ceramic materials based on silicon nitride are considered. The prospects of creating high-temperature wear-resistant ceramic materials based on silicon nitride for tribological purposes are shown. The data on the development of silicon nitride ceramics with dry lubricants are given.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Grashchenkov D.V., Shchegoleva N.E., Orlova L.A., Suzdaltsev E.I. Radioprozrachnaya steklokeramika na osnove strontsiyalyumosilikatnogo stekla [Radiotransparent glass ceramics based on strontium-aluminosilicate glass] // Ogneupory i tekhnicheskaya keramika. 2016. №6. S. 31–38.
  3. Sevastyanov V.G., Simonenko E.P., Simonenko N.P., Grashchenkov D.V., Solntsev S.St., Ermakova G.V, Prokopchenko G.M., Kablov E.N., Kuznetsov N.T. Polucheniye nitevidnykh kristallov karbida kremniya s primeneniyem zol-gel metoda v obeme SiC-keramiki [Preparation of whiskers of silicon carbide using the sol-gel method in the bulk of SiC ceramics] // Kompozity i nanostruktury. 2014. T. 6. №4. S. 198–211.
  4. Kablov E.N., Zhestkov B.E., Grashchenkov D.V., Sorokin O.Yu., Lebedeva Yu.E., Vaganova M.L. Issledovaniye okislitelnoy stoykosti vysokotemperaturnogo pokrytiya na SiC-materiale pod vozdeystviyem vysokoental'piynogo potoka [Investigation of the oxidative resistance of a high-temperature coating on a SiC material under the influence of a high-enthalpy flow] // Teplofizika vysokikh temperatur. 2017. T. 55. №6. S. 704–711.
  5. Evdokimov S.A., Shchegoleva N.E., Sorokin O.Yu. Keramicheskiye materialy v aviatsionnom dvigatelestroyenii (obzor) [Ceramic materials in aviation engineering (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2018. №12 (72). St. 06. Available at: http://www.viam-works.ru (accessed: March 10, 2019). DOI: 10.18577/2307-6046-2018-0-12-54-61.
  6. Inozemtsev A.A., Sandratskiy V.L. Gazoturbinnyye dvigateli [Gas turbine engines]. Per: Aviadvigatel, 2006. S. 278–280.
  7. Gromov V.I., Kurpyakova N.A., Korobova E.N., Sedov O.V. Novaya teplostoykaya stal dlya aviatsionnykh podshipnikov [New heat resistant steel for aircraft bearings] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2019. №2 (74). St. 02. Available at: http://www.viam-works.ru (accessed: March 10, 2019). DOI: 10.18577/2307-6046-2019-0-2-17-23.
  8. Kulagina G.S., Zhelezina G.F., Levakova N.M. Antifriktsionnyye organoplastiki dlya vysokonagruzhennykh uzlov treniya [Antifriction organoplastics for high-loaded friction knots] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2019. №2 (74). St. 09. Available at: http://www.viam-works.ru (accessed: March 10, 2019). DOI: 10.18577/2307-6046-2019-0-2-89-96.
  9. Makarchuk V.V. Strategiya razvitiya metodov rascheta i konstruirovaniya vysokoskorostnykh podshipnikov aerokosmicheskogo primeneniya [Strategy of development of methods of calculation and designing of high speed bearings of space application] // Aviatsionnaya i raketno-kosmicheskaya tekhnika. 2009. №3 (19). S. 361–365.
  10. Shevchenko V.Ya. Vvedeniye v tekhnicheskuyu keramiku [Introduction to technical ceramics]. M.: Nauka, 1993. 112 s.
  11. Kritskiy V.Yu., Zubko A.I. Issledovaniye vozmozhnosti ispolzovaniya keramicheskikh aviatsionnykh podshipnikov skolzheniya novogo pokoleniya v konstruktsiyakh opor rotorov gazoturbinnykh dvigateley [Study of the possibility of using a new generation of ceramic aviation bearings in the construction of the supports of the rotors of gas turbine engines] // Dvigatel. 2013. №3. S. 24–26.
  12. Pallini R.A. Turbine engine bearings for ultra-high temperatures // SKF Ball Bearing Journal. 1989. Vol. 234. P. 12–15.
