Abstract

Internal thermal stresses appearing during the curing of a polyester maleate binder and fiberglass on its base are considered. The effect of moisture (air humidity) on the breaking strength of samples and internal stresses appearing in the process of their production, storage (using) and heat treatment has been studied. It is shown that the internal stresses mainly depend on the difference in the moisture content of the samples compared to their initial state, while the breaking strength of the samples decreases with increasing moisture content.

Reference list
  1. Mukhametov R.R., Petrova A.P. Svoystva epoksidnykh polimernykh svyazuyushchikh i ikh pererabotka v polimernyye kompozitsionnyye materialy [Properties of epoxy binders and their processing in polymers composition materials] // Novosti materialovedeniya. Nauka i tekhnika: elektron. nauch.-tekhnich. zhurn. 2018. №3–4. St. 06. Available at: http://www.materialsnews.ru (accessed: April 04, 2019).
  2. Muhametov R.R., Petrova A.P., Ponomarenko S.A., Ahmadieva K.R., Pavlyuk B.F. Vliyanie tkanyh voloknistyh napolnitelej razlichnyh tipov na svojstva otverzhdennogo svyazuyushchego VS-2526K [Influence of woven fibrous fillers of various types on properties of cured binder VS-2526K] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2018. №3 (63). St. 04. Available at: http//www.viam-works.ru (accessed: April 12, 2019). DOI: 10.18577/2307-6046-2018-0-3-28-36.
  3. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  4. Kablov E.N. Materialy novogo pokoleniya [New generation materials] // Zashchita i bezopasnost. 2014. №4. S. 28–29.
  5. Kablov E.N. Iz chego sdelat budushcheye? Materialy novogo pokoleniya, tekhnologii ikh sozdaniya i pererabotki – osnova innovatsiy [What to make the future from? Materials of the new generation, technologies of their creation and processing - the basis of innovation] // Krylya Rodiny. 2016. №5. S. 8–18.
  6. Postnova M.V., Postnov V.I. Opyt razvitiya bezavtoklavnyh metodov formovaniya PKM [Development experience out-of-autoclave methods of formation PCM]// Trudy VIAM: ehlektron. nauch.-tekhnich. zhurn. 2014. №4. St. 06. Available at: http://www.viam-works.ru (accessed: April 12, 2019). DOI 10.18577/2307-6046-2014-0-4-6-6.
  7. Panina N.N., Kim M.A., Gurevich Ya.M., Grigorev M.M., Chursova L.V., Babin A.N. Svyazuyushchiye dlya bezavtoklavnogo formovaniya izdeliy iz polimernykh kompozitsionnykh materialov [Binders for non-autoclaving molding products from polymer composite materials] // Klei. Germetiki. Tekhnologii. 2013. №10. S. 18–27.
  8. Kablov E.N., Chursova L.V., Babin A.N., Mukhametov R.R., Panina N.N. Razrabotki FGUP «VIAM» v oblasti rasplavnykh svyazuyushchikh dlya polimernykh kompozitsionnykh materialov [Developments of FSUE «VIAM» in the field of melt binders for polymer composite materials] // Polimernyye materialy i tekhnologii. 2016. T. 2. №2. S. 37–42.
  9. Doneckij K.I., Hrulkov A.V. Principy «zelenoj himii» v perspektivnyh tehnologiyah izgotovleniya izdelij iz PKM [Principles of «green chemistry» in perspective manufacturing technologies of PCM articles] // Aviacionnye materialy i tehnologii. 2014. №S2. S. 24–28.
  10. Kablov E.N., Chursova L.V., Lukina N.F., Kutsevich K.E., Rubtsova E.V., Petrova A.P. Issledovaniye epoksidno-polisulfonovykh polimernykh sistem na osnove vysokoprochnykh kleyev aviatsionnogo naznacheniya [Study of epoxy-polysulfone polymer systems based on high-strength aviation-grade adhesives] // Klei. Germetiki. Tekhnologii. 2017. №3. S. 7–12.
  11. Vorobev A.E. Poliefirnyye smoly [Polyester resins] // Komponenty i tekhnologii: elektron. nauch.-tekhnich. zhurn. 2003. №6. St. 23. Available at: https://www.kit-e.ru (accessed: April 12, 2019).
  12. Dholakiya B. Unsaturated Polyester Resin for Specialty Applications // Intech open access publisher. 2012. Ch. 7. P. 167–202. DOI: 10.5772/48479.
  13. Gooch J.W. Vinyl Ester Resin // Encyclopedic Dictionary of Polymers. Springer, Science+Business Media, LLC, 2011. 794 p.
  14. Chursova L.V., Grebeneva T.A., Panina N.N., Tsybin A.I. Svyazuyushchiye dlya polimernykh kompozitsionnykh materialov stroitelnogo naznacheniya [Binders for polymeric composite materials for construction] // Vse materialy. Entsiklopedicheskiy spravochnik. 2015. №8. S. 13–17.
  15. Sanzharovskiy A.T. Metody opredeleniya mekhanicheskikh i adgezionnykh svoystv polimernykh pokrytiy [Methods for determining the mechanical and adhesive properties of polymer coatings]. M.: Nauka, 1974. 116 s.
  16. Illarionov V.A., Nanushyan S.R. Priroda vnutrennikh napryazheniy v zashchitnykh kompaundakh [The nature of internal stresses in protective compounds] // Komponenty i tekhnologii: elektron. nauch.-tekhnich. zhurn. 2004. №7. St. 25. Available at: https://www.kit-e.ru (accessed: April 12, 2019).
  17. Muzhichenko O.G., Plis N. Termomekhanicheskiye napryazheniya v sborochnykh mikrouzlakh [Thermomechanical stresses in assembly micro-sites] // Elektronika: nauka, tekhnologiya, biznes. 2000. №6. S. 63–64.
  18. Sorina T.G., Polyakov D.K., Korobko A.P., Penskaya T.V. Vinilefirnyye smoly dlya poltruzionnoy tekhnologii [Vinyl ether resins for poltrusion technology] // Elektronika. 2002. №4. S. 49–51.
  19. Evtushenko G.N., Evtushenko Yu.I., Simonov D.V. Perspektivy razvitiya proizvodstva nenasyshchennykh poliefirnykh smol [Prospects for the development of the production of unsaturated polyester resins] // Dvoynyye tekhnologii. 2010. №4. S. 65–69.