Modern paint and varnish materials for use in aviation equipment products
UDC
629.7.023.222
DOI
10.18577/2307-6046-2019-0-5-62-67
Article PDF (Russian)
(539.84 KB)
How to cite
Zheleznyak V.G. Modern paint and varnish materials for use in aviation equipment products // Proceedings of VIAM. 2019. No. 5. DOI: 10.18577/2307-6046-2019-0-5-62-67. URL: https://viam-works.ru/en/journal/2019/5/7
Keywords
aviation equipment, paint and varnish materials, paintwork coatings, external influencing factors, operating conditions.
Abstract
Ensuring reliable protection of aviation equipment products from external influencing factors depends on the choice of paintwork and varnish materials and coatings based on them, which provide high adhesion, physicomechanical, protective and decorative properties. The main directions of work of the laboratory «Paintwork materials and coatings» of FSUE «VIAM», as well as the properties of paintwork and varnish materials and coatings based on them are presented. The key trends in the development of aviation paint and varnish materials and coatings based on them are presented.
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kraev I.D., Popkov O.V., Shuldeshov E.M. i dr. Perspektivy ispolzovaniya kremniyorganicheskikh polimerov pri sozdanii sovremennykh materialov i pokrytiy razlichnykh naznacheniy [Prospects for the use of organosilicon elastomers in the development of modern polymer materials and coatings for various purposes] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2017. №12. St. 05. Available at: http://www.viam-works.ru (accessed: September 28, 2018). DOI: 10.18577/2307-6046-2017-0-12-5-5.
- Kablov E.N. Materialy novogo pokoleniya – osnova innovatsiy, tekhnologicheskogo liderstva i natsionalnoy bezopasnosti Rossii [Materials of the new generation - the basis of innovation, technological leadership and national security of Russia] // Intellekt i tekhnologii. 2016. №2 (14). S. 16–21.
- Lakokrasochnyye pokrytiya. Istoriya aviatsionnogo materialovedeniya: VIAM – 75 let poiska, tvorchestva, otkrytiy / pod obshch. red. E.N. Kablov [Paint coatings. History of Aeronautical Materials Science: VIAM – 75 years of search, creativity, discoveries / gen. ed. by E.N. Kablov]. M.: Nauka, 2007. S. 326.
- Kablov E.N., Semenova L.V., Eskov A.A., Lebedeva T.A. Kompleksnyye sistemy lakokrasochnykh pokrytiy dlya zashchity metallicheskikh polimernykh kompozitsionnykh materialov, a takzhe ikh kontaktnykh soyedineniy ot vozdeystviya agressivnykh faktorov [Complex systems of paint and varnish coatings for the protection of metal polymer composites, as well as their contact compounds from the effects of aggressive factors] // Lakokrasochnyye materialy i ikh primeneniye. 2016. №6. S. 34–37.
- Kablov E.N. Materialy dlya aviakosmicheskoy tekhniki [Materials for aerospace] // Vse materialy. Entsiklopedicheskiy spravochnik. 2007. №5. S. 7–27.
- Semenova L.V., Malova N.E., Kuznetsova V.A., Pozhoga A.A. Lakokrasochnye materialy i pokrytiya [Paint and varnish materials and coatings] // Aviacionnye materialy i tehnologii. 2012. №S. S. 315–327.
- Nefedov N.I., Semenova L.V., Kuznecova V.A., Vereninova N.P. Lakokrasochnye pokrytiya dlya zashhity metallicheskih i polimernyh kompozicionnyh materialov ot stareniya, korrozii i biopovrezhdeniya [Paint coatings for protection of metallic and polymer composite materials against aging, corrosion and biodeterioration] // Aviacionnye materialy i tehnologii. 2017. №S. S. 393–404. DOI: 10.18577/2071-9140-2017-0-S-393-404.
- Eskov A.A., Lebedeva T.A., Belova M.V. Lakokrasochnye materialy s ponizhennym soderzhaniem letuchih veshhestv (obzor) [Paint-and-lacquer materials with lowered content of volatile organic compounds (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №6. St. 08. Available at: http://www.viam-works.ru (accessed: September 28, 2018). DOI: 10.18577/2307-6046-2015-0-6-8-8.