  13. Specialty Products Catalog // The Barden Corporation [Электронный ресурс]. Available at: http://www.bardenbearings.com (accessed: March 10, 2019).
  14. Petzow G., Herrmann M. Silicon nitride ceramics // High performance non-oxide ceramics II. Berlin, Heidelberg: Springer, 2002. Р. 47–167.
  15. Andriyevskiy R.A. Nitrid kremniya – sintez i svoystva [Silicon nitride – synthesis and properties] // Uspekhi khimii. 1995. T. 64. №4. S. 311–329.
  16. Liu X.J., Huang Z.Y., Ge Q.M. et al. Microstructure and mechanical properties of silicon nitride ceramics prepared by pressureless sintering with MgO–Al2O3–SiO2 as sintering additive // Journal of the European Ceramic Society. 2005. Vol. 25. No. 14. Р. 3353–3359.
  17. Tatarko P., Kašiarová M., Dusza J. et al. Wear resistance of hot-pressed Si3N4/SiC micro/nanocomposites sintered with rare-earth oxide additives // Wear. 2010. Vol. 269. No. 11. P. 867–874.
  18. Herrmann M., Shen Z., Schulz I. et al. Silicon nitride nanoceramics densified by dynamic grain sliding // Journal of Materials Research. 2010. Vol. 25. No. 12. P. 2354–2361.
  19. Bal B.S., Rahaman M. The rationale for silicon nitride bearings in orthopaedic applications // Advances in Ceramics-Electric and Magnetic Ceramics, Bioceramics, Ceramics and Environment. IntechOpen, 2011. P. 421–432.
  20. Perevislov S.N. Mekhanizm zhidkofaznogo spekaniya karbida i nitrida kremniya s oksidnymi aktiviruyushchimi dobavkami [The mechanism of liquid-phase sintering of silicon carbide and nitride with oxide activating additives] // Steklo i keramika. 2013. №7. S. 34–38.
  21. Lysenkov A.S. Konstruktsionnaya keramika na osnove nitrida kremniya s dobavkoy alyuminatov kaltsiya: dis. … kand. tekhn. Nauk [Structural ceramics based on silicon nitride with the addition of calcium aluminates: thesis, Cand. Sc. (Tech.)]. M., 2014. 139 s.
  22. Bolsunovskaya T.A., Efimochkin I.Yu., Sevostyanov N.V., Burkovskaya N.P. Vliyaniye marki grafita v kachestve tverdoy smazki na tribotekhnicheskiye svoystva metallicheskogo kompozitsionnogo materiala [The graphite grades lubrication effect on tribotechnical properties of the metallic composite material] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2018. №7 (67). St. 08. Available at: http://www.viam-works.ru (accessed: March 10, 2019). DOI: 10.18577/2307-6046-2018-0-7-69-77.
  23. Zhu S., Cheng J., Qiao Z., Yang J. High temperature solid-lubricating materials: A review // Tribology International. 2018. Vol. 133. P. 206–223.
  24. Gangopadhyay A., Jahanmir S., Peterson M.B. Self-lubricating ceramic matrix composites // Friction and wear of ceramics. 1994. Р. 163–197.
  25. Carrapichano J.M., Gomes J.R., Silva R.F. Tribological behaviour of Si3N4–BN ceramic materials for dry sliding applications // Wear. 2002. Vol. 253. No. 9–10. Р. 1070–1076.
  26. Liu J., Yang J., Yu Y. et al. Self-Lubricating Si3N4-based composites toughened by in situ formation of silver // Ceramics International. 2018. Vol. 44. No. 12. Р. 14327–14334.
  27. Sun Q., Yang J., Yin B. et al. High toughness integrated with self-lubricity of Cu-doped Sialon ceramics at elevated temperature // Journal of the European Ceramic Society. 2018. Vol. 38. No. 7. Р. 2708–2715.
  28. Sun Q., Wang Z., Yang J. et al. High-performance TiN reinforced Sialon matrix composites: A good combination of excellent toughness and tribological properties at a wide temperature range // Ceramics International. 2018. Vol. 44. No. 14. Р. 17258–17265.