- Kuznetsova V.A., Semenova L.V., Kondrashov E.K., Lebedeva T.A. Lakokrasochnye materialy s ponizhennym soderzhaniem vrednyh i toksichnyh komponentov dlya okraski agregatov i konstrukcij iz PKM [Paint-and-lacquer materials with a low content of harmful and design of polymer composite materials] // Trudy VIAM: elektron. nauch-tehnich. zhurn. 2013. №8. St. 05. Available at: http://www.viam-works.ru (accessed: September 28, 2018).
- Kuznetsova V.A., Zheleznyak V.G., Silayeva A.A. Vliyaniye mekhanicheskikh kharakteristik gruntovochnykh pokrytiy na ustoychivost sistem erozionnostoykikh dispersno-armirovannykh pokrytiy k tsiklicheskim mekhanicheskim nagruzkam [Influence of mechanical characteristics of priming coverings on stability to cyclic mechanical loads of systems of the erosion resistant disperse reinforced coatings] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2018. №6 (66). St. 07. Available at: http://www.viam-works.ru (accessed: October 04, 2018). DOI: 10.18577/2307-6046-2018-0-6-59-67.
- Kuznetsova V.A., Kuznetsov G.V. Tendentsii razvitiya v oblasti toplivostojkih lakokrasochnyh pokrytij dlya zashhity toplivnyh kesson-bakov letatelnyh apparatov (obzor) [Development trends in the field of fuel resistant paintwork coatings for protection of integral fuel tanks of aircrafts (review)] // Trudy VIAM: elektron. nauchn.-tehn. zhurn. 2014. №11. St. 08. Available at: http://www.viam works.ru (accessed: October 04, 2018). DOI: 10.18577/2307-6046-2014-0-11-8-8.
- Kondrashov E.K., Kuznetsova V.A., Semenova L.V., Lebedeva T.A. Osnovnyye napravleniya povysheniya ekspluatatsionnykh, tekhnologicheskikh i ekologicheskikh kharakteristik lakokrasochnykh pokrytiy dlya aviatsionnoy tekhniki [The main directions of improving the operational, technological and environmental performance of paint coatings for aircraft] // Rossiyskiy khimicheskiy zhurnal. 2010. T. LIV. №1. S. 96–102.
- Klyukvina T.D., Vlasova K.A., Leonov A.A., Yashina S.A. Izuchenie mekhanizma obrazovaniya prochnosti v samotverdeyushchikh smesyakh s fenolnym svyazuyushchim (obzor) [Study of the mechanism of formation of strength in self-hardening mixtures with a phenolic binder (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2018. №3. St. 03. Available at: http://viam-works.ru (accessed: October 04, 2018). DOI: 10.18577/2307-6046-2018-0-3-18-27.
- Semyonova L.V., Bejder E.Ya., Petrova G.N., Nefedov N.I. Elektroizolyacionnye svojstva polimernyh pokrytij [Electro-insulative properties of polymer coatings] // Trudy VIAM elektron. nauch.-tehnich. zhurn. 2014. №8. St. 07. Available at: http://www.viam-works.ru (accessed: October 04, 2018). DOI: 10.18577/2307-6046-2014-0-8-7-7.
- Kuznetsova V.A., Kuznetsov G.V., Shapovalov G.G. Issledovanie vliyaniya molekulyarnoj massy epoksidnoj smoly na adgezionnye, fiziko-mehanicheskie svojstva i erozionnuyu stojkost pokrytij [Investigation of epoxy resin molecular mass influence by physiomechanical property and erosive resistant of coatings] // Trudy VIAM: elektron. nauchn.-tehnich. zhurn. 2014. №8. St. 08. Available at: http://www.viam-works.ru (accessed: October 04, 2018). DOI: 10.18577/2307-6046-2014-0-8-8-8.
- Kondrashov E.K. Termostoykiye kremniyorganicheskiye shpatlevki [Heat-resistant putties on base silicone resins] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №10 (58). St. 07. Available at: http://www.viam-works.ru (accessed: October 04, 2018). DOI: 10.18577/2307-6046-2017-0-10-7-7.